A new tool geometry was used to achieve friction stir spot welding (FSSW) in which the shoulder was designed separately from the rotating pin, and in order to examine weldment strength through the modified tool, a lap joints of AA2024 aluminum alloy plate 1 mm thick were welded successfully by using 6 mm pin diameter and varying process parameters (rotational speeds, tool nose geometry, and depth of tool penetration in the lower welded plate). Experimental tests indicate that the maximum average tensile shear load was 3100 N at the best selected condition. Microstructure examination and micro hardness test along the spot zones were investigated as well as measuring pin penetration load. Visual inspection of the welded spot surface shows a good appearance and clean surface and there is no need to any mechanical post treatment.
Background: Separation and deboning of artificial teeth from denture bases present a major clinical and labortory problem which affect both the patient and the dentist. The optimal bond strength of artificial teeth with denture base reinforced with nanofillers and flexible denture bases and the effect of thermo cycling should be evaluated. This study was conducted to evaluate and compare the shear bond strength of artificial teeth (acrylic and porcelain) with denture bases reinforced by 5% Zirconium oxide nanofillers and flexible bases under the effect of different surface treatments and thermo cycling and comparing the results with conventional water bath cured denture bases. Material and methods: Two types of artificial teeth; acrylic and
... Show MoreObjective(s): The world of dentistry is constantly evolving, and with the advent of 3D printing technology, the possibilities are endless. However, little is known about the effects of adding ZrO2 NPs to the denture base resin of 3D additive manufacturing technique.Aim of this study is to evaluate the behavior of resin which is used to 3D printing of denture base with the addition of ZrO2 NPs on denture adaptation property and diametral compression strength.Methods: 60 samples were printed, 30 disks for diametral compressive test and 30 denture base for denture adaptation test. Three groups per test (n=10). The control group for each test included unreinforced 3Dprinted denture base resin, and the other groups were reinforced with (2&
... Show MoreThis study aims to find the effect of water-cement ratio on the compressive strength of concrete by using ultrasonic pulse velocity test (UPVT). Over 230 standard cube specimens were used in this study, with dimensions of 150mm, and concrete cubes were cured in water at 20 °C. Also, the specimens used in the study were made of concrete with varied water-cement ratio contents from 0.48 to 0.59. The specimens were taken from Diyarbakir-Turkey concrete centers and tested at the structure and material science lab, civil engineering, faculty of engineering from Dicle University. The UPV measurement and compressive strength tests were carried out at the concrete age of 28 days. Their UPV and compressive strength ranged
... Show MoreThe effect of different Ti additions on the microstructure of Al-Ti alloy prepared by powder metallurgy was investigated. A certain amount of Ti (10wt%, 15wt%, and 20wt%) were added to aluminium and the tests like microhardness, density, scanning electron microscope (SEM), optical microscope (OM) and X-Ray Diffraction (XRD) were conducted to determine the influence of different Ti additives on the Al-Ti alloy properties and microstructure. The results show that the grains of α-Al changed from large grains to roughly spherical and then to small rounded grains with increasing Ti content, the micro-hardness of the alloy increases with increasing Ti, and XRD results confirm the formation of TiAl3 intermetallic co
... Show MoreBackground: The longevity of any prosthesis depends on the materials from which it was fabricated, that is why, defects in the material properties may reduce the service life of prosthesis and necessitate its replacement. The aim of this study was to evaluate the effect of adding different concentrations of Polyamide-6 (Nylon-6) on the tear and tensile strength of A-2186 RTV silicone elastomer. Materials and Methods: 80 samples were fabricated by the addition of 0%, 1%, 3% and 5% by weight PA-6 micro-particles powder to A-2186 platinum RTV silicone elastomer. The study samples were divided into four (4) groups, each group containing 20 samples. One control group was prepared without PA-6 micro particles and three experimental groups were pr
... Show MoreHighly plastic soils exhibit unfavorited properties upon saturation, which produce different defects in engineering structures. Attempts were made by researchers to proffer solutions to these defects by experimenting in practical ways. This included various materials that could possibly improve the soil engineering properties and reduce environmental hazards. This paper investigates the strength behavior of highly plastic clay stabilized with brick dust. The brick dust contents were 10%, 20%, and 30% by dry weight of soil. A series of linear shrinkage and unconfined compression tests were carried out to study the effect of brick dust on the quantitative amount of shrinkage experienced by highly plastic clay and the undra
... Show More