In this study, the photodegradation of Congo red dye (CR) in aqueous solution was investigated using Au-Pd/TiO2 as photocatalyst. The concentration of dye, dosage of photocatalyst, amount of H2O2, pH of the medium and temperature were examined to find the optimum values of these parameters. It has been found that 28 ppm was the best dye concentration. The optimum amount of photocatalyst was 0.09 g/75 mL of dye solution when the degradation percent was ~ 96 % after irradiation time of 12 hours, while the best amount of hydrogen peroxide was 7μl/75 mL of dye solution at degradation percent ~97 % after irradiation time of 10 hours, whereas pH 5 was the best value to carry out the reaction at the highest degradation percent. In addition, temperature tested at range of (25-55) C˚, and it has been figured out which photodegradation percent of dye increase with raising temperature (degradation percent was ~ 98% after irradiation time of 4 hours at 55 C˚), and the activation energy of the reaction was calculated (34.8016 kJ/mole) from Arrhenius law. The thermodynamic functions ΔH#, ΔG#, and ΔS# were obtained, where ΔH# and ΔG# are positive value which means that the reaction is endothermic and non-spontaneous respectively, while ΔS# has a negative value, thus indicates that the reactants are more disordered than the excited intermediate formed. The kinetic of the reaction was studied, and it has been found that the photocatalytic reaction follows pseudo first order reaction.
Abstract
Locally natural occurring Iraqi rocks of Bauxite and Porcelanite (after pre calcinations at 1000oC for 1hr) were used, with the addition of different proportions of MgO and Al2O3, to prepare refractory materials. The effects of these additives on the physical and thermal properties of the prepared refractories were investigated.
Many batches of Bauxite/MgO, Bauxite/Al2O3, Bauxite/MgO/Al2O3, and Porcelanite/ MgO/Al2O3 were prepared. The mixture is milled and classified into different size fractions; fine (less than 45μm) 40%, middle (45-75μm) 40%, and coarse (75-106μm) 20% .
... Show MoreOrganizations adopt a number of procedures and instructions in their field of activities in order to aid their resources development and energies to serve their entrepreneurial orientations. This calls for preparing a range of mechanisms to mitigate the strictness and complexity of procedures. The ambiguity and severe complexity of procedures means acknowledging the loss in energy and this in turn impedes the hopes while in the same time weakens the enthusiasm in these organizations and an impedes the possibility to achieve continues innovation, thereby losing opportunities to the level of surrender to the risks and assuming them to be unconquered obstacles.
There
... Show MoreBackground: Entamoeba histolytica is the causative agent of amoebic dysentery and hepatic abscesses. Despite the efficacy of metronidazole in alleviating infectious diseases, the global dissemination of drug-resistant parasites raises the possibility that Punica granatum could serve as an effective natural alternative treatment. Objective: To evaluate the effect of P. granatum methanolic and aqueous extracts of various parts against E. histolytica trophozoites in an in vitro setting. Methods: Various concentrations (0.14, 0.7, 1.4, and 2.8 mg/ml) of P. granatum extracts of the flowers, leafs, peels, and seeds were chosen for this purpose. A culture medium containing 0.05x106/ml E. histolytica trophozoites was treated with different
... Show MoreThis research studies the effect of adding micro, nano and hybrid by ratio (1:1) of (Al2O3,TiO2) to epoxy resin on thermal conductivity before and after immersion in HCl acid for (14 day) with normality (0.3 N) at weight fraction (0.02, 0.04, 0.06, 0.08) and thickness (6mm). The results of thermal conductivity reveled that epoxy reinforced by (Al2O3) and mixture (TiO2+Al2O3) increases with increasing the weight fraction, but the thermal conductivity (k) a values for micro and Nano (TiO2) decrease with increasing the weight fraction of reinforced, while the immersion in acidic solution (HCl) that the (k) values after immersion more than the value in before immersion.