Denture cleansing is an essential step that can stop cross‑contamination and adds to the health of the patient, denture durability, and the general quality of life. A disinfection technique must be practical and devoid of damaging effects on the material's properties used to construct the denture base. The main aim of this study is to evaluate the effect of three concentrations of electrolyzed water denture cleanser on heat cure acrylic and polyamide after immersion in electrolyzed water. The evaluation is based on their efficacy on surface hardness, wettability, and color stability compared with one submerged in distilled water as a control group. The method consists of eighty samples of heat-cured acrylic and polyamide material. The samples were immersed in electrolyzed water at a concentration of (100-200ppm) and in distilled water for 5 minutes, 30 times, and daily for 12 days to simulate a one-year interval. The tests showed that the surface hardness and color stability were maintained, with no significant difference between the control and experimental groups. In comparison, the result of wettability showed a statistically significant difference between the control and experimental groups. Thus, electrolyzed water does not affect the surface hardness and color stability of heat-cure acrylic and polyamide denture base materials. However, the wettability of these materials was significantly increased. Keywords: Electrolyzed water; Heat cure acrylic; Polyamide material
Background: Fluoridated acrylic resin material can present more stable properties when compared with conventional one.The most widely used fluoride –containing substance added to dental resin materials is sodium fluoride (Naf). This study evaluated the effect of Naf in different concentration to the acrylic resin denture base material and its effect on tensile strength ,modules of elasticity with long –term water immersion (after 4 months immersion in de-ionized water) Materials and methods: Eighty specimens from dumbbells shaped metal pattern for tensile strength test were preparedaccording to ISO 527: 1993 plastic –Determination tensile properties ,in dimensions(60mm, 12mm, 3 ± 0.2mm) length, width and depth respec
... Show MoreBackground: In this study we evaluate the effect of plasma treatment (oxygen and argon) gas in two different exposure times on the surface of heat cure and light cure acrylic resin. Materials and method: 100 specimens of heat cure and light cure acrylic resin were fabricated. The measurements of the samples were (75mm, 25mm and 4.5mm) length, width and depth respectively with stopper of 3mm depth. Two types of gas used oxygen and argon in (5,10) min by using (DC-glow discharge plasma device) then we apply cold cure soft lining material, with the help of Instron machine we test the shear stress value. Results: A highly significant effect after argon and oxygen gases treatment in both 5 and 10 min exposure times on shear bond strength to soft
... Show MoreStaphylococcus aureus is a common pathogenic agent due to its ability to cause various types of infections, ranging from mild skin infections to sever systemic diseases. One of the most virulence factors of this bacterium is its ability to from biofilms on solid surfaces by anchoring the planktonic cells and by producing a protective layer of extra polymeric substances. Biofilm formation is controlled through many genes. The most important ones are icaA and icaD. Dentures are prosthetic devices that are made of different materials to replace lost teeth. The aim of this study is to examine the ability of different types of denture materials to support the biofilm formation of S. aureus at phenotypic level by detecting ba
... Show MoreIn this research, the use of natural materials like wool and cannabis as intermediate reinforcement for prosthetic limbs due to their comfort, affordability, and local availability was discussed. As part of this study on below-the-knee (BK) prosthetic sockets, two sets of samples were made using a vacuum method. These sets were made of natural fiber-reinforced polymer composites with lamination 80:20: group (Y) had 4 perlon, 1 wool 4 perlon, and group (G) had 4 perlon, 1 cannabis 4 perlon. The two groups were compared with a socket made of polypropylene. Tensile testing was used to determine the mechanical characteristics of the socket materials. The Y group has a yield stress of 17 MPs, an ultimate strength of 18.75 MPa, and an elastic
... Show MoreBackground: During acrylic resin processing, the mold must be separated from the surface of the gypsum to prevent liquid resin from penetrating into the gypsum, and water from the gypsum seeping into the acrylic resin. For many years, tin foil was the most acceptable separating medium, and because it's difficult to apply, a tin-foil substitute is used. In this study, olive oil is used as an alternative to tin foil separating medium for first time, and evaluating its effect as a separating medium on some mechanical properties such as (indentation hardness and transverse strength) of acrylic resins denture base comparing it with those processed using tin-foil and tin foil substitute such as (cold mold seal) separating medium. Materials and M
... Show More
This study aims to evaluate and compare the cytotoxicity and biocompatibility of a modified heat-cured acrylic denture base material containing 15% phosphoric acid 2-hydroxyethyl methacrylate ester (PA2HEME) with those of nonmodified PMMA. Discs with a diameter of 12 mm and a thickness of 2 mm were prepared using a heat-cured PMMA denture base material and divided into control and experimental groups. The experimental group was modified with 15% phosphoric acid 2-hydroxyethyl methacrylate ester (PA2HEME). The modified and nonmodified materials were tested via FTIR, and the effect of modification on surface roughness was evaluated with AFM. An in vitro test was conducted to examine the cytotoxicity and biocompatibility of heat-cured acry
... Show MoreBackground: Denture fracture is one of the most common problems encountered by the patients and prosthodontists. The objective of present study was to evaluate the transverse strength of nylon denture base resin repaired by using conventional heat polymerized, autopolymerized and visible light cure {VLC} resins, surface treatment that used for repair and adjustment of insufficient nylon denture bases and in case of addition of artificial teeth. As these corrective procedures are common chair side procedures in dental clinic. Materials and methods: One hundred twenty nylon specimens were prepared by using metal patterns with dimension of (65x10x2.5 mm) length, width, and thickness respectively for transverse strength test while for tensile b
... Show MoreObjective(s): The aim of this study is to compare the impact strength of a heat cured denture-base acrylic resin
reinforced with metal wire and glass fibers.
Methodology: Forty five specimens were prepared from pink heat cure acrylic resin. Specimens were grouped into;
group-I (control group) which consists of 15 specimens with no reinforcement, group-II which consists of 15 specimens
reinforced with metal wire, and group-III consists of 15 specimens reinforced with glass fibers. Specimens were tested
by using charpy impact machine.
Results: The result showed that there was a highly significant difference in impact strength value among the testing
groups at (P < 0.001).
Conclusion: The impact str
... Show More