Corrosion inhibitors are widely used in industry to reduce the corrosion rate of metals and alloys. Corrosion inhibitors adsorb onto metallic surfaces and insulate them from deterioration. Plants abundant in nature offer a cost-effective replacement for toxic chemical inhibitors on the market. The current research used the potentiostatic polarization technique at room temperature to explore the inhibitory impact of water hyacinth extract on the corrosion of low-carbon steel specimens in a 3.5% NaCl solution. The Tafel curve was used to assess corrosion inhibition activity, with the best inhibition efficiency reaching 79.36% at a concentration of 200 ppm. Cyclic polarization indicated the type of corrosion was general corrosion. The surface of carbon steel was investigated using Scanning Electron Microscopy (SEM) and Fourier Transform Infrared Spectroscopy (FTIR). FTIR analysis reveals the presence of alkaloid compounds, which are known corrosion inhibitors. In addition, the polarization behavior indicates that this inhibitor acts as a mixed-type inhibitor. Kinetic and thermodynamic parameters have been obtained from temperature studies. The higher activation energy than the blank (26.17 kJ/mol to 46.4 kJ/mol) suggests that an inhibitor has been deposited on the metal surface that is corroding, providing a resist layer to prevent corrosion. The low-carbon steel dissolution process is exothermic, as evidenced by the negative enthalpy of activation value. A positive increase in the activation entropy during the formation of the film layer suggests more disordering.
Aleppo bentonite was investigated to remove ciprofloxacin hydrochloride from aqueous solution. Batch adsorption experiments were conducted to study the several factors affecting the removal process, including contact time, pH of solution, bentonite dosage, ion strength, and temperature. The optimum contact time, pH of solution and bentonite dosage were determined to be 60 minutes, 6 and 0.15 g/50 ml, respectively. The bentonite efficiency in removing CIP decreased from 89.9% to 53.21% with increasing Ionic strength from 0 to 500mM, and it increased from 89% to 96.9% when the temperature increased from 298 to 318 K. Kinetic studies showed that the pseudo second-order model was the best in describing the adsorption sys
... Show MoreCooling towers is one of the most important unit in industry, they are used to dispose heat from cooling media used in the integrated units. The choice of the cooling media plays recently an important rule due to fresh-water scarcity. The use of saline as a cooling media become of growing interest, but the corrosion problem has to be taken in consideration. In this study the simultaneous effect of cooling tower operation parameters on the corrosion rate of mild-steel is considered. The role of NaCl content is found to be pronounced more than the working solution temperature and flowrate. The corrosion of mild-steel in these studied factors had shown an interesting result especially with the NaCl% content. Firstly, there was an increase in t
... Show MoreIn this research is to study the influence of the aging heat treatment on the pitting corrosion resistance of martensitic stainless steel (MSS), where a number of specimens from martensitic stainless steel were subjected to solution treatment at 1100 oC for one hour followed by water quenching then aging in the temperatures range (500-750) oC for different holding times (1,5,10,15&20) hr. Accelerated chemical corrosion test and immersion chemical corrosion test were performed on samples after heat treatment. The results of the research showed that the pitting corrosion resistance is significantly affected by the aging temperature. Where found that the aging samples at a temperature of 500 °C have the highest ra
... Show MoreThe experimental and theoretical methods were studied for inhibition of the corrosion titanium in HCl by using neomycin sulfate drug. The results of neomycin sulfate drug had good corrosion protection for titanium in hydrochloric acid and the inhibition efficiency (%IE) increasing with increasing concentration of drug because the neomycin sulfate drug had adsorption from acid solution on surface of titanium metal. The program of hyperchem-8.07 was used for theoretical study of the drug by molecular mechanics and semi-empirical calculations. Quantum chemical was studied drug absorption and electron transferred from the drug to the Titanium metal, also inhibition potentials of drug attachment with the (LUMO-HOMO) energy gap,
... Show MoreInternal curing is a method that has been advised to decrease the primary age cracking, mainly of concrete mixes using low (water to cementitious materials - w/cm) ratios corresponding to the self-compacting concrete-(SCC). This research aims to study the effect of the internal curing using saturated lightweight aggregate- (LWA) on the steel reinforcing corrosion in SCC. In this research, crushed bricks or thermostone were partially replaced by (20%) by the weight of sand and volumetrically measured. The results showed that the steel reinforcement of internally cured concrete showed a slight increase in corrosion up to 300 days of exposure to the saline solution (containing 3.5% NaCl). The ability of using the crushed bricks or thermostone
... Show MoreInternal curing is a method that has been advised to decrease the primary age cracking, mainly of concrete mixes using low (water to cementitious materials - w/cm) ratios corresponding to the self-compacting concrete-(SCC). This research aims to study the effect of the internal curing using saturated lightweight aggregate- (LWA) on the steel reinforcing corrosion in SCC. In this research, crushed bricks or thermostone were partially replaced by (20%) by the weight of sand and volumetrically measured. The results showed that the steel reinforcement of internally cured concrete showed a slight increase in corrosion up to 300 days of exposure to the saline solution (containing 3.5% NaCl). The ability of using the crushed bricks or thermostone
... Show MoreAn overall mathematical model for copper pipe corrosion in flowing water was derived based on mass transfer fundamentals where we introduced the effects of boundary layer velocity, bulk flow velocity and the surface oxide protective film on the corrosion rate. A set of experiments were conducted in a straight 10mm diameter copper pipe, flow of water include six velocities of maximum value 7.33m/sec at 200C and 350C. The good agreement between the calculated and experimental corrosion rate values were achieved , the agreement reached 92% .
This study is concerned with the effect of Deep Cryogenic Treatment (DCT) at liquid nitrogen temperature (-196 o C) on the mechanical properties and performance of low carbon steel (A858). The tests specimens were divided in to two groups, the first group was subjected to the conventional heat treatment of normalizing, and the second group was also normalized then subjected to (DCT). The results have shown that after (DCT), the Hardness, Tensile properties and the impact energy absorbed were all slightly increased. However the fatigue test showed some positive improvement in fatigue limit by 20(N/mm2 ), and the volume wear rates at different loads were significantly decreased after (DCT). The changes in microstructure due to (DCT) were c
... Show More