Due to the specific characteristic of porcelain, the insertion of Beryllium oxide has been studied. The basic materials and quantities were selected carefully. In this work, porcelain containing 32 wt% feldspar, 24 wt% quartz and 44 wt% clay was synthesized and beryllium oxide (BeO) (1 wt.%, 3 wt.%, 5 wt% and 7wt%) were add. The basic and new composition porcelain powders were uniaxially compacted into standard samples dimensions and fired at various sintering temperatures, 1100°C, 1300°C, and 1450°C then held for 2 hour in a furnace.
The effects of sintering temperatures and beryllium oxide content on mechanical, electrical and structural properties were studied. The increasing of sintering temperature on the basi
...