This research presents an experimental investigation on the influence of metakaolin replacement percentage upon some properties of different concrete types. Three types of concrete were adopted (self- compacted concrete, high performance concrete and reactive powder concrete) all of high sulphate (SO3) percentage from the fine aggregate weight, 0.75%. Three percentages of metakaolin replacement were selected to be studied (5, 7 and 10) %. Three types of concrete properties (compressive, flexural and splitting tensile strength) were adopted to achieve better understanding for the influence of adding metakaolin.. The output results indicated that the percentage of metakaolin had a different level of positive effect on the compressive strength for both including and excluding of internal sulphate attack. This effect reached at 28 days of curing to (11.86, 10.22 and 4.75) % in case of excluding sulphate attack and to (13.82, 11.47and 6.53) % in the other case for SCC, HPC and RPC respectively. It can be concluded that the effect of metakaolin in both SCC and HPC are more influence than in RPC. Splitting and flexural strength have showed a similar behavior, flexural strength increased by (15.38, 9.42 and 5,84) % at age of 28 days when the sulphate attack is excluded, while it was (14.02, 10.66 and 4.28)% in case of sulphate attack included for SCC,HPC and RPC respectively. The response of splitting tensile strength for both including and excluding of sulphate attack reached to (13.03, 12.95 and 9.17) % and (16.88, 10.33 and 6.74) % respectively for SCC, HPC and RPC.
Background: This study aimed to evaluate the effect of zirconia different surface treatments (primer, sandblast with 50μmAl2O3, Er,Cr:YSGG laser) on shear bond strength between zirconia surface and resin cement. Material and methods: Sixty presintered Y-TZP zirconia cylinder specimens (IPS e.max ZirCAD, Ivoclar vivadent) will be fabricated and sintered in high temperature furnace of (1500 C for 8 hours) according to manufacturer’s instructions to the selected size and shape of (5mm. in diameter and 6mm in height). All specimens were ground flat using 600.800.1000.1200, aluminum oxide abrasive paper to obtain a standardized surface roughness. Surface roughness values were then recorded in µm using surface roughness tester (profi
... Show MoreInternal Audit is one of the most important backers of corporate governance, the researcher expanded his interest in this subject to examine the efficiency of Internal Auditors at the Arab Bank and its branches in Jordan to achieve Accountability which enhances the Corporate Governance and to identify the effect of the International Internal Audit Standards in strengthening the role of Internal Auditors in Accountability, and the effect of Attribute and Performance Standards in Accountability. The researcher applied descriptive analysis method to define the role of Internal Audit in the Arab Bank in achieving one of the basic principles of Corporate Governance assimilated in Accountability. The researcher’s sources include
... Show MoreBackground: The bond strength of the root canal sealers to dentin is very important property for maintaining the integrity and the seal of root canal filling. The aim of this study was to evaluate and compare the push-out bond strength of root filled with total fill Bioceramic, AH Plus and Gutta-flow®2 sealers using GuttaFusion®obturation system versus single cone obturation technique. Materials and method: sixty of mandibular premolars teeth with straight roots were used in this study, these roots were instrumented using Reciproc system, instrumentation were done with copious irrigation of 3 mL 5.25% sodium hypochlorite solution (NaOCl) during all the steps of preparation, and smear layer will be removed with 1 ml of 17% EDTA kept in
... Show MoreBackground: The bond strength of the root canal sealers to dentin is very important property for maintaining the integrity and the seal of root canal filling. The aim of this study was to evaluate and compare the push-out bond strength of root filled with total fill Bioceramic, AH Plus and Gutta-flow®2 sealers using GuttaFusion®obturation system versus single cone obturation technique. Materials and method: sixty of mandibular premolars teeth with straight roots were used in this study, these roots were instrumented using Reciproc system, instrumentation were done with copious irrigation of 3 mL 5.25% sodium hypochlorite solution (NaOCl) during all the steps of preparation, and smear layer will be removed with 1 ml of 17% EDTA kept in
... Show MoreConcrete pavements are essential to modern infrastructure, but their low tensile and flexural strengths can cause cracking and shrinkage. This study evaluates fiber reinforcement with steel and carbon fibers in various combinations to improve rigid pavement performance. Six concrete mixes were tested: a control mix with no fiber, a mix with 1% steel fiber (SF1%), a mix with 1% carbon fiber (CF1%), and three hybrid mixes with 1% fiber content: 0.75% steel /0.25% carbon fiber (SF0.75CF0.25), 0.25% steel /0.75% carbon fiber (SF0.25CF0.75), and 0.5% steel /0.5% carbon fiber ((SF0.5CF0.5). Laboratory experiments including compressive, flexural, and splitting tensile strength tests were conducted at 7, 28, and 90 days, while Finite Element Analys
... Show MoreThis paper presents experimental results regarding the behaviours of eight simply supported partially prestressed concrete beams with internally unbonded tendons, focusing particularly on the effect of three different variables: concrete compressive strength,
The introduction of concrete damage plasticity material models has significantly improved the accuracy with which the concrete structural elements can be predicted in terms of their structural response. Research into this method's accuracy in analyzing complex concrete forms has been limited. A damage model combined with a plasticity model, based on continuum damage mechanics, is recommended for effectively predicting and simulating concrete behaviour. The damage parameters, such as compressive and tensile damages, can be defined to simulate concrete behavior in a damaged-plasticity model accurately. This research aims to propose an analytical model for assessing concrete compressive damage based on stiffness deterioration. The prop
... Show MoreThe aim of this research is to know danger of radioactive isotopes
that are found in samples of drugs traded in Iraqi markets. The
samples are Iraqi Amoxicillin, English Amoxicillin, UAE
Amoxicillin, Indian Amoxicillin, Iraqi Paracetamol, English
Paracetamol, UAE Paracetamol and Indian Paracetamol. By high
purity germanium the activity of the following isotopes 40K, 214Pb,
228Ac and 137Cs is measured and the specific activity was used to
calculate the annual effective dose. Then the calculated annual
effective dose values are compared with the allowable annual
effective dose values of each part of digestive channel. This research
concluded that the measured annual effective dose values are not
dangerous.<