The studies on unbonded post-tensioned concrete members strengthened with Carbon Fiber Reinforced Polymers (CFRPs) are limited and the effect of strengthening on the strain of unbonded pre-stressed steel is not well characterized. Estimating the flexural capacity of unbound post-tensioned members using the design methodology specified in the design guidelines for FRP strengthening techniques of bonded post-tensioned members does not provide a reliable evaluation. This study investigates the behavior of unbonded post-tensioned concrete members with partial strand damage (14.3% and 28.6% damage) and strengthened with CFRP laminates using a near-surface mounted technique with and without U-wrap anchorages. The experimental results showed that the use of CFRP laminates significantly affects strand strain, especially with the use of anchors. The CFRP reinforcement affected flexural strength, crack width, and midspan deflection. However, the flexural stiffness of strengthened members during the serviceability phases is critical as strand damage ratios increase. In comparison with the nondamaged girder, the NSM-CFRP laminates enhanced the flexural capacity by 11% and 7.7% corresponding to strand damage of 14.3% and 28.6% respectively. Additionally, semiempirical equations were proposed to predict the actual strain of unbonded strands whilst considering the effects of FRP laminates. The suggested equations are simple to apply and provide accurate predictions with little variance.
Moisture-induced damage is a serious problem that severely impairs asphaltic pavement and affects road serviceability. This study examined numerous variables in asphalt concrete mixtures to assess their impact on moisture damage resistance. Mix design parameters such as the asphalt content (AC) and aggregate passing sieve No. 4 (PNo. 4) were considered as variables during this study. Additionally, hydrated lime (HL) was utilized as a partial substitute for limestone dust (LS) filler at 1.5% by weight of the aggregate in asphalt concrete mixtures for the surface layer. This study also investigated the potential enhancement of traditional asphalt binders and mixtures by adding nano-additives, specifically nano-silica oxide (NS) and na
... Show MoreThe aim of this work is to study the effect of mud compositions on it’s rheological behavior under high temperature conditions. Seventeen samples of five types of water base mud in which (fresh water bentonite mud. Lignosulphonate mud, gypsum mud, polymer mud, and salt saturated mud) were tested with different temperatures using the fann viscometer model 50-c. All the tested samples, except the fresh water bentonite mud, have the same trend reduction in both plastic viscosity and yield point with increasing temperature. Six rheological models has been adapted: Bingham plastic, power law, Casson model represent the laboratory data accurately
Recycling process presents a sustainable pavement by using the old materials that could be milled, mixed with virgin materials and recycling agents to produce recycled mixtures. The objective of this study is to evaluate the impact of water on recycled asphalt concrete mixtures, and the effect of the inclusion of old materials into recycled mixtures on the resistance of water damage. A total of 54 Marshall Specimens and 54 compressive strength specimens of (virgin, recycled, and aged asphalt concrete mixtures) had been prepared, and subjected to Tensile Strength Ratio test, and Index of Retained Strength test. Four types of recycling agents (used oil, oil + crumb rubber, soft grade asphalt cement, and asphalt cement + Su
... Show MoreThe aim of this study is to determine the flexural properties of steel fiber as a metal fiber and polyester resin as a matrix. The steel fibers were added to polyester resin at the various fiber volume fractions of 5, 10, and 15% steel fiber, and with different fiber orientations such as woven steel fiber type (0-45) ° and woven steel fiber type (0-90) ° indicate. Hand layup processes in these experiments were used to produce specimens test with the curing time of 24 hr. for the composite at room temperature. The results show that the flexural strength and flexural modulus values for 15 % vol.of woven steel fiber composite type (0-90) ° are (210MPa) and (2.29GPa( respectively. The results above indicate that the woven steel fiber (0-9
... Show MoreThis study investigates the impact of varying glass fiber-reinforced polymer (GFRP) stirrup spacing on the performance of doubly GFRP-reinforced concrete beams. The research focuses on assessing the behavior of GFRP-reinforced concrete beams, including load-carrying capacity, cracking, and deformability. It explores the feasibility and effectiveness of GFRP bars as an alternative to traditional steel reinforcement in concrete structures. Six concrete beams with a cross-section of 300 mm (wide) × 250 mm (deep), simply supported on a 2100 mm span, were tested. The beams underwent four-point bending with two concentrated loads applied symmetrically at one-third of the span length, resulting in a shear span (a)-to-depth (h) ratio of 2.
... Show MoreChlorine disinfection is a globally used method to ensure the safety of drinking water. However, it has not always been successful against viruses and, therefore, it is important to find new methods to disinfect water. Seventeen different coliphages were isolated from the treated municipal wastewater. These coliphages and MS2 were treated with different dosages of chlorine in drinking water, and a combined chlorine/ultraviolet irradiation treatment for the chlorine-resistant coliphages. Chlorine disinfection with 0.3–0.5 mg/L total chlorine (free Cl-dosage 0.12–0.21 mg/L) for 10 min achieved 2.5–5.7 Log10-reductions for 11 sensitive coliphages. The six most resistant coliphages showed no reduction with these chlorine concentra
... Show MoreThe main objective of this study is to characterize the main factors which may affect the behavior of segmental prestressed concrete beams comprised of multi segments. The 3-D finite element program ABAQUS was utilized. The experimental work was conducted on twelve simply supported segmental prestressed concrete beams divided into three groups depending on the precast segments number. They all had an identical total length of 3150mm, but each had different segment numbers (9, 7, and 5 segments), in other words, different segment lengths. To simulate the genuine fire disasters, nine beams were exposed to high-temperature flame for one hour, the selected temperatures were 300°C (572°F), 500°C (932°F) and 700°C (1292°F) as recomm
... Show More