Corrosion Resistance Enhancement for low carbon steel is very important to extend its life service, the coating process is one of the methods which can using to achieve this, and it's the most important in surface treatments to improve the properties of metals and alloys surfaces such as corrosion resistance. In this work, low carbon steel was nitrided and coated with nano zinc using gas phase coating technical, to enhance the resistance of corrosion. The process included adding two layers. The first, a nitride layer, was added by precipitating nitrogen (N) gas, and the second, a zinc (Zn) layer, was added by precipitating Zn. The process of precipitating was carried out at different periods (5, 10, and 15 minutes). Scan electron microstructure (SEM), X-ray diffraction (XRD) and corrosion tests were carried out. The SEM and XRD results showed a new microstructure with the emergence of new phases (C3N4, Zn(N3)2, and γN). Also, the results of the corrosion test showed a significant improvement in corrosion resistance through a reduction in the corrosion rate (CR) and corrosion current density (icorr) which reached (1.598x10-3 mmpy) and (1.422x10-7 Amp/cm2) respectively, for coated samples, compared with 1.803×10-1 and 1.604x10-5, respectively, for the base metal. also found an appreciable increase in corrosion protection efficiency (CPE), which reached 99.11%.
In present work an investigation for precise hole drilling via continuous wave (CW) CO2 laser at 150 W maximum output power and wavelength 10.6 μm was achieved with the assistance of computerized numerical controlled (CNC) machine and assist gases. The drilling process was done for thin sheets (0.1 – 0.3 mm) of two types of metals; stainless steel (sst) 321H, steel 33 (st). Changing light and process parameters such as laser power, exposure time and gas pressure was important for getting the optimum results. The obtained results were supported with computational results using the COMSOL 3.5a software code.
In this paper the analysis of the corrosion basic types destructions on an example of buildings constructions is carried out and the basic requirements to materials for designs in construction are defined. A classification of corrosion damage is proposed, which became a prerequisite for selecting the main indicators of materials that maximally affect the quality and durability. The main methods for determining the main indicators of corrosion damage are identified.
Activated carbon (AC) is a highly important adsorbent material, as it is a solid form of pure carbon that boasts a porous structure and a large surface area, making it effective for capturing pollutants. Thanks to its exceptional features, AC is widely used for purifying water that is contaminated with odors and removing dyes in a cost-effective manner. A variety of carbonic materials have been employed to prepare AC, and this study aimed to evaluate the suitability of utilizing waste mango and avocado seeds for this purpose, followed by testing their efficacy in removing dye from aqueous solutions. The results indicate that using waste mango and avocado as AC is technically feasible, achieving dye removal percentages of 98% and 93%,
... Show Morethis paper contains preparation of Active carbon surface (AC) from pro so millet grain husks and Loading and activating by Iron oxide and hydrogen peroxide sequentially to obtain surface (ACIPE). The changes of previous processes on Active carbon surface were diagnosed by Fourier transform infrared spectroscopy (FTIR) and Scanning electron microscopy ( SEM ). These surfaces (AC and ACIPE ) were using as adsorbent for removing of congo red dye from aqueous solutions under certain conditions through batch system. More than one kinetic model was applied to congo red dye adsorption process and it was found that the most kinetic model applied to it is a model ( pseudo second order model).
In this work the design and construction of a flash photolysis pulsed HCl laser was presented. The parameters of the pumping source and discharge current density was obtained, which sufficient to shift the flash lamp spectrum towards uv portion of spectrum. The maximum pulse laser energy parameters was measured. Total pressure and ratio of active gases to optimized the output pulse energy were measured , where at 125 mbar of total pressure and 1:7:14 Cl2:H2: He ratio, the laser energy was measured to be 200 mJ at pumping four flash lamps energy in the order of 6400J .The resonator consists of copper a near hemispherical mirror with the radius of curvature 3m coated by gold and reflectivity 98%,the output coupler sapphire mirror of
... Show MorePsi prepared by Electrochemical etching technique at invariable etching current density of 10 mA/cm2 and at different times (7 and 17) min. The porous Si structure was studied using XRD, (FE-SEM) and EDS. The process of sensing NH3 gas is carried out at different operating temperatures (R.t,80,130 and 200)°C and the gas concentration is constant. It is measured by changing the resistance of the sensor as a function of exposure time to the gas. The result showed the XRD patterns of the PS at (7 and 17) min etching time. the peak samples at (111) around 2θ = 28.5°. It is observed that the peak intensity declines with rising the etching time,