Background: Denture lining materials are widely used in prosthodontic treatment and management of traumatized oral mucosa. A contaminated prosthesis can provide a source of cross-contamination between patients and dental personnel as well as a cause for denture stomatitis. Therefore, denture disinfection has been recommended as an essential procedure for maintenance of a healthy oral mucosa. This study investigated the effect of SOLO disinfectant solution on some properties of different denture lining materials. Materials and methods: Three different solutions were used in this study; SOLO disinfectant solution, sodium hypochlorite solution, and water on three types of acrylic denture lining materials; hot cure, cold cure, and soft acrylic resin. Twenty seven disk-shaped samples were used to evaluate the color stability and forty five rectangular samples were used for testing the surface micro hardness and surface roughness of the different denture lining materials. Data measurements of the color stability, surface hardness, and surface roughness were analyzed and compared statistically. Results: The color stability for the tested denture lining materials was insignificantly affected (p>0.05) by the immersion in the SOLO disinfectant solution. There was a highly significant difference (p< 0.01) in the surface hardness of the hot cure while it was insignificant (p>0.05) for cold cure denture lining materials when immersed in the SOLO disinfectant solution. For surface roughness there was no significant difference (p>0.05) by immersion in SOLO disinfectant solution for the different denture lining materials. Conclusions: Based on the results of this study SOLO disinfectant solution produced no adverse effect on the color stability, surface hardness, and surface roughness of the hot cure, cold cure, and soft acrylic denture lining materials
This research is concerned with a new type of ferrocement characterized by its lower density and enhanced thermal insulation. Lightweight ferrocement plates have many advantages, low weight, low cost, thermal insulation, environmental conservation. This work contain two group experimental : first different of layer ferrocement, second different of ratio aggregate to cement. The experiments were made to determined the optimum proportion of cement and lightweight aggregate (recycle thermestone ). A low W/C ratio of 0.4 was used with super plasticizer conforming to ASTM 494 Type G. The compressive strength of the mortar mixes is 20-25 MPa. The work also involved the determination of thermal properties .Thermal conductivity value of thi
... Show MoreThe using of waste products as a recycled material was one of the most important studies for saving money and reduces the pollution. Mortar and concrete mixes with (10, 20 and 30)% of brick, glass and tile powder as replacement by weight of cement was investigated. The concrete mixes using brick or glass as 10%replacement of cement exhibited enhancement in compressive strength about (6, 4.7 and 2.0)% and (7.2, 5.6 and 2)% at age 7, 28 and 90 days respectively compared to reference mix. The 20% replacement of glass powder also showed an increase in the compressive strength up to (8, 6.3 and 4) %at age 7,28 and 90 days respectively compared to reference mix. Finally concrete mix using (10, 20 and 30) % tile powder as replacement of cement sho
... Show MoreIn this research we prepared CdS thin films by Spray pyrolysis method on a glass substrates and we study its structural , optical , electrical properties .The result of (X-Ray ) diffraction showed that all thin films have a polycrystalline structure , The relation of the transmission as a function of wavelength for the CdS films had been studied , The investigated of direct energy gap of the CdS its value is (2.83 eV). In Hall effect measurement of the CdS we find the charge carriers is p – type and Hall coefficient 1157.33(cm3/c) ,Hall mobility 6.77(cm2/v.s)
The using of waste products as a recycled material was one of the most important studies for saving money and reduces the pollution. Mortar and concrete mixes with (10, 20 and 30)% of brick, glass and tile powder as replacement by weight of cement was investigated. The concrete mixes using brick or glass as 10%replacement of cement exhibited enhancement in compressive strength about (6, 4.7 and 2.0)% and (7.2, 5.6 and 2)% at age 7, 28 and 90 days respectively compared to reference mix. The 20% replacement of glass powder also showed an increase in the compressive strength up to (8, 6.3 and 4) %at age 7,28 and 90 days respectively compared to reference mix. Finally concrete mix using (10, 20 and 30) % tile powder as replacement of cement sho
... Show MoreThe using of waste products as a recycled material was one of the most important studies for saving money and reduces the pollution. Mortar and concrete mixes with (10, 20 and 30)% of brick, glass and tile powder as replacement by weight of cement was investigated. The concrete mixes using brick or glass as 10%replacement of cement exhibited enhancement in compressive strength about (6, 4.7 and 2.0)% and (7.2, 5.6 and 2)% at age 7, 28 and 90 days respectively compared to reference mix. The 20% replacement of glass powder also showed an increase in the compressive strength up to (8, 6.3 and 4) %at age 7,28 and 90 days respectively compared to reference mix. Finally concrete mix using (10, 20 and 30) % tile powder as replacement of cement sho
... Show MoreConducted the study of the experimental conditions of the interaction of glass the visual Alpmuth containing 15% Mall of zinc with phosphoric acid ????? various degrees of thermal and clip areas prone to interact different way turntable
This work involves theoretical and experimental studies for seven compounds to calculate the electrons spectrum and NLO properties. The theoretical study is done by employing the Time Depending Density Functional Theory TD-DFT and B3LYP/high basis set 6-311++G (2d,2p), using Gaussian program 09. Experimental study by UV/VIS spectrophotometer device to prove the theoretical study. Theoretical and experimental results were applicable in spectrum and energy gap values, in addition to convergence theoretically the energy gap results from ΔEHOMO-LUMO and UV/VIS. spectrum. Consider the theoretical method very appropriate to compounds that absorb in vacuum UV.
Abstract:
In this study a type of polymeric composites from melting poly propylene as a basic substance with Palm fronds powder were prepared. Evaluation of polymeric composites was done by studying some of it is mechanical properties, which included:Yong modulus (E), Impact Strength (I.S), Brinell hardness (B.H) and Compression Strength (C.S). The polymeric composites were studied before and after reinforcment by comparing between them. There was an increase in resistance of Yong modulus (E), Impact Strength (I.S), Brinell hardness (B.H) and compression Strength (C.S). Also, the effect of some acids were studied such as (HCl, H2
Objective: The approximate life span of a silicone maxillofacial prosthesis is as short as1.5–2 years of clinical service, then a new prosthesis should be fabricated. The most common reasonfor re-making the prosthesis is silicone mechanical properties degradation. The aim of this studywas to assess some mechanical properties of VST-30 silicone for maxillofacial prostheses after addi-tion of intrinsic pigments.Methods: Two types of intrinsic pigments (rayon flocking and burnt sienna); each of them wasincorporated into silicone. One hundred and twenty samples were prepared and split into 4 groupsaccording to the conducted tests (tear strength, hardness, surface roughness, and tensile strengthand elongation percentage) with 30 samples for ea
... Show MoreResearch in Iraq has expanded in the field of material technology involving the properties of the lightweight concrete using natural aggregate. The use of the porcelinate aggregate in the production of structural light concrete has a wide objective
and requires a lot of research to become suitable for practical application. In this work metakaolin was used to improve compressive strength of lightweight porcelinate concrete which usually have a low compressive strength about 17 MPa . The effect of metakaolin on compressive, splitting tensile, flexure strengths and modulus of elasticity of lightweight porcelinate concrete have been investigated. Many experiments were carried out by replacing cement with different percentages of