In this study, doped thin cadmium peroxide films were prepared by pulsed laser deposition with different doping concentrations of aluminium of 0.0, 0.1, 0.3, and 0.5 wt.% for CdO2(1-X)Al(X) and thicknesses in the range of 200 nm. XRD patterns suggest the presence of cubic CdO2 and the texture factor confirms that the (111) plane was the preferential growth plane, where the texture factor and the grain size decreased from 2.02 to 9.75 nm, respectively, in the pure sample to 1.88 and 5.65 nm, respectively, at a concentration of 0.5 wt%. For the predominant growth plane, the deviation of the diffraction angle Δθ and interplanar distance Δd from the standard magnitudes was 2.774° and 0.318 Å, respectively, for the pure sample decreased to − 2.633° and 0.301 Å for the largest doping concentration. The optical absorption was found to decrease with increasing doping concentration, where the changes in threshold wavelengths from the standard λ = 496 nm were blue shifted by Δλ = 142, 133, 128, and 152 nm, respectively, for the concentrations used. The occurrence of such blue shifts points to a widening of the band gap to Eg = 3.5, 3.4, 3.35, and 3.6 eV for concentrations of 0.0, 0.1, 0.3, and 0.5 wt%, respectively.
Chemical bath deposition was used to synthesize ZnO nanorods (NRs) on glass and fluorine_doped tin oxide (FTO) substrates. X-ray diffraction was performed to examine the crystallinity of ZnO nanorod. Results showed that ZnO NRs had a wurtzite crystal structure. Field emission scanning electron microscopy images showed that glass sample had rod-like structure distribution with (50 nm) diameter and average length of approximately (700 nm), whereas the FTO-coated glass sample had 25 nm diameter and average length of approximately 950 nm. The direct optical transition band gaps of the glass and FTO_coated glass samples were( 4 and 4.43 eV), respectively. The structural and optical properties of the synthesized ZnO p
... Show MoreThe present study includes a theoretical treatment to derive the general equations of pumping threshold power ( ), laser output power (Pout), and laser device efficiency (ƞ) of the element-doped thin-disk laser (Yb3+) with a quasi-three-level pumping scheme in the continuous wave mode at a temperature of (299K°). In this study, the host crystals (YAG) were selected as typical examples of this laser design in a Gaussian transverse mode. The numerical solution of these equations was made using Matlab software by selecting the basic parameters from the recently published scientific articles for the laser design of these crystal hosts. According to this simulation, this article studied the effect o
... Show MoreThe integral breadth method has been utilized to analyse line
proIiles broadening and lattice strain of CaO at different temperatures
The effect of tcmperattre on crystallite size and strain has also been investigated . The crystall i tes are found to be highly anisotropic even at high temperatures
In this research, the X-ray diffraction pattern was used, which was obtained experimentally after preparation of barium oxide powder. A program was used to analyze the X-ray diffraction lines of barium oxide nanoparticles, and then the particle size was calculated by using the Williamson-Hall method, where it was found that the value of the particle size is 25.356 nm. Also, the dislocation density was calculated, which is equal to1.555 x1015 (lines/nm2), and the value of the unit cell number was also calculated, as it is equal to 23831.
The thermal evaporation technique was used to prepare the Ni-Cr films with a thickness of 200 nm and a rate of deposition of 0.22nm/Sec. The annealing was performed at 373 and 473 K. The structural and optical analyses of the grown layers were achieved and XRD patterns showed amorphous structure transferred to polycrystalline for film annealed at 373 and 473 K. AFM analysis showed that the surface of Ni-Cr films is homogenous and the average roughness, optical energy gap and absorption coefficient were increased with increasing annealing temperature (Ta).
optical properties of pure poly(vinyl Alcohol) films and poly(vinyl Alcohol) doped with methyl red were study, different percentage prepared with constant thickness using casting technique. Absorption, Transmission spectra have been recorded in order to study the optical parameters such as absorption coefficient, energy gap, refractive index, Extinction coefficient and dispersion parameters were measured in the wavelength range (200-800)nm. This study reveals that the optical properties of PVA affect by increasing the impurity concentration.
The electrical properties of polycrystalline cadmium telluride thin films of different thickness (200,300,400)nm deposited by thermal evaporation onto glass substrates at room temperature and treated at different annealing temperature (373, 423, 473) K are reported. Conductivity measurements have been showed that the conductivity increases from 5.69X10-5 to 0.0011, 0.0001 (?.cm)-1 when the film thickness and annealing temperature increase respectively. This increasing in ?d.c due to increasing the carrier concentration which result from the excess free Te in these films.
Some of structural ,and electrical properties of pure and zinc (Zn) doped cadmium telluride thin films with impurity percentages (0.5, 1, 1.5)%, deposited on hot glass substrate (temperature equals to 423K) of thickness of 300nm and rate deposition of 0.5 nm.s-1 by thermal co-evaporation technique under vacuum of (2×10-5)Torr have been investigates. The structural properties for the prepared films were studied before and after. doping process by analysis of the X-ray diffraction, and it appeared that pure and dopant CdTe thin films are polycrystalline and have the cubic structure with preferential orientation in the [111] direction, and the crystal structure of the films were improved due to doping process. From d.c
... Show MoreThe paper include study the effect thickness of the polymeric sample which is manufactured by thermo press way. The sample was used as an active tunable R6G laser media. The remarks show that, when the thickness of the samples is increased, with the same concentration, the spectrum will shift towards the short wavelength, & the quantum fluorescence yield will increased. The best result we obtained for the quantum fluorescence yield is (0.68) at the sample, with thickness (0.304mm) in Ethanol solvent, while when we used the Pure Water as a solvent, we found that the best quantum fluorescence yield is (0.63) at (0.18mm) thickness of the sample.