The deposition method of perovskite solar cell layers significantly impacts device functionality and the achievement of industrial goals. Aluminum (Al) nanoparticles with rutile titanium oxide (TiO2) nanoparticle thin films are fabricated on Fluorine Tin Oxide (FTO) glass substrates by nanosecond pulsed fiber laser deposition (PLD) to be used as a plasmonic electron transport layer (ETL) in perovskite solar cell (PSC). The effect of various pulsed fiber laser parameters on the structural, optical, and surface morphology on Al/TiO2 films is extensively examined utilizing a variety of measurement techniques; X-ray diffraction (XRD), Ultraviolet–visible (UV–Vis) spectroscopy, Field emission scanning electron microscopy (FE-SEM) and Atomic Force microscope (AFM). XRD demonstrates that Al/TiO2 thin films has a mixed phase (anatase/rutile). The minimum average crystallite size of Al/TiO2 thin films deposited at (2 W - 40 kHz) is (19.8 nm). The absorption spectrum of the deposited Al/TiO2 thin film at (10 W - 20 kHz) shows a red-shifted absorption peak at 316 nm, while 307 nm is detected at (2 W - 20 kHz). As the pulse repetition rate rise (40, 60 kHz), a new absorption peak in the UV spectral region at 341 nm was observed. FESEM images demonstrate the nanoparticles’ uniformity and polycrystalline nature. The shape of nanoparticles becomes more uniform and smaller size when the power increases. The minimum power required to get a uniform film is 0.8 W nm with suitable thickness of 398.8 obtained by fitting the thickness values curve of Al/TiO2 thin films. The elemental analysis examined by the EDX spectrum of Al/TiO2 thin films consists of oxygen, aluminum, and titanium. AFM images reveal a granular microstructure, and a flat texture, with the lowest surface roughness. The obtained results from the current study indicate that the structural, optical, and morphological properties can be controlled by varying the fiber laser parameters to deposit an efficient plasmonic Al/TiO2 thin films could be used as an electron transport layer which open new trends to improve the performance of perovskite solar cell.
The structural, optical properties of cupper indium gallium selenite (CuIn1-xGaxSe) have been studied. CuIn1-xGaxSe thin films for x=0.6 have been prepared by thermal evaporation technique, of 2000±20 nm thickness, with rate of deposition 2±0.1 nm/sec, on glass substrate at room temperature. Heat treatment has been carried out in the range (373-773) K for 1 hour. It demonstrated from the XRD method that all the as-deposited and annealed films have polycrystalline structure of multiphase. The optical measurement of the CIGS thin films conformed that they have, direct allowed energy gap equal to 1.7 eV. The values of some important optical parameters of the studied films such as (absorption coefficient, refractive index, extinction coeffici
... Show MoreCadmium sulfide and Aluminum doped CdS thin films were prepared by thermal evaporation technique in vacuum on a heated glass substrates at 373K. A comparison between the optical properties of the pure and doped films was made through measuring and analyzing the transmittance curves, and the effect of the annealing temperature on these properties were estimated. All the films were found to exhibit high transmittance in the visible/ near infrared region from 500nm to 1100nm.The optical band gap energy was found to be in the range 2.68-2.60 eV and 2.65-2.44 eV for CdS and CdS:Al respectively , with changing the annealing temperature from room temperature to 423K.Optical constants such as refractive index, extinction coefficient, and complex di
... Show MoreCarbides or nitrides thin films present materials with good mechanical properties for industrial applications as they can be coatings at low temperatures serve temperature sensitive surfaces. In this work the effect of the C percentage on the mechanical properties represented by the Young modulus (E) of combinatorial magnetron sputtered TiCx (34%x˂65%) has been studied. The structure of the produced films is TiC independent on the C concentration. The mechanical properties are increased with increasing the C concentration up to 50%, and then decreasing with further C % increasing. These results can be explained by considering the resultant residual stresses.
In this report Silver doped Tin Sulfide (SnS) thin films with ratio of (0.03) were prepared using thermal evaporation with a vacuum of 4*10-6 mbar on glass with (400) nm thickness and the sample annealing with ( 573K ). The optical constants for the wavelengths in the range (300-900) nm and Hall effect for (SnS and SnS:3% Ag) films are investigated and calculated before and after annealing at 573 K. Transition metal doped SnS thin films the regular absorption 70% in the visible region, the doping level intensification the optical band gap values from 1.5- 2 eV. Silver doped tin sulfide (SnS) its direct optical band gap. Hall Effect results of (SnS and SnS:3% Ag) films show all films were (p-type) electrical conductivity with resistivity of
... Show MoreThe present work aims to fabricate n-i-p forward perovskite solar cell (PSC) withئ structure (FTO/ compact TiO2/ compact TiO2/ MAPbI3 Perovskite/ hole transport layer/ Au). P3HT, CuI and Spiro-OMeTAD were used as hole transport layers. A nano film of 25 nm gold layer was deposited once between the electron transport layer and the perovskite layer, then between the hole transport layer and the perovskite layer. The performance of the forward-perovskite solar cell was studied. Also, the role of each electron transport layer and the hole transport layer in the perovskite solar cell was presented. The structural, morphological and electrical properties were studied with X-ray diffractometer, field emission s
... Show MoreIn the present work, pulsed laser deposition (PLD) technique was applied to a pellet of Chromium Oxide (99.999% pure) with 2.5 cm diameter and 3 mm thickness at a pressure of 5 Tons using a Hydraulic piston. The films were deposited using Nd: YAG laser λ= (4664) nm at 600 mJ and 400 number of shot on a glass substrate, The thickness of the film was (107 nm). Structural and morphological analysis showed that the films started to crystallize at annealing temperature greater than 400 oC. Absorbance and transmittance spectra were recorded in the wavelength range (300-
4400) nm before and after annealing. The effects of annealing temperature on absorption coefficient, refractive index, extinction coefficient, real and imaginary parts of d
The optical properties for the components CuIn(SexTe1-x)2 thin films with both values of selenium content (x) [0.4 and 0.6] are studied. The films have been prepared by the vacuum thermal evaporation method with thickness of (250±5nm) on glass substrates. From the transmittance and absorbance spectra within the range of wavelength (400-900)nm, we determined the forbidden optical energy gap (Egopt) and the constant (B). From the studyingthe relation between absorption coefficient (α) photon energy, we determined the tails width inside the energy gap.
The results showed that the optical transition is direct; we also found that the optical energy gap increases with annealing temperature and selenium content (x). However, the width of l