Crude oil is one of the most important sources of energy in the world. To extract its multiple components, we need oil refineries. Refineries consist of multiple parts, including heat exchangers, furnaces, and others. It is known that one of the initial operations in the refineries is the process of gradually raising the temperature of crude oil to 370 degrees centigrade or higher. Hence, in this investigation the focus is on the furnaces and the corrosion in their tubes. The investigation was accomplished by reading the thickness of the tubes for the period from 2008 to 2020 with a test in every two year, had passed from their introduction into the work. Where the thickness of more than one point was measured on each tube in the same row and the corrosion rate was extracted for three furnaces, starting from the area of heat transfer by radiation to the heat transfer area of the convection in three different operating units. It was found that the highest percentage corrosion value between the standard tube thickness and the thickness of conduction position was 37% with the conduction zone, and 31% with radiation zone. There, the tubes specification was tested. Five percent Cr-0.5 Moly and the temperature of radiation zone was 578 °C to 613 °C and the stack temperature was 410 °C to 450 °C. So, the results show that the maximum erosion occur at the convection zone.
Hydro cracking of heavy oil is used in refinery to produce invaluable products. In this research, a model of hydro cracking reactor has been used to study the behavior of heavy oil in hydro cracking under the conditions recommended by literature in terms lumping of feed and products. The lumping scheme is based on five lumps include: heavy oil, vacuum oil, distillates, naphtha and gases. The first order kinetics was assumed for the conversion in the model and the system is modeled as an isothermal tubular reactor. MATLAB 6.1 was used to solve the model for a five lump scheme for different values of feed velocity, and temperature.
As one type of heating furnaces, the electric heating furnace (EHF) typically suffers from time delay, non-linearity, time-varying parameters, system uncertainties, and harsh en-vironment of the furnace, which significantly deteriorate the temperature control process of the EHF system. In order to achieve accurate and robust temperature tracking performance, an integration of robust state feedback control (RSFC) and a novel sliding mode-based disturbance observer (SMDO) is proposed in this paper, where modeling errors and external disturbances are lumped as a lumped disturbance. To describe the characteristics of the EHF, by using convection laws, an integrated dynamic model is established and identified as an uncertain nonlinear second ord
... Show MoreThe corcosion behoviour of Aluminum bronze in sodium chloride solution has been studied ^tentiostatically at five temperatures in the range 293-313K.The corrosion potential shifted to more negative values with increasing temperature. The corrosion current density increased with increasing temperature. Values of Tal'el slopes and the transfer coefficients indicated hydrogen evolution reaction to occur at the cathode and mainly the dissolution at the anode.Benzotriazole (BTA) had an inhibiting effect ??? the corrosion of the Al-bronze in deaerated NaCl solution at a concentration (1*10'?- IxlO‘1) mol dm'^ over the temperature range 293-313K. Values of the protection efficiency and kinetics parameters were obtained from the corrosion current
... Show MoreWater injection equipments such as pipelines, which are used in the second recovery of oil in the Al-Ahdeb wells, suffer from the corrosion in water during maintaining vacuum deoxygenated tower that used to decrease concentration of the dissolved oxygen gas in the water from 6.2-9.1 ppm to o.5 ppm. This study involved calculation the corrosion rates of the internal surfaces of the pipelines either during operation of the vacuum unit or when the tower out of operation. Finally, find the solution by one of the following suggestions. In the first suggestion removal of the dissolved O2 from water is achieved by increasing the dosage of the oxygen scavenger (sodium sulphite). The second suggestion involves re
... Show MoreWater injection equipments such as pipelines, which are used in the second recovery of oil in the Al-Ahdeb wells, suffer from the corrosion in water during maintaining vacuum deoxygenated tower that used to decrease concentration of the dissolved oxygen gas in the water from 6.2-9.1 ppm to o.5 ppm. This study involved calculation the corrosion rates of the internal surfaces of the
pipelines either during operation of the vacuum unit or when the tower out of operation. Finally, find the solution by one of the following suggestions. In the first suggestion removal of the dissolved O2 from water is achieved by increasing the dosage of the oxygen scavenger (sodium sulphite). The second suggestion involves removing the dissolved O2 from w
The petroleum industry, which is one of the pillars of the national economy, has the potential to generate vast wealth and employment possibilities. The transportation of petroleum products is complicated and changeable because of the hazards caused by the corrosion consequences. Hazardous chemical leaks caused by natural disasters may harm the environment, resulting in significant economic losses. It significantly threatens the aim for sustainable development. When a result, determining the likelihood of leakage and the potential for environmental harm, it becomes a top priority for decision-makers as they develop maintenance plans. This study aims to provide an in-depth understanding of the risks associated with oil and gas pipeli
... Show MoreThis paper studies the influence of temperature on the corrosion rate of coated AA6111 aluminum alloy used in vehicle bodies under static and vibration states. The vibration test system was collected laboratory and used for testing of five different types of paints (EASI, Numix, Lesonal, DENSO and Polaron paints) in the 5 % NaCl solution using immersion test method. Lesonal paint provided the best corrosion protection, while DENSO paints show large values of corrosion rate, other coatings exhibit moderate values. Model of paints corrosion was developed to characterize the corrosion processes occur at the surfaces. It is found that corrosion rate obtained at vibration cases is larger than static cases and vibration effect
... Show MoreWe have studied theoretically the response of atomic three- level cascade scheme
of rubidium vapor to a strong laser under conditions in which electromagnetically
induced transparency would be induced on a weak probe beam. We show that the
medium that is an opaque to a probe laser can, by applying both lasers
simultaneously, be made transparent.
Different cooking conditions were examined for aluminum content in food cooked while wrapped with aluminum foil. The influence of each anticipated factor (the acidity of the cooking medium, type of acids normally used in cuisines namely acetic and tartaric acids, various cooking temperatures, influence of the presence of sodium chloride salt, the effect of cooking oil, and the length of time of cooking) was studied thoroughly as a function of aluminum degraded out of the aluminum foils to the medium. The experimental samples were digested with nitric acid upon fulfillment of examining each factor separately before quantifying aluminum with the sensitive technique of atomic absorption spectroscopy. The outcomes of the study have shown that t
... Show MoreA metal mandrel was designed for manufacturing the cathodes of high power electron tube ( Tetrode ) used in broadcasting transmitting tubes type TH558 and CQS200.The cathodes were manufactured in the present work from thoriated tungsten wires ( 2? ThO2- W) with different diameters .These cathodes were carbonized in sequences of processes to determine the carbonization parameters (temperature, pressure, time, current and voltage).Then the carbonized cathodes dimension were accurately measured to determine the deviation due to the high temperature distortion effect at about 1800°C .the distorted cathodes due to the carbonization process was treated when it was subjected inside the vacuum chamber and heat treated again .The carbonized cat
... Show More