Aims: This study was conducted to assess the effect of the addition of yttrium oxide (Y2O3) nanoparticles on the tensile bond strength, tear strength, shore A hardness, and surface roughness of soft-denture lining material. Materials and Methods: Y2O3 NPs with 1.5 and 2 wt.% were added into acrylic-based heat-cured soft-denture liner. A total of 120 specimens were prepared and divided into four groups according to the test to be performed (tensile bond strength, tear strength, surface hardness, and surface roughness). Results: There was a highly significant increase in tensile bond strength between the soft liner and the acrylic denture base, tear strength, and hardness at both concentrations as compared to the control group, whereas there was a nonsignificant difference between 1.5wt% of Y2O3 nanoparticles and the control group, and between 1.5wt% and 2wt% of Y2O3 nanoparticles. But there was a significant difference between 2wt% of Y2O3 nanoparticles and the control group. Conclusion: The Y2O3 nanoparticles impregnated in soft-lining materials increased the mechanical properties of both tensile bonding strength and tear strength. Also, there was a significant increase in hardness but there was no change in surface roughness of acrylic-based denture soft-lining materials.
Leaf samples of Lawsonia inermis were collected from Basrah city, South of Iraq to examine their antimicrobial activity . The effects of water and chloroform crude extracts of the leaves in different concentrations were obtained and bioassayed in vitro for its bioactivity to inhibit the growth of six types of bacteria . The extract of water was clearly superior for all bacteria especially the bacteria Staphlylococcus aureus (inhibition zone was 21mm in concentration 70mg/ml) from gram positive bacteria, and Klebsiella pneumoniae (inhibition zone was 20mm in the same concentration) , and the growth of all bacteria was inhibited to varying degrees by increasing the concentration of the henna leaves and are commonly known to possess a
... Show MoreBackground: The bond strength of the root canal sealers to dentin seems to be a very important property for maintaining the integrity and the seal of root canal filling. The aim of this study was to evaluate the shear bond strength of four different obturation systems using push-out test. Materials and methods: Forty straight palatal roots of the maxillary first molars teeth were used in this study, these roots were instrumented using crown down technique and ProTaper system, instrumentation were done with copious irrigation of 2.5% sodium hypochlorite and 17% buffered solution of EDTA was used as final irrigant followed by distilled water, roots were randomly divided into four groups according to the obturation system (ten teeth for each g
... Show MoreBackground: Antimicrobial agents have been considered as having potential for the prevention of dental caries. This study aimed to test the effect of different concentrations of cardamom and black tea extracts on the sensitivity and growth of salivary mutans streptococci in comparison to chlorhexidine gluconate (0.2%) in vitro. Materials and methods: In this study. Mutans streptococci were isolated from saliva of 34 healthy people (aged between 22-40yrs). The bacteria was isolated, purifiedand diagnosed according to morphologicalcharacteristic and biochemical tests. Aqueous extracts of cardamom and black tea were prepared. Different concentrations of extracts were prepared and estimated in gm/ 100ml deionized water. The agar diffusion techn
... Show MoreAn improved Metal Solar Wall (MSW) with integrated thermal energy storage is presented in this research. The proposed MSW makes use of two, combined, enhanced heat transfer methods. One of the methods is characterized by filling the tested ducts with a commercially available copper Wired Inserts (WI), while the other one uses dimpled or sinusoidal shaped duct walls instead of plane walls. Ducts having square or semi-circular cross sectional areas are tested in this work.
A developed numerical model for simulating the transported thermal energy in MSW is solved by finite difference method. The model is described by system of three governing energy equations. An experimental test rig has been built and six new duct configurations have b
The heat and mass transfer coefficients of the indirect contact closed circuit cooling tower, ICCCCT, were investigated experimentally. Different experiments were conducted involving the controlling parameters such as air velocity, spray water to air mass flow rate ratio, spray water flow rate, ambient air wet bulb temperature and the provided heat load to investigate their effects on the performance of the ICCCCT. Also the effect of using packing on the performance of the ICCCCT was investigated. It was noticed that these parameters affect the tower performance and the use of packing materials is a good approach to enhance the performance for different operational conditions. Correlations for mass and heat transfer coefficients are pres
... Show MoreHydrogen sulfide removal catalyst was prepared chemically by precipitation of zinc bicarbonate at a controlled pH. The physical and chemical catalyst characterization properties were investigated. The catalyst was tested for its activity in adsorption of H2S using a plant that generates the H2S from naphtha hydrodesulphurization and a unit for the adsorption of H2S. The results comparison between the prepared and commercial catalysts revealed that the chemical method can be used to prepare the catalyst with a very good activity.
It has observed that the hydrogen sulfide removal over zinc oxide catalyst follows first order reaction kinetics with activation energy of 19.26 kJ/mole and enthalpy and e
... Show MoreAn overall mathematical model for copper pipe corrosion in flowing water was derived based on mass transfer fundamentals where we introduced the effects of boundary layer velocity, bulk flow velocity and the surface oxide protective film on the corrosion rate. A set of experiments were conducted in a straight 10mm diameter copper pipe, flow of water include six velocities of maximum value 7.33m/sec at 200C and 350C. The good agreement between the calculated and experimental corrosion rate values were achieved , the agreement reached 92% .