An aqueous chemical reaction has been used to prepare antifungal ZnS: Mn nanostructures, from manganese chloride, zinc acetate and thioacetamide in aqueous solution. The nanoparticle size has been controlled using thioglycolic acid as a capping factor. The major feature of the ZnS:Mn nanoparticles of average diameter ~ 2.73 nm is that possible preparing the sample from sources non-toxic precursors. The manufactured ZnS:Mn nanoparticles were identified and characterized to investigate the structure, morphology, composition of components of the nanoparticles and optical properties using (XRD, SEM, EDS and UV-Vis spectroscopy) techniques respectively. The agar dilution mechanism used to evaluate of the antifungal activity using ZnS:Mn nanoparticles which showed an efficient antifungal activity against four fungal models Aspergillus fumigatus ,Aspergillus falvus, Trichophyton mentagrophyte, and Microsporum audonii the inhibition increase with the increase of nanoparticle concentration. The antifungal property of manganese doped zinc sulphide nanoparticles creates from the interaction between nanoparticles and water led to generation the interactive oxygen species. Perturbation of the cell membranes due to the existence of Zn ions and S affecting on inhibition rate . the study aimed to evaluation the Antifungal Activity of ZnS:Mn Nanoparticles Against Some Isolated Pathogenic Fungi.
In this paper, the effect of iron oxide nanoparticles dust (Fe2O3 NPs) on the parameters of DC electric discharge plasma under vacuum in argon gas was studied with the presence of a mirror magnetron behind the electrodes (cathode and anode) at constant pressure and with different amounts of Fe2O3 nanoparticles. Calculations presented a reduction of the plasma emission intensity with the NPs content. Both the plasma density (calculated by Stark's broadening method) and the mean electron temperature (calculated using Boltzmann's equation) decreased with increasing the Fe2O3 nanoparticles dust content, which indicates clearly the effect of dust density on restricting
... Show MorePolycyclicacetal was prepared from the reaction of PEG with aldehyde derived from Erythro-ascorbic acid (pentulosono-ɣ-lactone-2,3-enedianisoate).All these compounds were characterized by Thin Layer Chromatography (TLC) and FTIR spectra and aldehyde was also characterized by (U.V-Vis), 1HNMR, 13CNMR, and mass spectra.The inhibitory effect of prepared polymer on the activity of human serum AcetylCholinesterase has been studied in vitro. The polymer showed a remarkable activity at low concentration (4.7x10-3 – 4.7x10-8M).
Liquid – liquid interface reaction is one of the method to prepare nanoparticles, the preparation of nanoparticles depends on the super saturation of ions which can satisfy by layered two immiscible liquid (toluene and deionized (DI) water). The XRD-diffraction analysis give a mix structure from hexagonal and cubic and the average grain size is 7.73 nm using Sherrer relation and 9.54 nm using Williamson –Hall method. Transmission electron microscopy (TEM) Showed that the size of particles around 3 nm which is comparable with Bohr radius of CdS.
From UV-Visible spectrum analysis which use two model to estimate the radius of particles , the first one is effective mass approximate (EMA) model and the second one is tight binding model
The microdrilling and nanodrilling holes are produced by a Q-switched Nd :YAG laser (1064 nm) interaction with 8009 Al alloy using nanoparticles. Two kinds of nanoparticles were used with this alloy. These nanoparticles are tungsten carbide (WC) and silica carbide (SiC). In this work, the microholes and nanoholes have been investigated with different laser pulse energies (600, 700 and 800)mJ, different repetition rates (5Hz and 10Hz) and different concentration of nanoparticles (90%, 50% and 5% ). The results indicate that the microholes and nanoholes have been achieved when the laser pulse energy is 600 mJ, laser repetition rate is 5Hz, and the concentration of the nanoparticles (for the two types of n
... Show MoreThis work aim to study the effect of silver nanoparticles on fluorescence intensity of Coumarin 480 dye by using the sandwiches technique where AgNP layer had been separated from C480 layer by different type of materials such as silica, PMMA polymer and PVA polymer layer. Silver nanoparticles had been prepared by the chemical reduction method so the AgNP layer coating had been done by hot rotation liquid method. The optical properties of prepared samples had been tested by using UV-VIS absorption spectrophotometer and Fluorescence spectrophotometer. Morphology, average size and the structure of nanoparticles were estimated using AFM, SEM testes
The present study was investigated the activity of aqueous extract from Cinnamomum cassia bark on the blood glucose levels in healthy and diabetic rats induced by Streptozotcin (STZ). In healthy rats the blood glucose levels were slightly decreased after six hoursof single oral administration with dose (25 mg/kg) of body wight, as well as four weeks after twice daily repeated oral administration of aqueous extract of Cinnamomum cassia bark. In streptozotocin induced diabetic rats we absorved high significant decreased (p<0.05) in blood glucose levels, after four weeks of oral administration of aqueous extract (25 mg /kg ).And blood glucose levels seems to be normal after the period of treatment .Glibenclamide used as standard drug to com
... Show MoreIn this research, the results of the Integral breadth method were used to analyze the X-ray lines to determine the crystallite size and lattice strain of the zirconium oxide nanoparticles and the value of the crystal size was equal to (8.2nm) and the lattice strain (0.001955), and then the results were compared with three other methods, which are the Scherer and Scherer dynamical diffraction theory and two formulas of the Scherer and Wilson method.the results were as followsScherer crystallite size(7.4nm)and lattice strain(0.011968),Schererdynamic method crystallite size(7.5 nm),Scherrer and Wilson methodcrystallite size( 8.5nm) and lattice strain( 0.001919).And using another formula for Schearer and Wilson methodwe obtain the size of the c
... Show MoreIn this paper, ZnO NPs were prepared using D.C high-voltage and high frequency with an output of 6 kHz at two different preparation times preparation (10,12) minutes. Transmission electron microscopy (TEM) with (FE-SEM) was used to examine the homogenous, compact, and dense surface of the zinc oxide nanoparticles created with apparent grain size determined by (XRD), XRD results explain that the increase of the preparation time from 10 minutes to 12-minute caused an increase in crystallite size. In addition, FE-SEM showed that the increase in the ZnO NPs cluster distribution with particle size increases with increasing the preparation time. AFM was also utilized to determine the degree of cooperation between the surfaces of the z
... Show MoreAqueous root extract has been used to examine the green production of silver nanoparticles (AgNPs) by reducing the Ag+ ions in a silver nitrate solution. UV-Vis spectroscopy, X-ray diffraction, field emission scanning electron microscopy, and Fourier transform infrared spectroscopy (FTIR) were used to analyze the produced AgNPs. The AgNPs that were created had a maximum absorbance at 416 nm, were spherical in form, polydispersed in nature, and were 685 nm in size.The AgNPs demonstrated antibacterial efficacy against Escherichia coli and Staphylococcus. The dengue vector Aedes aegypti's second instar larvae were very susceptible to the AgNPs' powerful larvicidal action.
Q-switch Nd: YAG laser of wavelengths 235nm and 1,460nm with energy in the range 0.2 J to 1J and 1Hz repetition rate was employed to synthesis Ag/Au (core/shell) nanoparticles (NPs) using pulse laser ablation in water. In this synthesis, initially the silver nano-colloid prepared via ablation target, this ablation related to Au target at various energies to creat Ag/Au NPs. Surface Plasmon Resonance (SPR), surface morphology and average particle size identified employing: UV-visible spectrophotometer, scanning electron microscopy (SEM) and transmission electron microscopy (TEM). The absorbance spectra of Ag NPs and Ag/Au NPs showed sharp and single peaks around 400nm and 410nm, respec