Asmari is the main productive reservoir in Abu Ghirab oilfield in the south-east part of Iraq. It has history production extends from 1976 up to now with several close periods. Recently, the reservoir suffers some problems in production, which are abstracted as water production rising with oil production declining in most wells. The water problem type of the field and wells is identified by using Chan's diagnostic plots (water oil ratio (WOR) and derivative water oil ratio (WOR') against time). The analytical results show that water problem is caused by the channeling due to high permeability zones, high water saturation zones, and faults or fracturing. The numerical approach is also used to study the water movement insi
... Show MoreAlthough many technological improvements are occurring in power production worldwide, power plants in third world countries are still using old technologies that are causing thermal pollution to the water bodies. Power facilities that dump hot water into water bodies are damaging aquatic life. In the study, the impact of the Al Dora thermal power plant on a nearby stretch of Tigris River in Baghdad city was assessed by measuring the temperature of the disposed of hot water in various cross-sections of the selected stretch of Tigris River, including measuring the thermal mixing length. The measurements were conducted in winter, spring, and summer. For field measurements, it was found that the impact of recovery distances
... Show MoreTwo‐dimensional buoyancy‐induced flow and heat transfer inside a square enclosure partially occupied by copper metallic foam subjected to a symmetric side cooling and constant heat flux bottom heating was tested numerically. Finite Element Method was employed to solve the governing partial differential equations of the flow field and the Local Thermal Equilibrium model was used for the energy equation. The system boundaries were defined as lower heated wall by constant heat flux, cooled lateral walls, and insulated top wall. The three parameters elected to conduct the study are heater length (7 ≤
Autorías: Suhair Meteab Munaf, Ali Abdulateef Ali, Mohannad Salman Dawood. Localización: Revista iberoamericana de psicología del ejercicio y el deporte. Nº. 4, 2022. Artículo de Revista en Dialnet.
The polymeric hydrogels composed of poly vinyl alcohol (m.wt 72000) and glutaraldehyde(5%,8% and 10%) , have been thermally prepared for the purpose of studying their swelling and drug release behavior . The swelling ratio was measured for all the hydrogel samples at 37°C, in three different media pH (1.2, 4.7 and 6.8) as a function of time. The results show that the maximum swelling ratios were arranged as follows :pH =6.8 > pH =4.7 > pH =1.2 hydrogels cross linked PVA showed a typical pH responsive behavior such as high pH has maximum swelling while low pH shows minimum swelling.
Six proposed simply supported high strength-steel fiber reinforced concrete (HS-SFRC) beams reinforced with FRP (fiber reinforced polymer) rebars were numerically tested by finite element method using ABAQUS software to investigate their behavior under the flexural failure. The beams were divided into two groups depending on their cross sectional shape. Group A consisted of four trapezoidal beams with dimensions of (height 200 mm, top width 250 mm, and bottom width 125 mm), while group B consisted of two rectangular beams with dimensions of (125 ×200) mm. All specimens have same total length of 1500 mm, and they were also considered to be made of same high strength concrete designed material with 1% volume fraction of steel fiber.
... Show MoreGlass Fiber Reinforced Polymer (GFRP) bars have gained popularity as a corrosion-resistant alternative to traditional steel reinforcement in Reinforced Concrete (RC) elements. This study investigates the flexural behavior of PRC panels reinforced with GFRP bars. The study variables included the GFRP reinforcement ratio and the number of embedded steel section distributions. Six concrete panels were fabricated, each measuring 2500 mm in length, with a rectangular cross-section of 750 mm in width and 150 mm in thickness. All panels were reinforced with GFRP bars and divided into two groups based on the reinforcement ratios of 0.532% and 0.266%. For each group, one panel served as the control specimen, while the remaining two were inte
... Show MoreThis paper describes flexural behavior of two spans continuous rectangular concrete beams reinforced with mild steel and partially prestressing strands, to evaluate using different prestressing level and prestressing area in continuous prestressed beams at serviceability and ultimate stages. Six continuous concrete beams with 4550 mm length reinforced with mild steel reinforcement and partially prestressed with two prestressing levels of (0.7fpy or 0.55fpy.) of and different amount of 12.7 mm diameter seven wire steel strand were used. Test results showed that the partially prestressed reinforced beams with higher prestressing level exhibited the narrowest crack width, smallest deflection and strain in both steel and concrete at ul
... Show MoreImproving the accuracy of load-deformation behavior, failure mode, and ultimate load capacity for reinforced concrete members subjected to in-plane loadings such as corbels, wall to foundation connections and panels need shear strength behavior to be included. Shear design in reinforced concrete structures depends on crack width, crack slippage and roughness of the surface of cracks.
This paper illustrates results of an experimental investigation conducted to investigate the direct shear strength of fiber normal strength concrete (NSC) and reactive powder concrete (RPC). The tests were performed along a pre-selected shear plane in concrete members named push-off specimens. The effectiveness of concrete compressiv
... Show More