The creation and characterisation of biodegradable blend films based on chitosan and polyvinyl alcohol for application in a range of packaging is described. The compatibility between the chitosan and PVA polymers was good. Composite films had a compact and homogeneous structure, according to the morphology analysis. The mechanical test result of PVA/CH at concentrations 5% showed, that The higher values of TS recorded in sample (p1, with 40 MPa) while the lower values appeared in sample (p9, with 22.09 MPa), the TS decreased gradually as the amount of PVA increased in blend film. While the blend film of pure Chitosan exhibits a poor mechanical strength which makes it a poor candidate for packaging but Blending CH with PVA together improved tensile strength. PVA/CH at concentrations 10%. Showed the higher TS values appeared in sample (C1 with 36.64MPa) while the lower values of TS appeared in sample (C9 with 24.4 MPa). In comparison with pure PVA have the lower TS than all blend film. The result of mechanical properties after addition of borax solution revealed that the Borax improves the E at max and TS of blend films. Mechanical properties results of CH/PVA/Tio2, Showed that the TS and E at max were increased after introducing of Tio2 into the polymer matrix. The P1 sample have been chosen according to their possess acceptable TS, E at max to be subjected to gamma radiation at different doses 2.3, 3.5, 4.5, 6, 7.5 kGy. The results demonstrated, that the increasing the radiation doses lead to increasing in TS of blend film, following increasing in E at max, the highest TS of the irradiated films is observed at 7.5.kGy dose.
In the present research synthesis and study of biological activity a series of new polymers modified of chitosan with compounds containing azo group. Beginning diazonium salt produced from 3,3'-dimethyl-[1,1'-biphenyl]-4,4'-diamine reacted with concentrated HCl acid and sodium nitrite. The coupling reaction between diazonium salt with substituted aromatic aldehyde to produce Azo derivatives )1-6(. Azo Schiff bases Chitosan )7-12( were synthesized by condensation of Chitosan with Azo derivatives )1-6( in ethanol with some drops of glacial acetic acid. The structural modifications of Chitosan ring (linked to a bioactive azo moiety) were expected to give new derivatives )7-12( with a diverse range of biological functions. These compounds' st
... Show Moreفي البحث الحالي تم تحضير ودراسة النشاط الحيوي لسلسلة من البوليمرات الجديدة المحورة من الكيتوسان مع مركبات تحتوي على مجموعة الآزو. في البداية تم تحضير ملح الديازونيوم من تفاعل 3,3'-dimethyl-[1,1'-biphenyl]-4,4'-diamine مع حامض الهيدروكلوريك المركز ونتريت الصوديوم .ثم تفاعل الازدواج بين ملح الديازونيوم مع الديهايدات اروماتية معوضة لإنتاج مشتقات الازو (1-6). ازو شف بيس كيتوسان((12-7 والتي حضرت من تفاعل الكيتوسان مع مشتقات
... Show MoreThis study was carried out to investigate the possibility of chickpea soaked water as a substitute for yeast in dough fermentation and its effects on sensory properties of the laboratory loaf bread. Chickpea was soaked for 24,48 and 72 hours at room temperature and used in proportion with or without yeast in dough fermentation . The results revealed that , as the percentage of soaked chickpea water substitution increased, the volume of the produced loaf bread decreased as compared with the control treatment (only yeast ).Best results were obtained by using soaked chickpea water for 24 hours in proportion of 1:1 soaked chickpea water : yeast regarding the sensory properties ,volume and leavening of the loaf bread.
Keywords: chickpea so
Numerous drilling additives and materials are used continuously because they are necessary to support and give the required properties of the drilling fluid so that to ensure the stability of the borehole. This paper aspires to evaluate the rheological properties of bentonite (montmorillonite) Trefawey as an alternative to using commercial bentonite. Monitoring and evaluating of the rheological and filtration properties were prepared. This exertion aims to focus on the effect of hematite, and barite on the rheological properties of the three aforementioned bentonite types. An improvement in the rheological properties of bentonite (montmorillonite). Trefawey was observed after adding the previous heavy materials. Hematite has by some
... Show MoreA polycrystalline PbxS1-x alloys with various Pb content ( 0.54 and 0.55) has been prepared successfully. The structure and composition of alloys are determined by X-ray diffraction (XRD), atomic absorption spectroscopy (AAS) and X-ray fluorescence (XRF) respectively. The X-ray diffraction results shows that the structure is polycrystalline with cubic structure, and there are strong peaks at the direction (200) and (111), the grain size varies between 20 and 82 nm. From AAS and XRF result, the concentrations of Pb content for these alloys were determined. The results show high accuracy and very close to the theoretical values. A photoconductive detector as a bulk has been fabricated by taking pieces of prepared alloys and polished chemic
... Show MoreThe structural, optical and electrical properties of ZnS films prepared by vacuum evaporation technique on glass substrate at room temperature and treated at different annealing temperatures (323, 373, 423)K of thickness (0.5)µm have been studied. The structure of these films is determined by X-ray diffraction (XRD). The X-ray diffraction studies show that the structure is polycrystalline with cubic structure, and there are strong peaks at the direction (111). The optical properties investigated which include the absorbance and transmittance spectra, energy band gab, absorption coefficient, and other optical constants. The results showed that films have direct optical transition. The optical band gab was found to be in the range t
... Show More