Objective. This study aimed to evaluate and compare the force degradation of two types of elastomeric chains following different periods of immersion in zinc-containing mouthwashes. Materials and Methods. Four hundred and forty pieces of Elasto-Force and Super Elasto-Force elastomeric chains were divided into two control and eight experimental groups. The pieces were stretched to 25 mm on pins mounted on an acrylic block and stored in distilled water at 37°C. The experimental groups were immersed in four different types of mouthwash for one minute twice a day throughout the test period. Ten continuous thermocycles per day between cold and hot water baths (5–55°C) were carried out. Forces were measured at six-time intervals (initial, 24 hours, 1, 3, 6, and 8 weeks). The mean force was calculated and compared among different elastomeric chains, mouthwashes, and times using the t-test and one-way ANOVA test followed by Tukey’s HSD test. The level of significance was set at 0.05. Results. Both types of elastomeric chains had significant force degradation over time (74–79% at 8 weeks). The Super Elasto-Force generated a higher force level than the Elasto-Force elastomeric chain at all time points. SmartMouth Clinical DDS mouthwash had a significantly lower effect on force degradation than other mouthwashes with no significant difference compared to control groups. Conclusions. Depending on these results: there is no clinically significant difference between both types of elastomeric chains, although Super Elasto-Force delivered a higher force level. The pH of the mouthwashes could play a role in force degradation over time, rather than other ingredients including zinc. The SmartMouth mouthwash had the minimum effect on force degradation of elastomeric chains, followed by Halita, Listerine Total Care Zero, and Breath Rx, respectively.
Background: Green Tea is made from the leaf of the plant “Camellia sinensisâ€. Green tea is reported to contain thousands of bioactive ingredients including catechins which have shown great promise for having antimicrobial effects. Periodontal diseases represent one of the most prevalent diseases around the world and the main etiologic factor behind it, is plaque accumulation, in addition certain kinds of bacteria have been detected frequently in subjects suffering from periodontitis, Several studies suggested that the outcome of periodontal treatment is better if particular pathogens including Aggregatibacteractinomycetemcomitans can no longer be detected after therapy. Materials and Methods: plaque samples were collected from 2
... Show MoreBackground:The demand for esthetic orthodontic appliances is increasing so that the esthetic orthodontic archwires were introduced. This in vitro study was designed to evaluate the surface roughness offiber-reinforced polymer composite (FRPC) archwires compared to coated nickel-titanium (NiTi) archwires immersed in artificial saliva. Materials and Methods:Three types of esthetic orthodontic archwires were used: FRPC (Dentaurum), Teflon coated NiTi (Dentaurum) and epoxy coated NiTi (Orthotechnology). They were round (0.018 inch) in cross section and cut into pieces of 15 mm in length.Forty pieces from each type were divided into four groups; one group was left at a dry condition and the other three groups were immersed in artificial saliva (
... Show MoreBackground: Thermocycling simulates the temperature dynamics in the oral environment. This in vitro study done to measure and compare the effect of thermocycling on the shear bond strength of stainless steel and sapphire brackets bonded to human enamel teeth using light cured orthodontic adhesive and debonded at various time, and to measure adhesive remnant index after debonding. Materials and Methods: one-hundred-twenty extracted upper first premolars for orthodontic reason were used in this study; depending on weather thermocycled or not, the sample was divided into two main groups, then within each group 30 teeth were used for stainless-steel brackets (Bionic®) and for sapphire brackets (Pure®). Both groups were subdivided into three
... Show MoreBackground: This study aims to investigate the effect of fixed orthodontic appliances and/or antihypertensive drugs on the weight of experimental rats. Materials and Methods: Thir-ty-six male Wistar albino rats were subjected to a split-mouth design study, in which an orthodontic appliance was inserted in one side to move the first molar mesially for 2 weeks while the other side acted as a control to tooth movement. The rats were allocated into three groups: group A (n = 12), without any pharmacological treatment; group B (n = 12), subcu-taneous injection of bisoprolol fumarate (5 mg/kg) daily; and group C (n = 12), subcutaneous injection of valsartan (10 mg/kg) daily. A fixed orthodontic appliance with a closing coil spring delivering 5
... Show MoreBackground: Coated archwires have been introduced to improve esthetics during orthodontic treatment. Theaim of the present study was to evaluate and compare the load–deflection characteristics and force levels of six brands of coated nickel titanium orthodontic archwires using palatal and gingival deflection. Materials and methods: Ten round wires (0.016 inch) and ten rectangular wires (0.019x0.025 inch) were obtained from each of six brands (G&H, Opal, Ortho Technology, Dany, Hubit and Astar Companies). The load-deflection properties of these archwires were evaluated by the modified bending test usinga readymade dental arch model in both palatal and gingival directions at 37°C temperature using a universal material testing machi
... Show MoreBackground: Complete removal of filling material from the root canal is an essential requirement for endodontic retreatment. The purpose of the present study is to evaluate and compare the dissolving capabilities of various solvents (Xylene, Eugenate Desobturator, Eucalyptol, EDTA and Distilled water (as a control)) on four different types of sealer (Endofill, Apexit Plus, AH Plus and EndoSequence bioceramic sealer). Materials and method: Eighty samples of each sealer were prepared according to the manufacturers' instructions and then divided into ten groups (of 8 samples) for immersion in the respective solvents for 2 and 5 min immersion periods. Each sealer specimen was weighed to obtain its initial mass. The specimens were immersed in
... Show MoreMelatonin is a potent scavenger of reactive oxygen species or free radicals like superoxide and hydroxyl radicals. The oxidation of hemoglobin to methemoglobin (meth-Hb) by oxidizing compounds has been widely studied. The present work was designed to evaluate the ability of different concentrations of melatonin to inhibit nitrite–induced oxidation of hemoglobin. Blood samples were obtained from apparently healthy individuals from which erythrocyte hemolysate was prepared. Different concentrations of melatonin (10-9-1.0 mg/ml) were incubated for 10 min with the hemolysate, then to the resultant mixture 1 ml of sodium nitrite (final concentration 0.6 mM) was added, and the
... Show MoreEffects of Ozonated Water on Micro Leakage between Enamel and Fissure Sealants Prepared by Different Etching Technique (An in vitro Study), Baraa M Jabar*, Muna S Khalaf