Nanocrystalline TiO 2 and CuO doped TiO 2 thin films were successfully deposited on suitably cleaned glass substrate at constant room temperature and different concentrations of CuO (0.05,0.1,0.15,0.2) wt% using pulse laser deposition(PLD) technique at a constant deposition parameter such as : (pulse Nd:YAG laser with λ=1064 nm, constant energy 800 mJ, with repetition rate 6 Hz and No. of pulse (500). The films were annealed at different annealing temperatures 423K and 523 K. The effect of annealing on the morphological and electrical properties was studied. Surface morphology of the thin films has been studied by using atomic force microscopes which showed that the films have good crystalline and homogeneous surface. The Root Mean Square value of thin films surface roughness is increased with the increase of annealing temperature. Also, the grain size increases with the increasing of CuO concentration and annealing. The temperatures dependence of the electrical conductivity and the activation energy at temperature ranging from (293-473) K of the as-deposited and films annealed at different annealing temperatures have been studied. The results show that as the film concentration of and conductivity increases, while the activation energy (Ea 1 , E a2 ) decreases. Both, the annealing and composition effects on Hall constant, charge carrier concentration, Hall mobility were investigated. Hall Effect measurements show that all films have n- type charge carriers, and the concentration and annealing increase carriers concentration while the mobility decreases.
The technical of Flame Thermal Spray had been used in producing a cermet
composite based on powders of stabilized zirconium oxide containing amount of
Yatteria oxide (ZrO2- 8Y2O3) reiforced by minerals powders of bonding material
(Ni-Cr- Al- Y) in different rates of additions (25, 35, 50) on stainless steel base type
(304) after preparing it by the way of Grit Blasting.
Before heat treatment, the coated cermet layers were characterized for porosity
and electric resistivity. All samples were heat treated in vacuum furnace at different
temperature and times. The physical tests had been operated after heat treatment
and gave best results especially porosity, which found to be reduced dramatically
and producing hig
In this research thin films from SnO2 semiconductor have been prepared by using chemical pyrolysis spray method from solution SnCl2.2H2O at 0.125M concentration on glass at substrate temperature (723K ).Annealing was preformed for prepared thin film at (823K) temperature. The structural and sensing properties of SnO2 thin films for CO2 gas was studied before and after annealing ,as well as we studied the effect temperature annealing on grain size for prepared thin films .
The optical energy gap(Eopt) and the width of the tails of localized states in the band gap (?E) for Se:2%Sb thin films prepared by thermal co-evaporation method as a function of annealing temperature are studied in the photon energy range ( 1 to 5.4)eV.Se2%Sb film was found to be indirect transition with energy gap of (1.973,2.077, 2.096, 2.17) eV at annealing temperature (295,370,445,520)K respectively. The Eopt and ?E of Se:2%Sb films as a function of annealing temperature showed an increase in Eopt and a decrease in ?E with increasing the annealing temperature. This behavior may be related to structural defects and dangling bonds.
This research examines the phenomenon of the Arabic language repeated in the Qur'an and poetry, as some morphological formulas are valid in their uses and indications in more than one way. search).
The Cu2SiO3 composite has been prepared from the binary compounds (Cu2O, and SiO2) with high purity by solid state reaction. The Cu2SiO3 thin films were deposited at room temperature on glass and Si substrates with thickness 400 nm by pulsed laser deposition method. X-ray analysis showed that the powder of Cu2SiO3 has a polycrystalline structure with monoclinic phase and preferred orientation along (111) direction at 2θ around 38.670o which related to CuO phase. While as deposited and annealed Cu2SiO3 films have amorphous structure. The morphological study revealed that the grains have granular and elliptical shape, with average diameter of 163.63 nm. The electrical properties which represent Hall effect were investigated. Hall coeffici
... Show MoreA polycrystalline CdTe film has been prepared by thermal evaporation technique on glass substrate at substrate temperature 423 K with 1.0 m thicknesses. The film was heated at various annealing temperature under vacuum (Ta =473, 523 and K). Some of physical properties of prepared films such as structural and optical properties were investigated. The patterns of X-ray diffraction analysis showed that the structure of CdTe powder and all films were polycrystalline and consist of a mixture of cubic and hexagonal phases and preferred orientation at (111) direction.
The optical measurements showed that un annealed and annealed CdTe films had direct energy gap (Eg). The Eg increased with increasing Ta. The refractive index and the real p
The researchers have recently noticed the interest in the problem of overweight and how to find solutions to it until it is now at the forefront in terms of innovating various and different methods and treatment methods, and the interest in developing health fitness is one of the most important requirements of physical activity for the trainees, which led to the multiplicity of sports activities that promote the health aspect For the individual, in addition to the aesthetic aspect, the problem lies in not adopting training programs according to codified scientific foundations aiming, in addition to reducing weight, to raise the general health level of the trainee participating in fitness institutes, as the trainers do not follow the
... Show MoreIndium Antimonide (InSb) thin films were grown onto well cleaned glass substrates at substrate temperatures (473 K) by flash evaporation. X-ray diffraction studies confirm the polycrystalline of the films and the films show preferential orientation along the (111) plane .The particle size increases with the increase of annealing time .The transmission spectra of prepared samples were found to be in the range (400-5000 cm-1 ) from FTIR study . This indicates that the crystallinity is improved in the films deposited at higher annealing time.