The effect of the concentration of the colloidal nanomaterial on their optical limiting behavior is reported in this paper. The colloids of sliver nanoparticles in deionized water were chemically prepared for the two concentrations (31 ppm and 11ppm). Two cw lasers (473 nm Blue DPSS laser and 532 nm Nd:YAG laser) are used to compare the optical limiting performance for the samples. UV–visible spectrophotometer, transmission electron microscope (TEM) and Fourier Transformation Infrared Spectrometer (FTIR) were used to obtain the characteristics of the sample. The nonlinear refractive index was calculated to be in the order of 10-9 cm2/W. The results demonstrate that the observed limiting response is significant for 532nm. In addition, t
... Show MoreThe map of permeability distribution in the reservoirs is considered one of the most essential steps of the geologic model building due to its governing the fluid flow through the reservoir which makes it the most influential parameter on the history matching than other parameters. For that, it is the most petrophysical properties that are tuned during the history matching. Unfortunately, the prediction of the relationship between static petrophysics (porosity) and dynamic petrophysics (permeability) from conventional wells logs has a sophisticated problem to solve by conventional statistical methods for heterogeneous formations. For that, this paper examines the ability and performance of the artificial intelligence method in perme
... Show MoreThe effect of approaching nozzle jet from the deposition surface
on structural, optical and morphology properties of copper oxide thin
films was studied. The film was prepared by homemade fully
computerized CNC spray pyrolysis deposition technique at
preparations speed (3, 4, 5, and 6 mm/sec). The repeated line mode
was used at deposition temperature equal 450 °C whereas the
spraying time was in the range of (15-30 min) according to the
deposition speed. The film exhibit polycrystalline structure with
preferred orientation along (-111), (022) and (011), (002) at a 2θ
value of (35.63o) and (38.8o) respectively. Optical band gaps were
recorded at these speed shows variance in value from (1.53-2.08 eV).
Fi
Zinc Oxide thin film of 2 μm thickness has been grown on glass substrate by pulsed laser deposition technique at substrate temperature of 500 oC under the vacuum pressure of 8×10-2 mbar. The optical properties concerning the absorption, and transmission spectra were studied for the prepared thin film. From the transmission spectra, the optical gap and linear refractive index of the ZnO thin film was determined. The structure of the ZnO thin film was tested with X-Ray diffraction and it was formed to be a polycrystalline with many peaks.
The effect of adding different volume of coumarin dye (5, 15, 25 and 35) ml on optical properties of Poly (Methyl Meth Acrylate) was studied. Films of pure PMMA and PMMA with different volume of coumarin dye (5, 15, 25 and 35) ml were prepared using the casting technique. Transmission and absorption of the films were measured by using UV-VIS spectrometer technique type (100 Conc), in order to assess the type of transmission which was found an indirect transition. An optical energy gap of pure PMMA is (4.95e v) and after adding coumarin with volume (25, 35) ml, the energy gap for PMMA decrease by (0.05) compere to pure PMMA films and addition energy gap appear equal to (4.1 e v). It was found that the absorption coefficient, extinction coeff
... Show MoreThe technical of Flame Thermal Spray had been used in producing a cermet
composite based on powders of stabilized zirconium oxide containing amount of
Yatteria oxide (ZrO2- 8Y2O3) reiforced by minerals powders of bonding material
(Ni-Cr- Al- Y) in different rates of additions (25, 35, 50) on stainless steel base type
(304) after preparing it by the way of Grit Blasting.
Before heat treatment, the coated cermet layers were characterized for porosity
and electric resistivity. All samples were heat treated in vacuum furnace at different
temperature and times. The physical tests had been operated after heat treatment
and gave best results especially porosity, which found to be reduced dramatically
and producing hig
Porous silicon (PS) layers were formed on n-type silicon (Si) wafers using Photo- electrochemical Etching technique (PEC) was used to produce porous silicon for n-type with orientation of (111). The effects of current density were investigated at: (10, 20, 30, 40, and50) mA/cm2 with etching time: 10min. X-ray diffraction studies showed distinct variations between the fresh silicon surface and the synthesized porous silicon. The maximum crystal size of Porous Silicon is (33.9nm) and minimum is (2.6nm) The Atomic force microscopy (AFM) analysis and Field Emission Scanning Electron Microscope (FESEM) were used to study the morphology of porous silicon layer. AFM results showed that root mean square (RMS) of roughness and the grain size of p
... Show MoreFaujasite type NaY zeolite catalyst was prepared from locally available kaolin, then the prepared NaY zeolite have been modified by exchanging of sodium ion with ammonium to produce NH4Y zeolite. NH4Y zeolite was converted to HY zeolite by ion exchanging with oxalic acid. Zinc and nickel promoters have been added to the prepared HY zeolite catalyst, and the effect of these promoters on the catalytic activity of the prepared HY catalyst was studied in fluid catalytic cracking process using light gas oil as a feedstock. The experimental results show that the promoted catalyst gives higher gas oil conversion and gasoline yield than HY zeolite catalyst at the same reaction temperature and WHSV. It was also found that the promoted catalyst gi
... Show MoreIn this study, the photodegradation of Congo red dye (CR) in aqueous solution was investigated using Au-Pd/TiO2 as photocatalyst. The concentration of dye, dosage of photocatalyst, amount of H2O2, pH of the medium and temperature were examined to find the optimum values of these parameters. It has been found that 28 ppm was the best dye concentration. The optimum amount of photocatalyst was 0.09 g/75 mL of dye solution when the degradation percent was ~ 96 % after irradiation time of 12 hours, while the best amount of hydrogen peroxide was 7μl/75 mL of dye solution at degradation percent ~97 % after irradiation time of 10 hours, whereas pH 5 was the best value to carry out the reaction at the highest deg
... Show More