Enhancing asphalt binder performance through nano-SiO2 and nano-CaCO3 additives: Rheological and physical insights
...Show More Authors

During the last two decades, nanomaterial application has gained a significant attraction into asphalt technology due to their effect in enhancing asphalt binder improving the asphaltic mixture. This study will modify the asphalt binder with two different nano types, nano SiO2 and CaCO3, at levels ranging from 1% to 7%. The resulting optimum nano-modified Asphalt will be subject to a series of rheological tests, including dynamic shear rheometer (DSR), Viscosity, and bending beam rheometer (BBR) to determine asphalt binder sensitivity towards low-medium-high temperature range. Results indicate that both nano types improved the physical characteristics of Asphalt, and 5% by weight of Asphalt was suggested as a reasonable dosage of nano-SiO2 and nano-CaCO3 based on the overall desirability analysis of physical tests. The viscosity and temperature sensitivity of bitumen were improved by adding nano SiO2 and CaCO3. On the other hand, the asphalt rutting resistance's capabilities were improved at higher temperatures. In contrast, it decreases resistance against fatigue at intermediate temperatures due to the lowest phase angles and higher loss moduli. The BBR test, however, reveals a modest decrease in bituminous anti-cracking.

Scopus Clarivate Crossref
View Publication
Publication Date
Mon Apr 15 2013
Journal Name
Eng. & Tech. Journal,
Assessment the Impact of Different Hydrated Lime Addition Methods on Fatigue Life Characteristic
...Show More Authors

The purpose of this study is to evaluate the effect of hydrated lime addition methods as filler replacement on fatigue performance of Hot Mix Asphalt (HMA). Three types of addition methods of hydrated lime were introduced namely dry HL on dry aggregate and saturated surface aggregate above 3% and slurry HL on dry aggregate, ordinary Lime stone powder was reduced by three HL percentage (1.0, 2.0 and 3.0 %). The effect of different methods were investigated on the fatigue properties of HMA using, third-point flexural fatigue bending Test. Pneumatic Repeated Load System (PRLS) was carried out to establish the effect of hydrated lime on the fatigue failure criteria and to select the proper hydrated lime application methods on fatigue behavior o