Objectives: Maxillofacial silicone is used to restore abnormalities due to congenital or acquired causes. However, the quality of silicone is far from ideal. This study was aimed at assessing the influence of the addition of cellulose nanofibers (CNFs; several nanometers wide and 2-5 micro m long) on the physical and mechanical characteristics of maxillofacial silicone elastomers. Methods: Two CNF weight percentages (0.5% and 1%) were tested, and 180 specimens were divided into one control and two experimental groups. Each group was subdivided into six subgroups. In each subgroup, ten specimens subjected to each of the following tests: tearing strength, Shore-A hardness, tensile strength, elongation percentage, surface roughness, and color stability. The samples were additionally analyzed with Fourier transform infrared spectroscopy (FTIR) and field emission scanning electronic microscopy (FESEM). Results: The 0.5% CNF group, compared with the control group, exhibited highly significantly greater tearing strength, elongation percentage, hardness Shore-A, and surface roughness, and substantially greater tensile strength. However, color stability did not significantly differ between groups. The 1% CNF group showed significantly greater Shore-A hardness, tear strength, color stability, and surface roughness, and insignificantly lower tensile strength and percentage elongating values, than the control group. FESEM imaging revealed good CNF dispersion. The FTIR spectra indicated that CNFs interacted with silicon through surface functional hydroxyl groups. Conclusion: Addition of 0.5 wt. % CNF to silicone elastomers increased the material’s mechanical tensile strength, tear strength, elongation percentage, and hardness as long as it stayed within the acceptable range for clinical use. Surface roughness increased in direct proportion to the amount of nanofibers added. Moreover, addition of 0.5 wt. % CNF to silicone polymers had insignificant effects on color stability.
The current study was conducted on 504(Ros-308) broiler chicks during the period 28/9/2017-9/11/2018to determine the effect of heat shock in early age and additives such as ginseng in three levels on birds weight and feedconsumption. Results showed that the exposure to high temperature (38-400C) lead to significant decrease (p≤≤≤≤≤0.05 (inaverage body weight at7 day of age and significant decrease in body weight in birds expousured to high temperature inthe periods 2, 4 and 6 hours compared with control (Table 1). Significant decrease in live body weight when exposure to2hr compared with 6hr namely (138.54) and (144.21), respectively while no significant difference between 2 and 4h.Results showed no significant effect in body we
... Show MoreThe present study was conducted in order to focus on the effect of the addition of Carnitine and Niacin on some blood serum parameters of Common Carp Cyprinus Carpio. 48 fish carp mean weight 44.13 gm were distributed randomly on four feeding treatments (12 fish each) with replicates (6 fish each) in 8 glass aquaria. Treatments were as follows: fish were fed on basic diet without any addition and conducted as control (T1); addition of 200 mg Carnitine/ Kg diet, (T2) addition of 28 mg Niacin/Kg diet (T3), addition of a mixture of 200 mg Carnitine and 28 mg Niacin/ Kg diet as (T4). The experiment was conducted for 70 days and the results showed an increase in the Cholesterol concentration of T1 (187.6 mg/ 100 ml) and differed s
... Show MoreIn this work, the photodetection performance of polyvinyl alcohol (PVA) nanofibers and its composite with yttrium oxide (Y2O3) at different concentrations (2.5, 5, 10) wt% are examined deposited on p-type Si with (111) orientation. Electrospinning technique was used to create nanofiber composites. Adding Y2O3 significantly impacts the PVA nanofibers where ultraviolet-visible (UV-Vis) spectroscopy optical absorption energy gap decreases with increased concentration (2.8, 2.6, and 2.3) eV. X-ray diffraction was used to investigate crystal structure, which is cubic structure. The chemical composition study was conducted using Fourier transform infrared spectroscopy (FTIR) spectra, which revealed the stretching vibrations related to the Y-O bon
... Show MoreThe current work studies the effect of adding chopped carbon fiber (CCF) on gypsum plaster properties (precisely the compressive strength and the modulus of rupture). The research plan consists of using six mixes of gypsum plaster; these mixes are divided into two groups according to the (Water/Gypsum) ratios (0.5 & 0.6). Each group was divided into three subgroups according to CCF volume fraction (Vf): 0.0%, 0.2% and 0.4%. Three cubic (50×50×50) mm and three prismatic (40×40×160) mm samples were performed for each mix. It was found that, the addition of CCF to the gypsum plaster mixes increases both the compressive strength and the modulus of rupture for both (W/G) ratios, an
Cu-Al-Ni shape memory alloy specimens has been fabricated using powder metallurgy technique with tube furnace and vacuum sintering environment , three range of Nb powder weight percentage (0.3,0.6,0.9)% has been added. Micro hardness and sliding wear resist has been tested followed by X-ray diffraction, scanning electron microscope (SEM) and energy dispersive X-ray spectroscope (EDX) for micro structure observation. The experimental test for the samples has showed that the increase of Nb powder weight percentage in the master alloy has a significant effect on increasing the hardness and decreasing the wear resist therefore it will enhance the mechanical properties for this alloy.
Concrete pavements are essential to modern infrastructure, but their low tensile and flexural strengths can cause cracking and shrinkage. This study evaluates fiber reinforcement with steel and carbon fibers in various combinations to improve rigid pavement performance. Six concrete mixes were tested: a control mix with no fiber, a mix with 1% steel fiber (SF1%), a mix with 1% carbon fiber (CF1%), and three hybrid mixes with 1% fiber content: 0.75% steel /0.25% carbon fiber (SF0.75CF0.25), 0.25% steel /0.75% carbon fiber (SF0.25CF0.75), and 0.5% steel /0.5% carbon fiber ((SF0.5CF0.5). Laboratory experiments including compressive, flexural, and splitting tensile strength tests were conducted at 7, 28, and 90 days, while Finite Element Analys
... Show MoreBackground: to evaluate the effect of different dentifrices on the surface roughness of two composite resins (nanofilled-based and nanoceramic – based composite resins). Materials and methods: Forty specimens (diameter 12 mm and height of 2mm) prepared from different composite resin materials: Z350 (nanofilled composite, and Ceram-X (nanoceramic) .they were subjected to brushing simulation equivalent to the period of 1 year. The groups assessed were a control group brushed with distilled water (G1), Opalescence whitening toothpasteR (G2), Colgate sensitive pro-relief (G3) and Biomed Charcoal Toothpaste (G4). The initial and final roughness of each group was tested by surface roughness tester. The results were statistically analyzed using
... Show MoreIn this work a chemical sensor was built by using Plane Wave Expansion (PWE) modeling technique by filling the core of 1550 hollow core photonic crystal fiber with chloroform that has different concentrations after being diluted with distilled water. The minimum photonic bandgap width is.0003 and .0005 rad/sec with 19 and 7 cells respectively and a concentration of chloroform that filled these two fibers is 75%.