This work aimed to identify biosurfactant-producing bacterial strains isolated from hydrocarbon-contaminatedsites and to evaluate their biosurfactant properties. The drop-collapse method and minimal agar added witha layer of diesel as carbon source were used for screening, positive strains were able to grow in a liquidmedium, and surface tension and emulsification index were determined in cell-free supernatant and cellsuspension. 250 bacterial isolate were tested, and 16 were positive for the drop-collapse and hydrocarbonlayer agar method. Most of the strains were Pseudomonas, except for three strains (Acinetobacter, Bacillus,and Rhodococcus). Surface tension was similar in cell-free and cell suspension measurements, with valuesin the range of 58 to 26 (mN/m), and all formed stable emulsions with engine oil (77-92% E24). Consideringthe variety of molecular structures among microbial biosurfactants, they have different chemical propertiesthat can be exploited commercially, for applications as diverse as bioremediation or degradable detergents.
Biodegradation is utilizing microorganisms to degrade materials into products that are safe for the
environment, such as carbon dioxide, water, and biomass. The current study aims to isolate and characterize
bacteria with polyethylene terephthalate (PET) degradation ability isolated from Shatt al-Arab water and
sewage from Basra, the bacteria were identified as Klebsiella pneumonia. According to the findings, the
isolates showed a highly significant difference in degradation of PET (24% during 7 days) and the percent of
degradation increased to 46% at 4 weeks compared to the control. The study also involved determining the
optimum temperature of K. pneumonia growth, which was 37°C, while the preferred
This in vivo study was conducted to investigate the effect of different concentrations of ozonated water on experimentally skin infection with some of bacterial isolates (Pseudomonas aeruginosa and Staphylococcus aureus ) which Showed dermal infection in experimental animals after 48 hours of exposure to these Microorganisms. Results revealed that ozone has the power to accelerated the healing process depending on the perfect concentration of ozonated water used and the severity of infection & nature of causative agent , in which the recovering period was 7 days for the infection caused by P. aeruginosa and 5 day for S.aureus by using the concentration 60 µg/ml . Results also indicated in this study the stimulated effect of O
... Show MoreThe synthesis and bioactivity of zinc oxide nanoparticles has been extensively studied. The antibacterial activity of different antibiotics individually (ceftriaxone (C), chloramphenicol (CRO), penicillin (P) and amoxicillin (Ax)) and Zinc oxide nanoparticles (60μg/ml) in combination with the previously mentioned antibiotics has been demonstrated in the present study by using the disk diffusion assay method. The results showed a synergistic effect between Zinc oxide nanoparticles (ZnO NPs) and both Ax and P for most of the studied Gram-positive isolates (Staphylococcus aureus1, Staphylococcus aureus2, Staphylococcus epidermidis1, Staphylococcus epidermidis2, Enterococcus faecalis1, Enterococcus faecalis2 ) and between ZnO NPs and both C
... Show MoreFive Saccharomyces cerevisiae isolated from the ability of chitinase production from the isolates were studied. Quantitative screening appeared that Saccharomyces cerevisiae S4 was the highest chitinase producer specific activity 1.9 unit/mg protein. The yeast was culture in liquid and solid state fermentation media (SSF). Different plant obstanases were used for (SSF) with the chitine, while liquid media contained chitine with the diffrented nitrogen source. The favorable condition for chitinase producers were incubated at 30 ºC at pH 6 and 1% colloidal chitine.
Pyrolysis of virgin polyethylene plastics was studied in order to produce hydrocarbon liquid fuel. The pyrolysis process carried out for low and high-density polyethylene plastics in open system batch reactor in temperature range of 370 to 450°C.
Thermo-gravimetric analysis of the virgin plastics showed that the degradation ranges were between 326 and 495 °C. The results showed that the optimum temperature range of pyrolysis of polyethylene plastics that gives highest liquid yield (with specific gravity between 0.7844 and 0.7865) was 390 to 410 °C with reaction time of about 35 minutes. Fourier Transform Infrared spectroscopy gave a quite evidence that the produced hydrocarbon liquid fuel consisted ma