In this work, (Cu1-xAgx)2ZnSnSe4 (CAZTSe) alloys with various silver content (x= 0.0, 0.1and 0.2) have been prepared by reacting their high purity elements (Cu, Ag, Zn, Sn and Se) in an evacuated quartz tube under pressure of 10 -3Torr. The composition of the prepared alloys was determined by energy dispersive X-ray spectroscopy (EDXS) analysis, the results were close to the theoretical values. CAZTSe thin films with a thickness of 800 nm were deposited by thermal evaporation technique on glass substrates at room temperature (RT) with a deposition rate of 0.53nm/sec. Similarly, CdS thin films were deposited with a thickness of 100 nm on the same substrates at RT with a deposition rate of 0.3nm/sec from ready-made CdS alloy powder. All prepared thin films were annealed at temperatures of 373K and 473K under vacuum (10-3Torr) for 1h. X-ray analysis showed that all CAZTSe alloys and their thin films were polycrystalline and have the tetragonal structure with preferential orientation in the (112) direction, while all thin CdS films were polycrystalline and have the hexagonal structure with preferential orientation in the (002) direction. The scanning electron microscopy (SEM) technique was used to study the surface morphology of all prepared CAZTSe films, while the atomic force microscopy (AFM) technique was used to study the surface topography of all prepared CAZTSe and CdS films. SEM results revealed that CAZTSe films had uniform surface features with irregular sized grains, while AFM results showed that the surface roughness and the average grain size of CAZTSe and CdS thin films increased with increasing Ag content for CAZTSe thin films and annealing temperature for CAZTSe and CdS thin films. The absorbance and transmittance spectra for CAZTSe and CdS thin films were recorded in the wavelength ranges of (400-1100) nm and (350- 1100) nm, respectively. Optical measurements showed that all CAZTSe and CdS thin films have a direct energy gap (Eg) that decreased with increasing silver content for CAZTSe thin films and annealing temperature (Ta) for both types of prepared thin films, so it decreased from 1.73 eV to1.5 eV when x content increased from 0.0 to 0.2 and decreased from 1.5 eV to1.46 eV and from 2.47 eV to 2.38 eV when Ta increased from RT to 473K for CAZTSe thin films with x content equal to 0.2 and CdS thin films, respectively. Optical constants such as extinction coefficient, refractive index and dielectric constant were calculated for all prepared thin films. The measurements of the electrical properties for prepared films showed that the D.C electrical conductivity (σd.c) increased with increasing Ag content for CAZTSe thin films and annealing temperature for both types of thin films. So the electrical conductivity changed from 1.1276*10-2 (Ω.cm)-1 to 28.9266*10-2 (Ω.cm)-1 when x changed from 0.0 to 0.2 and changed from 28.9266*10-2 (Ω.cm)-1 to 57.4599*10-2 (Ω.cm)-1 and from 4.0476*10-4 (Ω.cm)-1 to 9.4227*10-4 (Ω.cm)-1 when Ta changed from RT to 473K for CAZTSe thin films with Ag content equal to 0.2 and CdS thin films, respectively. The prepared thin films have two activation energies (Ea1 & Ea2) in the temperature ranges of (318-488)K and (313-443)K for CAZTSe and CdS films, respectively. The results of Hall effect for CAZTSe thin films showed that all films were of acceptor type and the concentration of holes in them decreased with increasing silver content and annealing temperature, while CdS thin films were of donor type and the concentration of electrons in them increased with increasing annealing temperature. In this research, solar cells were fabricated from CdS/CAZTSe/Si structurThe C-V measurements revealed that all prepared heterojunctions were of the abrupt type and the junction capacitance and carrier concentration reduced while the width of depletion region and the built-in potential increased with increasing the silver content and annealing temperature. The current-voltage characteristics under dark condition of CAZTSe heterojunctions showed that both the ideality factor and saturation current decreased with increasing Ag content and annealing temperature. While,The current-voltage characteristics under dark condition of CAZTSe heterojunctions showed that both the ideality factor and saturation current decreased with increasing Ag content and annealing temperature. While, the current-voltage measurements under illumination showed that the performance of heterojunction solar cell improved with increasing Ag content and annealing temperature. The result indicated that the prepared solar cell with 0.2 Ag content and 473K annealing temperature exhibited the highest efficiency (η = 2.827%) compared to other prepared solar cells
Erratum for Organic acid concentration thresholds for ageing of carbonate minerals: Implications for CO2 trapping/storage.
This study depicts the removal of Manganese ions (Mn2+) from simulated wastewater by combined electrocoagulation/ electroflotation technologies. The effects of initial Mn concentration, current density (C.D.), electrolysis time, and different mesh numbers of stainless steel screen electrodes were investigated in a batch cell by adopting Taguchi experimental design to explore the optimum conditions for maximum removal efficiency of Mn. The results of multiple regression and signal to noise ratio (S/N) showed that the optimum conditions were Mn initial concentration of 100 ppm, C.D. of 4 mA/cm2, time of 120 min, and mesh no. of 30 (wire/inch). Also, the relative significance of each factor was attained by the analysis of variance (ANO
... Show MoreBackground: Ultrasonography has been used to examine the thickness of the lower uterine segment in women with previous cesarean sections in an attempt to predict the risk of scar dehiscence during subsequent pregnancy. The predictive value of such measurement has not been adequately assessed. Objectives: To correlate lower uterine segment thickness measured by trans abdominal ultrasound in pregnant women with previous cesarean section with that measured during cesarean section by caliper and to find out minimum lower uterine segment thickness indicative of integrity of the scar.Methods: A prospective observational study at Elwyia Maternity Teaching Hospital, from January 2011 to January 2012. A total of 143 women were enrolled in the stu
... Show MoreMJ Abbas, AK Hussein, Journal of Physical Education, 2019
Objectives: To determine the effectiveness of the instructional program on patients’ knowledge about home safety while receiving anti-cancer treatment at Al- Karama Teaching Hospital in Al-Kut City.
Methodology: A quasi-experimental design is conducted through the application of a pre-test and post-test approach for the study and control groups from February 5th, 2020 to April 25th, 2020. A non–probability (purposive) sample of (50) patients treated at the Blood Disease and Oncology Center is selected and divided into two groups. Each group contains (25) patients as control and study groups. An instrument is constructed that is comprised of two parts; t
... Show MoreObjective: The aims of present study to detect the effectiveness of instruction program of non-pharmacological guideline on blood pressure and laboratory test.
Methodology: A pre-experimental study was conducted in Al-Sader Teaching Hospital from 8th of September 2019 to 25th of May 2020, in order to find out the effectiveness of instruction program concerning non-pharmacological guideline on controlling essential hypertension among patients. A non- probability (purposive sample) of 50 patients with essential hypertension is selected. Those patients are already diagnosed with Essential Hypertension
... Show MoreA new, simple, sensitive and fast developed method was used for the determination of methyldopa in pure and pharmaceutical formulations by using continuous flow injection analysis. This method is based on formation a burgundy color complex between methyldopa andammonium ceric (IV) nitrate in aqueous medium using long distance chasing photometer NAG-ADF-300-2. The linear range for calibration graph was 0.05-8.3 mmol/L for cell A and 0.1-8.5 mmol/L for cell B, and LOD 952.8000 ng /200 µL for cell A and 3.3348 µg /200 µL for cell B respectively with correlation coefficient (r) 0.9994 for cell A and 0.9991 for cell B, RSD % was lower than 1 % for n=8. The results were compared with classical method UV-Spectrophotometric at λ max=280 n
... Show More