Castellated columns are structural members that are created by breaking a rolled column along the center-line by flame after that rejoining the equivalent halves by welding such that for better structural strength against axial loading, the total column depth is increased by around 50 percent. The implementation of these institutional members will also contribute to significant economies of material value. The main objectives of this study are to study the enhancement of the load-carrying capacity of castellated columns with encasement of the columns by Reactive Powder Concrete (RPC) and lacing reinforcement, and serviceability of the confined castellated columns. The Castellated columns with RPC and Lacing Reinforcement improve compactness and local buckling (web and flange local buckling), as a result of steel section encasement. This study presents axial load test results for four specimens Castellated columns section encasement by Reactive powder concrete (RPC) with laced reinforcement. The encasement consists of, flanges unstiffened element height was filled with RPC for each side and laced reinforced which are used inclined continuous reinforcement of two layers on each side o0f the web of the castellated column. The inclination angle of lacing reinforcement concerning the longitudinal axis is 45o. Four specimens with four different configurations will be prepared and tested under axial load at columns. The first group was the control group (CSC1) Unconfined castellated steel column, the second group was consists of Castellated columns (web and flange) confined with 17mm of (RPC), welded web, and 6mm laced reinforcement (CSC3). While group three (CSC4) consists of a Castellated steel column same as the sample (CSC3), but without using welding between two parts of the castellated steel column. Groups four and five consist of a Castellated steel column same as sample (CSC4) encased partially with reactive powder concrete (25.5 mm) (CSC5) and full encased flange with reactive powder concrete (34mm) mm (CSC6), respectively. The tested specimens' results show that an increase in the strength of the column competitive with increasing the encased reactive powder concrete thickness. And the best sample was sample CSC6 with (34mm) mm in experimental and ABAQUS results.
Roller compacted concrete (RCC) is a concrete of no slump, no reinforcement, no finishing, and compacted using vibratory roller. When compared with conventional concrete, it contains less water content
when compared to traditional concrete. The RCC technique achieves significant time and cost savings during the construction of concrete. This study demonstrates the preparation of RCC slab of (38 ×38× 10) cm
samples by using roller compactor which is manufactured in local markets. The Hydrated lime additive is used to study the mechanical and physical properties of that RCC slab samples. This investigation is divided
into two main stages: The First stage consists of hammer compaction method with two gradation of aggregate, dense
Background: Debonding orthodontic brackets and removal of residual bonding material from the enamel surface include critical steps that may cause enamel damage. The aim of the present study was to evaluate and compare the site of bond failure and enamel surface damage after debonding of three types of esthetic brackets (composite, ceramic, sapphire) bonded with light cure composite and resin-modified glass ionomer adhesive. Materials and methods: Seventy two maxillary premolars teeth were divided into three groups each group consisted of 24 teeth according to the type of brackets. Each group was subdivided into two subgroups (12 teeth for each) according to the bonding material that was used. After 7 days of bonding procedure, the brackets
... Show MoreContemporary life is racing against time in its temptations and variables, and it has become shaped and changed in an amazing way in its various aspects and fields. This was facilitated by intellectual and scientific communication between civilizations, and the rapid progression in successive inventions and discoveries in the fields of science and arts of knowledge. This contributed to a great economic and commercial renaissance. Then, these economic developments entered the world into a very strong competition, which forced producers to calculate all production costs, to reach the highest profits by reducing the price of the produced commodity on the one hand, and achieving quality in appearance (especially) on the other hand. Since the ma
... Show MoreIn this work, magnesium aluminate spinel (MA) (MgO 28 wt%, Al2O3 72 wt%) stoichiometric compound , were synthesized via solid state reaction (SSR) Single firing stage, and the impact of sintering on the physical properties and thermal properties as well as the fine structure and morphology of the ceramic product were examined. The Spinel samples were pressed at of (14 MPa) and sintering soaking time (2h). The effect of adding oxide titania (TiO2) was studied. The obtained powders were calcined at a temperature range of 1200 and 1400 °C. The calcined samples spinel were characterized by XRD, it showed the presence of developed spinel phase end also showed that the best catalyst is titania. The SEM image showed the high sintering temperat
... Show MoreThe study was trail to treated secondary hydatid cysts in white micepost-infection with Echinococcosis of sheep origin, by immunization with a mixture of CFAgs/PSAgs prepared from haydatid Cyst Fluid antigens (CFAgs) and Proto scolices antigens (PSAgs) respectively, two concentrations (7.5 &15 mg/ml) in addition to two derivatives of benzimidazole; albendazole (A) and mebendazole (M) 10 and 40μg/gm body weight, respectively, one week after challenged dose with protoscolices. to determine the efficacy of immunization and chemotherapy simultaneously in reduction the number of growing cysts, then measured both humoral and cell-mediated immunity. Results: elevation the immune responses that reflected decrease number and diameter of hydatid cys
... Show MoreAbstract:In this research we prepared nanofibers by electrospinning from poly (Vinyl Alcohol) / TiO2. The spectrum of the solution (Emission) was studied at 772 nm. Several process parameter were Investigated as concentration of PVA, the effect of distance from nozzle tip to the grounded collector (gap distance), and final the effect of high voltage. We find the optimum condition to prepare a narrow nanofibers is at concentration of PVA 16gm, the fiber has 20nm diameter.
In this research we prepared nanofibers by electrospinning
from poly (Vinyl Alcohol) / TiO2. The spectrum of the solution
(Emission) was studied at 772 nm. Several process parameter were
Investigated as concentration of PVA, the effect of distance from
nozzle tip to the grounded collector (gap distance), and final the
effect of high voltage. We find the optimum condition to prepare a
narrow nanofibers is at concentration of PVA 16gm, the fiber has
20nm diameter
Introduction: This study aimed to assess the color change of human teeth with artificial enamel white spot lesions (WSLs) after sandblasting with bioactive glass, resin infiltration, and microabrasion and to test color stability after pH cycling. Methods: Fifty extracted human mandibular first molars were randomly assigned into five groups: Sound, WSLs (untreated), and WSLs sandblasted with bioactive glass (Sylc), WSLs treated by resin infiltration (ICON), and WSLs treated by microabrasion (Opalustre), respectively. All specimens underwent a pH cycling procedure. The color parameters for each specimen were assessed using an Easyshade dental spectrophotometer at different time stages then the color changes (ΔE) were calculated. Results: The
... Show MoreThis work investigates the impacts of eccentric-inclined load on ring footing performance resting on treated and untreated weak sandy soil, and due to the reduction in the footing carrying capacity due to the combinations of eccentrically-inclined load, the geogrid was used as reinforcement material. Ring radius ratio and reinforcement depth ratio parameters were investigated. Test outcomes showed that the carrying capacity of the footing decreases with the increment in the eccentric-inclined load and footing radius ratio. Furthermore, footing tilt and horizontal displacement increase with increasing the eccentricity and inclination angle, respectively. At the same time, the increment in the horizontal displacement due t
... Show MoreThe research deals with a new type of high-performance concrete with improved physical properties, which was prepared by using metal additives minutes (Metakaolin) and by studing their impact on the properties of mortar and concrete high-performance through destructive and non destructive tests. This type of concrete is used broadly in public buildings and in other structures . The research involved a number of experiments such as finding the activity index of burned at a temperature of 750 º C according to the standard ( ASTM C-311/03), as well as casting models for the cubic mortar mixtures and concrete containers at different rates of metakaolin ranging between (5% - 20%) as an added part to the cement mix to get a high- compressive
... Show More