This study aims to compare the response of reinforced concrete (RC) T-beams strengthened with carbon fibre-reinforced polymer (CFRP) composite with that of non-strengthened control beams when subjected to monotonic two-point loading until failure for flexural once and shear again. The experimental programme tested eight RC T-beams, which included two reference beams without strengthening and six strengthened beams. The eight beams were divided into two main groups according to strengthening (flexural and shear). Experimental analysis was performed to study the effect of the CFRP laminate width in the flexural group and the spacing of CFRP U-wrap sheets in the shear group on the ultimate load capacity, load-strain relationship, and load-deflection relationship. Results show that increasing the width of the CFRP laminate in the flexural group improves the ultimate strengths to approximately 9.5%, 35%, and 41% for beams with CFRP laminate widths of 50, 100, and 150 mm, respectively, compared with the reference non-strengthened beam. The stiffness of the beams increases in direct proportion to the width of the CFRP laminate. In the meantime, decreasing the spacing of the CFRP laminate in the shear group increases the ultimate strengths to approximately 13.2%, 17.7%, and 23.5% for beams with CFRP U-wrap sheet spacings of 166, 125, and 100 mm, respectively, compared with the reference non-strengthened beam. Therefore, the spacing of the CFRP sheet is inversely proportional to the stiffness of the beam. Doi: 10.28991/CEJ-2023-09-08-05 Full Text: PDF
This study presents an investigation about the effect of fire flame on the punching shear strength of hybrid fiber reinforced concrete flat plates. The main considered parameters are the fiber type (steel or glass) and the burning steady-state temperatures (500 and 600°C). A total of 9 half-scale flat plate specimens of dimensions 1500mm×1500mm×100mm and 1.5% fiber volume fraction were cast and divided into 3 groups. Each group consisted of 3 specimens that were identical to those in the other groups. The specimens of the second and the third groups were subjected to fire flame influence for 1 hour and steady-state temperature of 500 and 600°C respectively. Regarding the cooling process, water sprinkling was applied directly aft
... Show MoreIn this study, the effect of the combination of micro steel fibers and additives (calcium hydroxide and sodium carbonate) on the size of cracks formation and healing them were investigated. This study aims to apply the use of self-healing phenomenon to repair cracks and to enhance the service life of the concrete structures. Micro steel fibers straight type were used in this research with 0.2% and 0.4% by volume of concrete. A weight of 20 and 30 kg/m3 of Ca(OH)2 and 2 and 3 kg/m3 of Na2CO3 were used as a partial cement replacement. The results confirm that the concrete cracks were significantly self-healed up to 30 days re-curing. Cracks width up to 0.2 mm were comp
... Show MoreThe construction of highly safe and durable buildings that can bear accident damage risks including fire, earthquake, impact, and more, can be considered to be the most important goal in civil engineering technology. An experimental investigation was prepared to study the influence of adding various percentages 0%, 1.0%, and 1.5% of micro steel fiber volume fraction (Vf) to reactive powder concrete (RPC)—whose properties are compressive strength, splitting tensile strength, flexural strength, and absorbed energy—after the exposure to fire flame of various burning temperatures 300, 400, and 500 °C using gradual-, foam-, and sudden-cooling methods. The outcomes of this research proved that the maximum reduction in mechanical prop
... Show MoreIn this paper, numerical and experimental studies on the elastic behavior of glass fiber reinforced polymer (GFRP) with stiffeners in the GFRP section's web (to prevent local buckling) are presented. The GFRP profiles were connected to the concrete deck slab by shear connectors. Two full-scale simply supported composite beams (with and without stiffeners) were tested under impact load (three-point load) to assess its structural response. The results proved that the maximum impact force, maximum deflection, damping time, and damping ratio of the composite beam were affected by the GFRP stiffeners. The experimental results indicated that the damping ratio and deflection were diminished compare
... Show MoreImproving in assembling technology has provided machines of higher evaluation with better resistances and managed behavior. This machinery led to remarkably higher dynamic forces and therefore higher stresses. In this paper, a dynamic investigation of rectangular machine diesel and gas engines foundation at the top surface of one-layer dry sand with various states (i.e., loose, medium and dense) was carried out. The dynamic investigation is performed numerically by utilizing limited component programming, PLAXIS 3D. The soil is accepted as flexible totally plastic material submits to Mohr-Coulomb yield basis. A harmonic load is applied at the foundation with amplitude of 10 kPa at a frequency of (10, 15 and 20) HZ and se
... Show MoreThis study investigated the structural behavior of a beam–slab member fabricated using a steel C-Purlins beam carrying a profile steel sheet slab covered by a dry board sheet filled with recycled aggregate concrete, called a CBPDS member. This concept was developed to reduce the cost and self-weight of the composite beam–slab system; it replaces the hot-rolled steel I-beam with a steel C-Purlins section, which is easier to fabricate and weighs less. For this purpose, six full-scale CBPDS specimens were tested under four-point static bending. This study investigated the effect of using double C-Purlins beams face-to-face as connected or separated sections and the effect of using concrete material that contains different recycled
... Show MoreSpray pyrolysis technique was subjected to synthesized (SnO2)1-x (TiO2: CuO) x Thin films on different substrates like glass and single crystal silicon using. The structure of the deposited films was studied using x-ray diffraction. A more pronounced diffraction peaks of SnO2 while no peaks of (CuO , TiO2 ) phase appear in the X-ray profiles by increasing of the content of (TiO2 , CuO) in the sprayed films. Mixing concentration (TiO2 , CuO) influences on the size of the crystallites of the SnO2 films ,the size of crystallites of the spray paralyzed oxide films change in regular manner by increasing of (TiO
... Show More