Corrosion inhibitors are widely used in industry to reduce the corrosion rate of metals and alloys. Corrosion inhibitors adsorb onto metallic surfaces and insulate them from deterioration. Plants abundant in nature offer a cost-effective replacement for toxic chemical inhibitors on the market. The current research used the potentiostatic polarization technique at room temperature to explore the inhibitory impact of water hyacinth extract on the corrosion of low-carbon steel specimens in a 3.5% NaCl solution. The Tafel curve was used to assess corrosion inhibition activity, with the best inhibition efficiency reaching 79.36% at a concentration of 200 ppm. Cyclic polarization indicated the type of corrosion was general corrosion. The surface of carbon steel was investigated using Scanning Electron Microscopy (SEM) and Fourier Transform Infrared Spectroscopy (FTIR). FTIR analysis reveals the presence of alkaloid compounds, which are known corrosion inhibitors. In addition, the polarization behavior indicates that this inhibitor acts as a mixed-type inhibitor. Kinetic and thermodynamic parameters have been obtained from temperature studies. The higher activation energy than the blank (26.17 kJ/mol to 46.4 kJ/mol) suggests that an inhibitor has been deposited on the metal surface that is corroding, providing a resist layer to prevent corrosion. The low-carbon steel dissolution process is exothermic, as evidenced by the negative enthalpy of activation value. A positive increase in the activation entropy during the formation of the film layer suggests more disordering.
Background: The demand for esthetic orthodontic appliances is increasing; so the esthetic orthodontic archwires were introduced. Among them, Teflon and Epoxy coated stainless steel archwires. The amount of force available from the archwire depends on the structural properties and susceptibility to corrosion. All metallic alloys are changed during immersion in artificial saliva, chlorhexidine mouthwash andtoothpaste, but their behaviors differ from one type to another. They corrode at different rates, which lead to decrease the amount of force applied to the teeth. This in vitro study was designed to evaluate the corrosion pits in stainless steel archwires coated with Teflon and with Epoxy in dry and after immersion in artificial saliva, chl
... Show MoreThe corrosion behavior of Titanium in a simulated saliva solution was improved by Nanotubular Oxide via electrochemical anodizing treatment using three electrodes cell potentiostat at 37°C. The anodization treatment was achieved in a non-aqueous electrolyte with the following composition: 200mL ethylene glycol containing 0.6g NH4F and 10 ml of deionized water and using different applied directed voltage at 10°C and constant time of anodizing (15 min.). The anodized titanium layer was examined using SEM, and AFM technique.
The results showed that increasing applied voltage resulted in formation titanium oxide nanotubes with higher corrosion resistance
The inhibitive effect of imidazol on the dissolution of Zn in (1M) HCl has been studied. The inhibion effect of imidazol ,protection efficiency and the corrosion rate of Zn in (1M) HCl were investigated at various concentrations (1x 10-3 – 5x10-3) M and tempearture range (285-328) K. The corrosion inhibitive of Zn by imidazol was studied using weight loss measurement and analytical titration of the amounts of dissolved zinc in acidic solution in presence and absent of imidazol. It was observed that imidazol led to protection efficiency reached to (88.93)% when (10)mM imidazol concentration was used. A linear relationship came true between (C/?) and (C); where (?) is the coverage of Zn surface by imidazol which could be obtained from
... Show MoreThe corrosion of low carbon steel boiler tubes in demi water had been investigated. The purpose of this investigation was to determine the change produced in corrosion behavior of the carbon steel as a result of the specific presence of chloride and copper ions in the water under different temperatures. For low carbon steel experiments, the temperature was taken in three levels (125, 175, and 215°C) under about 27 bar pressure and 1500 rpm in autoclave. Using weight loss technique, the corrosion rate ranges from (85 to 789 gmd) for low carbon steel boiler tubes.
Rotating cylinder electrode (RCE) is used . in weight loss technique , the salinity is 200000 p.p.m, temperatures are (30,5060,7080Co) . the velocity of (RCE) are (500,1500,3000 r.p.m). the water cut (30% , 50%). The corrosion rate of carbon steel increase with increasing rotating cylinder velocity. In single phase flow, an increase im rotational velocity from 500 to 1500 r.p.m, the corrosion rate increase from 6.88258 mm/y to 10.11563 mm/y respectively.
In multiphase flow, an increase in (RCE) from 500 to 1500 r.p.m leads to increase in corrosion rate from 0.786153 to 0.910327 mm/y respectively. Increasing brine concentration leads to increase in corrosion rate at water cut 30%.