Non-orthogonal Multiple Access (NOMA) is a multiple-access technique allowing multiusers to share the same communication resources, increasing spectral efficiency and throughput. NOMA has been shown to provide significant performance gains over orthogonal multiple access (OMA) regarding spectral efficiency and throughput. In this paper, two scenarios of NOMA are analyzed and simulated, involving two users and multiple users (four users) to evaluate NOMA's performance. The simulated results indicate that the achievable sum rate for the two users’ scenarios is 16.7 (bps/Hz), while for the multi-users scenario is 20.69 (bps/Hz) at transmitted power of 25 dBm. The BER for two users’ scenarios is 0.004202 and 0.001564 for
... Show MoreIn this research ,Undoped Nio and 1%Li doped Nio thin films were deposited utilizing chemical spray pyrolysis on the glass substrates heated (450C). The effects of non-thermal plasma on the structural and optical properties were studied. XRD measurement shows that Nio and Nio:1%Li films were found to be polycrystalline and have cubic structure with a preferred orientation (111). Decreased crystal size after exposure especially at (7) sec. AFM data indicate that the surface roughness average and (RMS) values of the prepared doped films are increasing after exposure to plasma, the transmittance increases after doped samples exposure to plasma, it was found that the energy gap value decreased when doped samples exposure to plasma, also, thickn
... Show MoreThin film technology is one of the most important technologies
that have contributed to the development of semiconductors and their
applications in several industrial fields. The Iron Oxides (Fe20) and
(Co3O4) thin films and their applications are of importance, in that these
two materials are considered as important industrial materials, and used
in spectrally selective coating, temperature sensors, resistive heaters, and
photo cells.
Thin films of Iron Oxide (Fe20,), Cobalt Oxide (Co304) and
their mixtures in different ratios (75:25, 50:50, 25:75) were prepared by
the method of chemical spray pyrolysis deposition at different thicknesses
(77s t S200) nm on cover-glass substrates: thickness of (1) mm at
In this research , pure Cadmium Oxide thin films were prepared by thermal evaporation Under vacuum method , where pure cadmium metal was deposited on glass Substrate in Room temperature (300K) at thickness (400 ± 30) nm with Deposition rate(1.1 ± 0.1) nm/sec And then we oxidize a pure cadmium Film in Temperature ( 350ºC ) for one hour with existence air flow. This research contained study of the influence of doping process by Tin metal (Sn) with two different ratios (1,3) % at substrate temperature (473K ) on th
... Show MoreAfter this systematic presentation of the phenomenon of rotation of formulas, ie the construction of the verb and the verb, and the narrated narratives therein differed among the readers, it became clear to us how the difference was clear between reading and the other, and how readers have varied in their readings of the verb, As we have noted through our modest research that the phenomenon of building the verb for the actor and the effect have included the act of both past and present tense, and not limited to a specific time, and this difference in reading was not limited to a particular environment, but beyond To more than one environment This is evidenced by the readings of various readers from the environment of Kufa, Basra, Mecca,
... Show More(Cu1-x,Agx)2ZnSnSe4 alloys have been fabricated with different Ag content(x=0, 0.1, and 0.2) successfully from their elements. Thin films of these alloys have been deposited on coring glass substrate at room temperature by thermal evaporation technique under vacuum of 10-5Torr with thickness of 800nm and deposition rate of 0.53 nm/sec. Later, films have been annealed in vacuum at (373, and 473)K, for one hour. The crystal structure of fabricated alloys and as deposited thin films had been examined by XRD analysis, which confirms the formation of tetragonal phase in [112] direction, and no secondary phases are founded. The shifting of main polycrystalline peak (112) to lower Bragg’s angle as compared to Cu2ZnSnSe4 angle refers to incorpora
... Show MoreIn this work, SnO2 and (SnO2)1-x(ZnO)x composite thin films with different ZnO atomic ratios (x=0, 5, 10, 15 and 20%) were prepared by pulsed laser deposition technique on clean glass substrates at room temperature without any treatment. The deposited thin films were characterized by x-ray diffraction atomic force microscope and UV-visible spectrophotometer to study the effect of the ZnO atomic ratio on their structural, morphological and optical properties. It was found that the crystallinety and the crystalline size vary according to ZnO atomic ratio. The surface appeared as longitudinal structures which was convert to spherical shapes with increasing ZnO atomic ratio. The optical trans
... Show MoreSpray pyrolysis technique was subjected to synthesized (SnO2)1-x (TiO2: CuO) x Thin films on different substrates like glass and single crystal silicon using. The structure of the deposited films was studied using x-ray diffraction. A more pronounced diffraction peaks of SnO2 while no peaks of (CuO , TiO2 ) phase appear in the X-ray profiles by increasing of the content of (TiO2 , CuO) in the sprayed films. Mixing concentration (TiO2 , CuO) influences on the size of the crystallites of the SnO2 films ,the size of crystallites of the spray paralyzed oxide films change in regular manner by increasing of (TiO
... Show MoreIn this research, we studied the structural properties of SnO2 films nanostructure which prepared by chemical spray pyrolysis method at room temperature on the rules of glass heated (400oC) with rate of spraying (2.5 ml/ min). The effect of annealing temperaturs (450,500,550,600 and 650oC) for two hours on those properties has been indicated. The results of x-ray diffraction showed that all of the prepared films were polycrystalline with tetragonal type and orientation was (110) for all models before and after annealing, and the annealing led to an increase in the grain size. The full width at half maximum (FWHM) values of the (110) peaks of the films decreased from 1.492o to 1.064o with increasing annealing temperature .The surface morp
... Show More