Mn2O3 was coated onto reduced titania nanotubes by reverse pulse electrodeposition, showing smooth and homogenous deposits without covering the opening of the nanotubes.
In this study, the melting-cooling method was used to prepare the chalcogenide compound S60-Se40-X-PbX. Four samples were obtained by partial replacement of Selenium with Lead in the weight ratios x = 0, 10, 20, and 30, respectively. The materials were mixed separately, ground, placed in quartz ampoules, and heated to 500 degrees Celsius. After conducting several operations on the samples, their insulating properties were studied, represented by the real dielectric constant and the imaginary dielectric constant, and the electrical conductivity was measured as a function of the frequency. It was found that partial replacement plays an impo
The compound Fe0.5CoxMg0.95-xO where (x= 0.025, 0.05, 0.075, 0.1) was prepared via the sol-gel technique. The crystalline nature of magnesium oxide was studied by X-ray powder diffraction (XRD) analysis, and the size of the sample crystals, ranging between (16.91-19.62nm), increased, while the lattice constant within the band (0.5337-0.4738 nm) decreased with increasing the cobalt concentration. The morphology of the specimens was studied by scanning electron microscopy (SEM) which shows images forming spherical granules in addition to the presence of interconnected chips. The presence of the elements involved in the super
Copper zinc tin sulfide selenide, Cu2 ZnSn(S1−x Se x)4 , absorbers are promising earth-abundant and environmentally benign materials for low-cost photovoltaic applications. This study investigates the structural and optical properties of Cu 2 ZnSn(S1−x Se x)4 nanostructured thin films prepared by pulsed laser deposition using melt-quenched targets with selenium compositions x = 0.0–1.0. X-ray diffraction revealed that films with low selenium content remained amorphous, whereas higher selenium incorporation promoted the formation of polycrystalline kesterite–stannite phases with preferred orientations along (112), (200), (220), and (312). The crystallite size increased from 12.3 to 17.9 nm as selenium reached x = 1.0, indicating enha
... Show MoreThe synthesis of ligands with N2S2 donor sets that include imine, an amide, thioether, thiolate moieties and their metal complexes were achieved. The new Schiff-base ligands; N-(2-((2,4-diphenyl-3-azabicyclo[3.3.1]nonan-9-ylidene)amino)ethyl)-2-((2-mercaptoethyl)thio)-acetamide (H2L1) and N-(2-((2,4-di-p-tolyl-3-azabicyclo[3.3.1]nonan-9-ylidene)amino)ethyl)-2-((2-mercaptoethyl)thio) acetamide (H2L2) were obtained from the reaction of amine precursors with 1,4-dithian-2-one in the presence of triethylamine as a base in the CHCl3 medium. Complexes of the general formula K2<
Abstract Ternary Silver Indium selenide Sulfur AgInSe1.8S0.2 in pure form and with a 0.2 ratio of Sulfur were fabricated via thermal evaporation under vacuum 3*10-6 torr on glasses substrates with a thickness of (550) nm. These films were investigated to understand their structural, optical, and Hall Characteristics. X-ray diffraction analysis was employed to examine the impact of varying Sulfur ratios on the structural properties. The results revealed that the AgInSe1.8S0.2 thin films in their pure form and with a 0.2 Sulfur ratio, both at room temperature and after annealing at 500 K, exhibited a polycrystalline nature with a tetragonal structure and a predominant orientation along the (112) plane, indicating an enhanced de
... Show MoreThis study includes the preparation of the ferrite nanoparticles CuxCe0.3-XNi0.7Fe2O4 (where: x = 0, 0.05, 0.1, 0.15, 0.2, 0.25, 0.3) using the sol-gel (auto combustion) method, and citric acid was used as a fuel for combustion. The results of the tests conducted by X-ray diffraction (XRD), emitting-field scanning electron microscopy (FE-SEM), energy-dispersive X-ray analyzer (EDX), and Vibration Sample Magnetic Device (VSM) showed that the compound has a face-centered cubic structure, and the lattice constant is increased with increasing Cu ion. On the other hand, the compound has apparent porosity and spherical particles, and t
... Show MoreBulk AlxSb1-x samples were prepared with different x ratios (0.1, 0.3, 0.5, 0.7 and 0.9) by quenching technique. This was done throughout mixing the aluminum and antimony elements according to the proper atomic weight and put them in an evacuated quartz ampoule which then sealed and heated at 1273 K for five hours and left to cool in air. Thin films of AlxSb1-xwere prepared by using thermal evaporation under vacuum of 10-5 mbar on glass substrates at room temperature with deposition rate (10-15nm/min) at thickness of ∼ 500nm. The structures of AlxSb1-x bulk and thin films have been studied by X–ray diffraction technique. The results showed that all alloys have polycrystalline structures and the p
Aromaticity, antiaromaticity and chemical bonding in the ground (S0), first singlet excited (S1) and lowest triplet (T1) electronic states of disulfur dinitride, S2N2, were investigated by analysing the isotropic magnetic shielding, σiso(r), in the space surrounding the molecule for each electronic state. The σiso(r) values were calculated by state-optimized CASSCF/cc-pVTZ wave functions with 22 electrons in 16 orbitals constructed from gauge-including atomic orbitals (GIAOs). The S1 and T1 electronic states were confirmed as 11Au and 13B3u, respectively, through linear response CC3/aug-cc-pVTZ calculations of the vertical excitation energies for eight singlet (S1–S8) and eight triplet (T1–T8) electronic states. The aromaticities of S
... Show More