Bulk AlxSb1-x samples were prepared with different x ratios (0.1, 0.3, 0.5, 0.7 and 0.9) by quenching technique. This was done throughout mixing the aluminum and antimony elements according to the proper atomic weight and put them in an evacuated quartz ampoule which then sealed and heated at 1273 K for five hours and left to cool in air. Thin films of AlxSb1-xwere prepared by using thermal evaporation under vacuum of 10-5 mbar on glass substrates at room temperature with deposition rate (10-15nm/min) at thickness of ∼ 500nm. The structures of AlxSb1-x bulk and thin films have been studied by X–ray diffraction technique. The results showed that all alloys have polycrystalline structures and the peaks at composition ratio x = 0.3, 0.5 and 0.7 were identical with the AlSb standard peaks while at x = 0.1 and 0.9 the peaks are identical with Sb and Al respectively. The x-ray pattern of the prepared thin films are polycrystalline and the peaks identical with cubic structure also the peaks intensity decrease with the increase of aluminum ratio in the prepared thin films. AFM measurements showed the non-regular variation (increasing and decreasing) of both the average grain size and average surface roughness with the increasing of composition ratio. AlxSb1-x thin films showed high charge carrier concentration nHespecially at x = 0.1 and 0.3 on the other side charge carrier concentration showed reduction with the increase of aluminum content whereas nHreach minimum value at x = 0.7 and then increases with further increase of aluminum content. The electrical conductivity of AlxSb1-x declare similar behavior where it reach minimum value at x = 0.5. From another side AlxSb1-x thin films show high conductivity resemble that of metallic material especially also at x = 0.1 and 0.3.
Thin films of highly pure (99.999%) Tellurium was prepared by high vacuum technique (5*10-5torr), on glass substrates .Thin films have thickness 0.6m was evaporated by thermal evaporation technique. The film deposited was annealed for one hour in vacuum of (5*10-4torr) at 373 and 423 K. Structural and electrical properties of the films are studies. The x-ray diffraction of the film represents a poly-crystalline nature in room temperature and annealed film but all films having different grain sizes. The d.c. electrical properties have been studied at low and at relatively high temperatures and show that the conductivity decreases with increasing temperature at all range of temperature. Two types of conduction mechanisms were found to d
... Show MoreInSb alloy was prepared then InSb:Bi films have been prepared successfully by thermal evaporation technique on glass substrate at Ts=423K. The variation of activation energies(Ea1,Ea2)of d.c conductivity with annealing temperature (303, 373, 423, 473, 523 and 573)K were measured, it is found that its values increases with increasing annealing temperature. To show the type of the films, the Hall and thermoelectric power were measured. The activation energy of the thermoelectric power is much smaller than for d.c conductivity and increases with increasing annealing temperature .The mobility and carrier concentration has been measured also.
BixSb2-xTe3 alloys with different ratios of Bi (x=0, 0.1, 0.3, 0.5, and 2) have been prepared, Thin films of these alloys were prepared using thermal evaporation method under vacuum of 10-5 Torr on glass substrates at room temperature with different deposition rate (0.16, 0.5, 0.83) nm/sec for thickness (100, 300, 500) respectively. The X–ray diffraction measurements for BixSb2-xTe3 bulk and thin films indicate the polycrystalline structure with a strong intensity of peak of plane (015) preferred orientation with additional peaks, (0015) and (1010 ) reflections planes, which is meaning that all films present a very good texture along the (015) plane axis at different intensities for each thin film for different thickness. AFM measureme
... Show MorePulsed-laser deposition (PLD) technique was used to prepare thin films from cerium oxide (CeO2) doped with erbium and indium oxides. In order to characterize the morphology and sensing features, these films were deposited on glass and/or single silicon substrates, respectively, with erbium and indium oxides. The morphological investigation conducted using atomic force microscope has shown an increase in the non-regularity of particle diameter with increasing doping ratios of both oxides. The maximum particle diameter of 61.45nm was obtained for 9% Eu2O3-doped CeO2. The surface roughness value of Eu2O3-doped ceria was higher than those of In2O3-doped ceria. The gas sensing measurements were done at
... Show MoreThe effect of different doping ratio (0.3, 0.5, and 0.7) with thickness in the range 300nmand annealed at different temp.(Ta=RT, 473, 573, 673) K on the electrical conductivity and hall effect measurements of AgInTe2thin film have and been investigated AgAlxIn(1-x) Te2 (AAIT) at RT, using thermal evaporation technique all the films were prepared on glass substrates from the alloy of the compound. Electrical conductivity (σ), the activation energies (Ea1, Ea2), Hall mobility and the carrier concentration are investigated as a function of doping. All films consist of two types of transport mechanisms for free carriers. The activation energy (Ea) decreased whereas electrical conductivity increases with increased doping. Results of Hall Effect
... Show MoreSub-threshold operation has received a lot of attention in limited performance applications.However, energy optimization of sub-threshold circuits should be performed with the concern of the performance limitation of such circuit. In this paper, a dual size design is proposed for energy minimization of sub-threshold CMOS circuits. The optimal downsizing factor is determined and assigned for some gates on the off-critical paths to minimize the energy at the maximum allowable performance. This assignment is performed using the proposed slack based genetic algorithm which is a heuristic-mixed evolutionary algorithm. Some gates are heuristically assigned to the original and the downsized design based on their slack time determined by static tim
... Show MoreIn this paper the effect of thermal annealing on the structural and optical properties of Antimony Selenide (Sb2Se3) is investigated. Sb2Se3 powder is evaporated on clean amorphous glass substrates at room temperature under high vacuum pressure (4.5×10-6 mbar) to form thin films. The structural investigation was done with the aid of X-ray diffraction (XRD) and atomic force microscopy (AFM). The amorphous to polycrystalline transformation of these thin films was shown by X-ray diffraction analysis after thermal annealing. These films' morphology is explained. (UV-Vis ) spectra in ranges from 300 to 1100 nm was used to examine the optical properties of the films .The absorption coefficient and optical energy gap of the investigated films are
... Show MoreAbstract
This study investigates the mechanical compression properties of tin-lead and lead-free alloy spherical balls, using more than 500 samples to identify statistical variability in the properties in each alloy. Isothermal aging was done to study and compare the aging effect on the microstructure and properties.
The results showed significant elastic and plastic anisotropy of tin phase in lead-free tin based solder and that was compared with simulation using a Crystal Plasticity Finite Element (CPEF) method that has the anisotropy of Sn installed. The results and experiments were in good agreement, indicating the range of values expected with anisotropic properties.
Keywords<
... Show MoreIn this study, thin films of pure titanium dioxide (TiO2) and titanium dioxide dual mixed with zinc oxide (ZnO) and magnesium oxide (MgO) with varying concentrations of (ZnO: MgO)x ranging from 0 to 30 wt% undoped and doped gold nanoparticles (AuNPs) were prepared on glass using the chemical spray pyrolysis (CSP) technique. The morphological, structural, and sensing properties of the prepared thin films were examined. Atomic Force Microscopy (AFM) analysis revealed that these films exhibit a consistent structure before and after doping. Initially, the roughness of these films was observed to increase upon the introduction of impurities (ZnO: MgO)x. This trend reversed at x=0.20, where a decrease in roughness occurred. Interestingly, a sub
... Show MoreIn this study, thin films of pure titanium dioxide (TiO 2 ) and titanium dioxide dual mixed with zinc oxide (ZnO) and magnesium oxide (MgO) with varying concentrations of (ZnO: MgO) x ranging from 0 to 30 wt% undoped and doped gold nanoparticles (AuNPs) were prepared on glass using the chemical spray pyrolysis (CSP) technique. The morphological, structural, and sensing properties of the prepared thin films were examined. Atomic Force Microscopy (AFM) analysis revealed that these films exhibit a consistent structure before and after doping. Initially, the roughness of these films was observed to increase upon the introduction of impurities (ZnO: MgO) x . This trend reversed at x = 0.20, where a decrease in roughness occurred. Interestin
... Show More