Highly Modified Asphalt (HiMA) binders have garnered significant attention due to their superior resistance to rutting, fatigue cracking, and thermal distress under heavy traffic loads and extreme environmental conditions. While elastomeric polymers such as Styrene- Butadiene-Styrene (SBS) have been extensively used in HiMA applications, the potential of plastomeric polymers, including Polyethylene (PE) and Ethylene Vinyl Acetate (EVA), remains largely unexplored. This study aims to evaluate the performance of reference binder (RB) modified with plastomeric HiMA asphalt in comparison to SBS-modified binders and determine the optimal polymer dosage for achieving an optimal balance between rutting resistance and fatigue durability. The experimental program involved modifying a base asphalt binder with SBS, PE, and EVA at dosages of 6%, 7%, and 8% by weight of binder. A comprehensive evaluation was conducted, including conventional tests (penetration, softening point, viscosity, mass loss, storage stability, and specific gravity) and rheological characterization using the Dynamic Shear Rheometer (DSR). The Multiple Stress Creep Recovery (MSCR) test was employed to assess high-temperature performance, while the Linear Amplitude Sweep (LAS) test evaluated fatigue behavior. Additionally, an Overall Desirability (OD) analysis was performed to integrate multiple performance criteria and establish a ranking for each modification. The results demonstrated that SBS-modified binders exhibited the most balanced performance, with SBS8 achieving the highest elastic recovery (52.87%) and superior fatigue life, exceeding 1,017,904 cycles at 2.5% strain. PE8 exhibited exceptional rutting resistance, reaching the lowest Jnr 3.2 value (0.0078 kPa−1); however, its limited elasticity (15.7% recovery) indicated reduced flexibility. EVA modifications demonstrated marginal improvements in fatigue resistance but failed to meet the AASHTO M332 criteria for high-traffic applications. The OD analysis ranked SBS8 as the most effective HiMA binder (OD score = 0.715), followed by SBS7 (0.588) and SBS6 (0.509). PE7 (0.354) and PE6 (0.337) demonstrated moderate performance, whereas EVA had the lowest desirability score (0.000). Based on these findings, SBS-modified binders are recommended for applications requiring a balance between fatigue and rutting resistance, whereas PE-based HiMA is more suitable for high-temperature regions where rutting is the primary concern. Further field studies are necessary to validate the long-term durability of plastomeric HiMA binders and optimize their use for specific pavement conditions.
This research aims to investigate the effect of four types of nanomaterial on the Marshall properties and durability of warm mix asphalt (WMA). These types are; nano silica(NS), nano carbonate calcium (NCC), nano clay(NC), and nanoplatelets (NP). For each type of Nanomaterial, three contents are tried as following; NS(1%, 3%, and 5%), NCC(2%, 4%, and 6%), NC(3%, 5%, and 7%), and NP (2%, 4%, and 6%) by weight of asphalt cement. Following Marhsall mix design method, the optimum asphalt cement content is determined, thereafter the optimum dosage for each nanomaterial is obtained based on the highest Marshall stability value. The durability of the control mix (no nanomaterial) and modified mixtures have been compared based on moisture damage, r
... Show MoreRutting is a crucial concern impacting asphalt concrete pavements’ stability and long-term performance, negatively affecting vehicle drivers’ comfort and safety. This research aims to evaluate the permanent deformation of pavement under different traffic and environmental conditions using an Artificial Neural Network (ANN) prediction model. The model was built based on the outcomes of an experimental uniaxial repeated loading test of 306 cylindrical specimens. Twelve independent variables representing the materials’ properties, mix design parameters, loading settings, and environmental conditions were implemented in the model, resulting in a total of 3214 data points. The network accomplished high prediction accuracy with an R
... Show MoreImplementation of Warm Mix Asphalt concrete (WMA) is getting global acceptance due to the restrictions for protecting the environment and the requirements to reduce fuel consumption. In this investigation, two WMA mixtures have been prepared in the laboratory using medium curing cutback (MC-30) and Cationic emulsion asphalt. Hot Mix Asphalt (HMA) was also prepared for comparison. The cylinder specimens (63.5mm) in height and (101.6mm) in diameter were constructed from the mixtures and subjected to indirect tensile strength test to determine the Tensile Strength Ratio (TSR). The cylinder specimens of (101.6mm) in height and (101.6mm) in diameter were also constructed from those mixtures and subjected to static compressive
... Show MoreSustainable pavements are pavements that meet the requirements of present generation without influencing the capability of the future generation to meet their needs. One of the problems of the warm mix asphalt is that it has low resistance to moisture damage; therefore, the aim of this research paper is to study the possibility of producing more durable warm mixes against the moisture damage with the use of recycled concrete aggregate (RCA) which has not been studied before. Six replacement rates (0, 20, 40, 60, 80, and 100%) for the coarse version aggregate (VA) with RCA were studied. The Marshall mix design method was used to determine the optimum asphalt cement content for each replacement rate. Thereafter, specimens with the opt
... Show MoreSustainable pavements are pavements that meet the requirements of present generation without influencing the capability of the future generation to meet their needs. One of the problems of the warm mix asphalt is that it has low resistance to moisture damage; therefore, the aim of this research paper is to study the possibility of producing more durable warm mixes against the moisture damage with the use of recycled concrete aggregate (RCA) which has not been studied before. Six replacement rates (0, 20, 40, 60, 80, and 100%) for the coarse version aggregate (VA) with RCA were studied. The Marshall mix design method was used to determine the optimum asphalt cement content for each replacement rate. Thereafter, specimens with the opt
... Show MoreMolecularly imprinted polymers (MIPs) are an effective method for separating enantiomeric compounds. The main objective of this research is to synthesize D-arabinitol MIPs, which can selectively separate D-arabinitol and its potential application to differentiate it from its enantiomer compound through a non-covalent approach. A macroporous polymer was synthesized using D-arabinitol as a template, acrylamide as a functional monomer, ethylene glycol dimethacrylate (EGDMA) being a cross-linker, dimethylsulfoxide (DMSO) being a porogen, as well as benzoyl peroxide being an initiator. After polymer synthesis, D-arabinitol was removed by a mixture of methanol and acetic acid (4:1, v/v). Fourier-Transform Infrared spectroscopy (FT-IR) and Scan
... Show MoreTwo field experiments were conducted during the spring season 2020 in Karbala governorate to study the effect of irrigation systems, irrigation intervals, biofertilizers and polymers on some characteristics of vegetative growth and potato production. The results showed that there were significant differences in the values of the average plant height due to the effect of the double interference between the irrigation system and the improvers, The height of potato plant under any irrigation system was superior when adding conditioners compared to the control treatment, as it reached 48.56, 58.00 and 64.33cm when adding polymer, biofertilizer, and polymers+ biofertilizers, respectively compared with the control treatment of 44.64cm in the surf
... Show MoreMoisture induced damage can cause a progressive deterioration in the performance of asphalt pavement by the loss of adhesion between asphalt binder and aggregate surface and/or loss of cohesion within the binder in the presence of water. The objective of this paper is to improve the asphalt mixtures resistance to moisture by using hydrated lime as an anti-stripping additive. For this purpose, two types of asphalt binder were utilized; asphalt grades (40-50) and (60-70) with one type of aggregate of 19.0 mm aggregate nominal maximum size, and limestone dust as a mineral filler. Marshall method was adopted to find the optimum asphalt content. Essentially, two parameters were determined to evaluate the moisture susceptibili
... Show MoreTwo grades of paving asphalt with penetration of 46 and 65 are studied for determining changes in their physical and chemical properties caused by ageing.
The ageing process has been conducted on two petroleum paving asphalt cement using thin film oven test at 150, 163 and 175 C, and ageing time 5, 10,15, 20, 25 and 30 hours. The effect of ageing time and temperature on penetration, kinematic viscosity, softening point, solubility in trichloroethylene, heat loss and changes in chemical composition are investigated. The results of thin film oven test process indicte that the asphaltenes concentration of all aged asphalt increases with increasing ageing time, while the opposite was observed for polar-aromatic and naphthene-aromatic. The