The optimal design of any structural elements requires examining all environmental risks, emergency accidents, and standard load cases. Exposure to fire is one of the most common safety threats. Nowadays wide developments are achieved in the field of concrete technology, therefore, experimental and theoretical investigations should be performed on the characteristics of such developed materials under different loading conditions. This study investigates the impact of fire exposure on the mechanical characteristics of self-compacting concrete, specifically compressive and tensile strength, modulus of elasticity, and stress-strain relation. The adopted fire exposure consisted of six steady-state temperatures (300, 400, 500, 600, 700, and 800°C) for one hour and a sudden cooling method. Four glass fiber volume fractions were adopted: 0, 0.5, 1, and 1.5%. The glass fiber volume fractions considered (0.5-1.5%) improved the mechanical properties investigated. Two states were detected for the effect of fire exposure. The effect of fire exposure was inversely proportional to fiber content in burning temperatures of 300-700°C, while the reduction in mechanical properties of 1.5% fiber content was greater than those of 0.5 and 1% when the temperature increased to 800°C. Furthermore, the addition of glass fiber changed the brittle mode stress-strain relation to semi-ductile for the non-burned and burned up to 600°C specimens, whereas a brittle behavior was detected when the temperature increased above 600°C. In general, a similar effect was noticed for all the glass fiber ratios considered regarding the slope of the stress-strain linear stage compared to the non-burned specimens, which was more salient when the burning temperature increased.
This research is devoted to study the strengthening technique for the existing reinforced concrete beams using external post-tensioning. An analytical methodology is proposed to predict the value of the effective prestress force for the external tendons required to close cracks in existing beams. The external prestressing force required to close cracks in existing members is only a part from the total strengthening force.
A computer program created by Oukaili (1997) and developed by Alhawwassi (2008) to evaluate curvature and deflection for reinforced concrete beams or internally prestressed concrete beams is modified to evaluate the deflection and the stress of the external tendons for the externally strengthened beams using Matlab
Resin-modified glass ionomer cement tends to shrink due to polymerization of the resin component. Additionally, they are more prone to syneresis and imbibition during the setting process. This
Thin films of (Cu2S)100-x( SnS2 )x at X=[ 30,40, &50)]% with thickness (0.9±0.03)µm , had been prepared by chemical spray pyrolysis method on glass substrates at 573 K. These films were then annealed under low pressure of(10-2) mbar ,373)423&473)K for one hour . This research includes , studying the the optical properties of (Cu2S)100-x-(SnS2)x at X=[ 30,40, &50)]% .Moreover studying the effect of annealing on their optical properties , in order to fabricate films with high stability and transmittance that can be used in solar cells. The transmittance and absorbance spectra had been recorded in the wavelength range (310 - 1100) nm in order to study the optical properties . It was found that these films had direct optical band
... Show MorePhoenix dactylifera l. pinnae (the green leaves of dates palm) were used as natural reinforcing (strengthening) fibers to improve the mechanical properties of polyester as a matrix material, the fibers of the green leaves of dates palm were used in two lengths, 10 and 20mm with five rates of 0, 2.5, 5, 10, and 20% , where the reinforcing with the leaves fibers increases the hardness strength from 76.5 to be about 86.55 , the Impact value raised from about 0.313 to 0.461 , in addition to that the flexural strength from 2.66 to be about 55 , and the thermal conductivity increases from 2.54 𝑤∕𝑚.℃ to 5.41 𝑤∕𝑚.℃. The results of the present search explains that the composite samples reinforced at rate 20% and 10mm fiber length
... Show MoreThe structural, optical and electrical properties of ZnS films prepared by vacuum evaporation technique on glass substrate at room temperature and treated at different annealing temperatures (323, 373, 423)K of thickness (0.5)µm have been studied. The structure of these films is determined by X-ray diffraction (XRD). The X-ray diffraction studies show that the structure is polycrystalline with cubic structure, and there are strong peaks at the direction (111). The optical properties investigated which include the absorbance and transmittance spectra, energy band gab, absorption coefficient, and other optical constants. The results showed that films have direct optical transition. The optical band gab was found to be in the range t
... Show MoreThe lead-acid battery has become so dependable in its used applications of automobile starting, emergency lighting and telecommunications, which left an impression that no further investigation is necessary or desirable. While there has been slow continuous improvements in lead-acid battery performance and mainly limited to design and material engineering. This work is mainly devoted to the properties of the active mass of the positive electrode and the acid/water ratio during the manufacturing process. A field study is carried out at the State Battery Manufacturing Company located in Baghdad, to prepare batches of lead mono-oxide with predefined quantities of liquid additives (i.e. sulfuric acid and water). Quality control and laborator
... Show MoreABSTRACT:In this paper, Cd10–xZnxS (x = 0.1, 0.3, 0.5) films were deposited by using chemical spray pyrolysis technique, the molar concentration precursor solution was 0.15 M/L. Depositions were done at 350°C on cleaned glass substrates. X-ray dif- fraction technique (XRD) studies for all the prepared film; all the films are crystalline with hexagonal structure .The optical properties of the prepared films were studied using measurements from VIS-UV-IR spectrophotometer at wave- length with the range 300 - 900 nm; the average transmission of the minimum doping ratio (Zn at 0.1%) was about 55% in the VIS region, it was decrease at the increasing of Zn concentration in the CdS films, The band gap of the doped CdS films was varied as 3.7, 3
... Show MoreNumerous drilling additives and materials are used continuously because they are necessary to support and give the required properties of the drilling fluid so that to ensure the stability of the borehole. This paper aspires to evaluate the rheological properties of bentonite (montmorillonite) Trefawey as an alternative to using commercial bentonite. Monitoring and evaluating of the rheological and filtration properties were prepared. This exertion aims to focus on the effect of hematite, and barite on the rheological properties of the three aforementioned bentonite types. An improvement in the rheological properties of bentonite (montmorillonite). Trefawey was observed after adding the previous heavy materials. Hematite has by some
... Show MoreThis work compares the changes in optical and structural properties of cerium oxide (CeO2) when doped with different concentrations (3%,5%,7%, and 9%) of two oxides, In2O3 and Eu2O3. X-ray diffraction and spectrophotometry were employed in the visible, ultraviolet, and near-infrared regions. The findings demonstrated that CeO2 doped with In2O3 and Eu2O3 thin films were polycrystalline and had a cubic structure. The crystal size increased from 20.5 to 32.15 when Eu2O3 doping ratio increased from 0% to 7% and then decreased to 28.46 nm at 9%. While the crystal size showed an increase from 20.5 to 21.42 nm with the increase of the In2O3 doping ratio, while the lattice constant measured for cubic CeO2 changed opposite to that
... Show MoreIn this study a polymeric composite material was prepared by hand
lay-up technique from epoxy resin as a matrix and magnesium oxide
(MgO) as a reinforcement with different weight fraction (5,10,15,
and 20)% to resin. Then the prepared samples were immersed under
normal condition in H2So4(1 M) solution, for periods ranging up to
10 weeks. The result revealed that the diffusion coefficient
decreasing as the concentration of MgO increase. Also we studied
Hardness for the prepared samples before and after immersion. The
result revealed that the hardness values increase as the concentration
of MgO increase, while the hardness for the samples after immersion
in H2SO4 dec