The proposed method is sensitive, simple , fast for the determination of mebeverine hydrochloride in pure form or in pharmaceutical dosage . Using Homemade instrument fluorimeter continuous flow injection analyser with solid state laser (405 nm) as a source. Where it is based upon the fluorescence of fluorescein sodium salt and quenching effect of fluorescence by mebeverine in aqueous medium. The calibration graph was linear in the concentration range 0.05 to10 mMol.L-1 (r= 0.9629) with relative standard deviation (RSD%) for 1 mMol.L-1mebeverine solution was lower than 3% (n=6). Three pharmaceutical drugs were used as an application for the determination of mebeverine. A comparison was made between the newly developed method of analysis with the quoted value using the standard addition method. It can be noticed that there was no significant differences between the newly developed method and the quoted value by the manufacturers companies. It indicates clearly that the new method can be used for the assessment as well as the method adopted by the manufactures companies that can be described.
In this paper, we have examined the influence of heat- transfer on the magnetohydrodynamics oscillatory flow of Williamson fluid during porous medium for two types of geometries "Poiseuille flow and Couette flow". We use perturbation technique in terms of the Weissenberg number to obtain explicit forms for velocity profiles. The results that obtained are illustrated by graphs.
Background: The irradiation of teeth with a laser results in an interaction between the light and the biological constituents of the dental hard substance, which is converted directly into heat.This thermal effect is the cause of the structural and chemical enamel changes.The combined treatment of topical fluoride agent with laser may increase fluoride uptake, and reduce progression of caries-like lesions. The aim of this study was to measure the uptake of the acidulated phosphate fluoride and sodium fluoride to the buccal and lingual caries-like lesion enamel surfaces before and after irradiated by Nd-YAG laser in comparison with matching control group. Materials and methods: The sample consisted of 30 human healthy upper premolar teeth wh
... Show MoreTiO2 thin films have been deposited at different concentration of
CdO of (x= 0.0, 0.05, 0.1, 0.15 and 0.2) Wt. % onto glass substrates
by pulsed laser deposition technique (PLD) using Nd-YAG laser
with λ=1064nm, energy=800mJ and number of shots=500. The
thickness of the film was 200nm. The films were annealed to
different annealing (423 and 523) k. The effect of annealing
temperatures and concentration of CdO on the structural and
photoluminescence (PL) properties were investigated. X-ray
diffraction (XRD) results reveals that the deposited TiO2(1-x)CdOx
thin films were polycrystalline with tetragonal structure and many
peaks were appeared at (110), (101), (111) and (211) planes with
preferred orientatio
In this work, pure and Ag-doped nickel oxide (NiO) thin films were deposited on glass substrates with different dopant concentrations (0.1, 0.2, 0.3 and 0.4 wt.%) by pulsed-laser deposition (PLD) technique at room temperature. These films were annealed at temperature of 450 °C. The structural and optical properties of the prepared thin films were studied. It was found that annealing process has lead to increase the transmittance of the deposited films. Also, the transmittance was found to increase with doping concentration of silver in the deposited NiO films. The optical energy gap was decreased from 3.5 to 3.2 eV as the doping concentration was increased to 0.4 %.
Colloidal dispersions of mono Au, Ag , Cu and bimetallic Ag/Au and Cu/Au
core/shell nanoparticles are synthesized by pulsed laser ablation of metals targets
immersed in 5 ml distilled water (DW). Surface Plasmon resonance (SPR) and
particle sizes are characterized by UV-VIS and HRTEM, the X-ray diffraction
shows the structure of core/shell. The Surface Plasmon resonance of the produced
nanoparticles solutions for silver nanoparticles about 402 nm and copper
nanoparticles about 636 nm. While for the core-shell observed two peaks of SPR,
Ag/Au core/shell at (406-516) nm, and Cu/Au core/shell observed one peak at
565nm, because the region of gold and copper close together. The shape and
particle size have been con
In this paper, Al and Cu Plasmas that produced by pulsed Nd:YAG laser with fundamental wave length with a pulse duration of 6 nS focused onto Al and Cu targets in atmospheric air are investigated spectroscopically. The influence of pulse laser energy on the some Al and Cu plasmas characteristics was diagnosed by using optical emission spectroscopy for the wavelength range 320-740 nm. The results observed that the increase of pulse laser energy causes to increase all plasma characteristics of both plasmas under study and shown increasing of the emission line intensity. The appearance of the atomic and ionic emission lines of an element in the emission spectrum depends on the ionization energy of target atoms. The plasma characteristics ar
... Show MoreA total of 20 raw milk samples were used as the fouling agent for evaluating the bacteriological effectiveness of cleaning and sanitizing of domestic milking equipment by using ozonated water at 0.5 ppm comparing to the warm water at 55! for 5 minutes respectively. The mean values of total aerobic bacteria, Coliform and E.coli that present on the plastic and stainless-steel containers after using the raw milk as fouling agent were 3.4×10-6 , 6.7x10-5 and 5.8×10-3 cfu/cm2 respectively , after cleaning the stainless steel containers by the ozonated water the mean values of total aerobic bacterial counts, Coliforms and E.coli bacteria were reduced to 1.2×10-6, 4.7×10-5 and 3.3×10-3 CFU/cm2 respectively. while after cleaning by the warm wa
... Show MoreNd:YAG laser pulses of 9 nanosecond pulse duration and operating wavelength at 1.06 μm, were utilized to drill high thermal conductivity and high reflectivity aluminum and copper foils. The results showed a dependence of drilled holes characteristics on laser power density and the number of laser pulses used. Drilled depth of 74 ϻm was obtained in aluminum at 11.036×108 W/cm2 of laser power density. Due to its higher melting point, copper required higher laser power density and/or larger number of laser pulses to melt, and a maximum depth of 25 μm was reached at 13.46×108 W/cm2 using single laser pulse.