We aimed to examine the effect of amoxicillin and azithromycin suspensions on the microhardness of sliver-reinforced glass ionomer and nano-resin modified glass ionomer (GI). Method: Thirty discs (2mm height x 4mm diameter) of each type of GI were prepared, which were randomly assigned to amoxicillin, azithromycin, and artificial saliva groups. Microhardness was evaluated by Vickers hardness test before and after three immersion cycles. Results: The overall model (P < 0.001), before/after intervention (P < 0.001), intervention group (type of antibiotic) (P=0.013), and type of glass ionomer (P < 0.001) showed significant differences among study groups (P < 0.001). Post hoc test showed only non-significant before/after difference for Azithromycin and artificial saliva (control) groups regarding nano resinmodified GI. Conclusion: We found significant microhardness loss for sliver reinforced GI in comparison to nano resin-modified GI after the immersion cycles. Yet, sliver reinforced GI would have higher level of microhardness than nano resin-modified GI after the immersion cycles. Longer time studies are required to assess trend of microhardness loss
Dental caries (tooth decay) is one of the most prevalent infectious disease and although of multifactorial origin, Streptococcus mutans is considered the principal pathogen in its development (i.e. bacterial processes damage hard tooth structure (enamel, dentine and cementum), producing dental cavities (holes in the teeth). The bactericidal properties of the Nd:YAG laser has been researched analyzing its use in caries prevention and bacterial reduction. One hundred twenty five samples were collected from carious teeth and isolated bacteria were diagnosed using microscopic examination, culture, biochemical tests, and Api 20 strep system. The results of this study showed that a noticeable decrease in the viability of Streptococcus mutans w
... Show MoreABSTRACT Background: Bracket rebonding is a common problem in orthodontics which may result in many drawbacks. The aims of this study were to evaluate the effects of application of two enamel protective agents “Icon†and “ProSeal†on shear bond strength before and after rebonding of stainless steel orthodontic brackets using conventional orthodontic adhesive and to assess the site of bond failure. Materials and methods: Fifty sound extracted human upper first premolar teeth were selected and randomly divided into two equal groups; the first time bonding and the rebonding groups (n=30). Each group was subdivided into control, Icon and ProSeal subgroups. The enamel protective agents were applied after etching (precondi
... Show MoreBackground: Debonding orthodontic brackets and removal of residual bonding material from the enamel surface include critical steps that may cause enamel damage. The aim of the present study was to evaluate and compare the site of bond failure and enamel surface damage after debonding of three types of esthetic brackets (composite, ceramic, sapphire) bonded with light cure composite and resin-modified glass ionomer adhesive. Materials and methods: Seventy two maxillary premolars teeth were divided into three groups each group consisted of 24 teeth according to the type of brackets. Each group was subdivided into two subgroups (12 teeth for each) according to the bonding material that was used. After 7 days of bonding procedure, the brackets
... Show MoreProduction of the steroidal saponin digitonin in multiplied shoots of Digitalis purpurea , (var. Excelsior Mixed) has been achieved in vitro by two experiments. In the experiment 1, shoot tips ( 1cm length ) explants from the sterilized seedlings were excised and cultured on MS medium ( Murashige and Skoog medium) supplemented with 0.5 mg/L TDZ (thidiazuron) and cholesterol at the concentrations 0.0, 0.1, 0.3, 0.5, 1.0, 1.5, 2.0 or 4.0 mg/L. After 45 day, results showed that the treatment with 0.5 mg/L TDZ and 2.0mg/L cholesterol had a positive effected on increasing the dry weight of multiplied shoots and their production of digitonin when compared with other treatments, where this treatment gave 2
... Show MoreThis study involves the design of 24 mixtures of fiber reinforced magnetic reactive powder concrete containing nano Silica. Tap water has been used in mixing 12 of these mixtures, while the other 12 have been mixed using magnetic water. Nano Silica (NS) with ratios (1, 1.5, 2, 2.5 and 3) % were used. The results showed that the mixture containing 2.5%NS gives the highest compressive strength at age 7 days. Many different other tests were carried out, the results showed that the fiber reinforced magnetic reactive powder concrete containing 2.5% NS (FRMRPCCNS) has the higher bulk density, dynamic modulus of elasticity, ultrasonic pulse velocity electrical resistivity and lesser absorption than fiber reinforced
... Show MoreA total of 60 cotton swabs are collected from patients suffering from burn wound and surgical site infections admitted to Baghdad Teaching Hospital and Burn Specialist Hospital in Baghdad city during 9/2013 to 11/2013. All cotton swabs are cultured initially on blood agar and MacConkey agar and subjected for standard bacteriological procedures for bacteriological diagnosis. Twenty samples out of sixty are identified as Pseudomonas aeruginosa by conventional methods. The results of antibiotic susceptibility test illustrate that the antibiotics resistance rate of Pseudomonas aeruginosa isolates is as follows:100% (2020) for ceftriaxone, cefepime and carbencillin, 70% (14/20) for amikacin, 65%(13/20) for tobramycin, ceftazidim and gentamycin,
... Show MoreObjective(s): The world of dentistry is constantly evolving, and with the advent of 3D printing technology, the possibilities are endless. However, little is known about the effects of adding ZrO2 NPs to the denture base resin of 3D additive manufacturing technique.Aim of this study is to evaluate the behavior of resin which is used to 3D printing of denture base with the addition of ZrO2 NPs on denture adaptation property and diametral compression strength.Methods: 60 samples were printed, 30 disks for diametral compressive test and 30 denture base for denture adaptation test. Three groups per test (n=10). The control group for each test included unreinforced 3Dprinted denture base resin, and the other groups were reinforced with (2&
... Show MoreObjectives: Successful endodontic treatment outcome requires effective shaping and cleaning of root canals. This study aims to evaluate the smear layer removal after continuous chelation (CC) ) NaOCL\HEDP( and sequential chelation (SC) )NaOCL\EDTA( and their influence on the push-out bond strength (POBS) of Bio-C sealer. Materials and Methods: Palatal roots of the maxillary first molar (n=72) were divided into four groups (n=18) as follows: 3% NaOCL, SC: 3% NaOCL followed by 17% EDTA, CC: 3% NaOCL \9% HEDP and Distilled water. Thirty-two roots (n=8/group) were split longitudinally for smear layer evaluation using SEM. Forty roots were obturated with Guttapercha and Bio-C sealer using a single cone technique. Thre
... Show MoreThe presence of residual antibiotics in water results in the development of antibiotics resistant genes. The available wastewater treatment systems are not capable of removing such antibiotics from sewage. Thus, antibiotics need to be removed before the discharge of wastewater. Adsorption is among the promising techniques for the wastewater treatment to aid the removal of a wide range of organic and inorganic pollutants. The present work is a contribution to the search for an economical method for the removal of low concentrations of amoxicillin (AMX) from water by adsorption on water treatment residue, WTR, taken from a local drinking water facility. The chemical composition and the adsorptive characteristics of the material were first
... Show More