Objective. This study aimed to evaluate and compare the force degradation of two types of elastomeric chains following different periods of immersion in zinc-containing mouthwashes. Materials and Methods. Four hundred and forty pieces of Elasto-Force and Super Elasto-Force elastomeric chains were divided into two control and eight experimental groups. The pieces were stretched to 25 mm on pins mounted on an acrylic block and stored in distilled water at 37°C. The experimental groups were immersed in four different types of mouthwash for one minute twice a day throughout the test period. Ten continuous thermocycles per day between cold and hot water baths (5–55°C) were carried out. Forces were measured at six-time intervals (initial, 24 hours, 1, 3, 6, and 8 weeks). The mean force was calculated and compared among different elastomeric chains, mouthwashes, and times using the t-test and one-way ANOVA test followed by Tukey’s HSD test. The level of significance was set at 0.05. Results. Both types of elastomeric chains had significant force degradation over time (74–79% at 8 weeks). The Super Elasto-Force generated a higher force level than the Elasto-Force elastomeric chain at all time points. SmartMouth Clinical DDS mouthwash had a significantly lower effect on force degradation than other mouthwashes with no significant difference compared to control groups. Conclusions. Depending on these results: there is no clinically significant difference between both types of elastomeric chains, although Super Elasto-Force delivered a higher force level. The pH of the mouthwashes could play a role in force degradation over time, rather than other ingredients including zinc. The SmartMouth mouthwash had the minimum effect on force degradation of elastomeric chains, followed by Halita, Listerine Total Care Zero, and Breath Rx, respectively.
The objective of this study was to investigate the effect of Royal jelly RJ on morphology and motility of mice sperms. Sperms were collected from the cauda region of the epididymis of each 10 mice from the treatment and control groups. Direct activation techniques and evaluation of sperm morphology were carried out. Dhino microscope was used for sperm measurement. The inspection was carried out in Salamatic laboratory for pathological analysis in 2015.The result revealed that all of the sperm function parameters registered significant activation in the treatment group. There was a significant increase in both the percentage of the sperm motility grade A and the progressive motility (A+B) of the treatment gr
... Show MoreMechanical degradation hampers the practical usage of polymers for turbulent drag reduction
application. Mechanical degradation refers to the chemical process in which the activation energy of
polymer chain scission is exceeded by mechanical action on the polymer chain, and bond rupture
occurs. When a water-soluble polymer and surfactant are mixed in water solution, the specific structures
(aggregates) are formed, in which polymer film is formed around micelle. In this work, Xanthan gum (XG) –
Sodium lauryl ether sulfate (SELS) complex formation and its effect on percentage viscosity reduction
(%VR) was studied. It was found that SELS surfactant reduced the mechanical degradation of XG much
more efficiently than th
In this research, design of advanced material for sunlight conversion requires focused research to obtain efficient photocatalytic system. Nanostructured ZnO was synthesized using spin coating technique. The structural, morphological and optical properties of annealed nanostructured ZnO thin film at 390 Co for 3 hours were characterized by x-ray diffraction, atomic force microscope AFM and UV-VIS spectrophotometer. Nanostructured ZnO was applied for removal Methylene Blue (MB) dye from water using sunlight induced photocatalytic process. Overall degradation of MB/ZnO was achieved after 120 minutes of sunlight irradiation while it needs more time for MB alone. The reaction rate constant fit pseudo first order for MB/ZnO degradation was 0.
... Show MoreIn this research, hand lay- up technique is used to prepare samples from epoxy resin reinforced with multi- walled carbon nanotubes in different weight fractions (0, 2, 3, 4, 5) wt%. The immersion effect by sodium hydroxide solution (NaOH) at normality (0.3N) for a period of (15 days) on the thermal conductivity of nanocomposites was studied, and compared to natural condition (before immersion). The thermal conductivity of epoxy nanocomposites specimens were carried out using Lee’s disk method. The experimental results showed that thermal conductivity increased with increase weight fraction before and after immersion for all specimens, while the immersion effect leads to decrease thermal conductive values compared to thermal conductivi
... Show MoreZSM-5 zeolite was synthesis under hydrothermal conditions at 175oC. The synthesis parameters have been investigated to find optimum synthesis method. Firstly, the crystallization time has been investigated to find the optimum crystallization time. Also, the ageing time was studied. The morphology, structure, and composition of the synthesized ZSM-5 zeolite were characterized using scanning electron microscopy (SEM), pH meter, viscometer, and X-ray powder diffraction (XRD). The bulk Si/Al ratio of ZSM-5 zeolite was in the range of 9.5—11.7. The synthesized ZSM-5 zeolite with appropriate ageing time could adjust crystal size and degree of the crystallinity. The crystal size of ZSM-5 zeolite obtained at an agei
... Show MoreThis study was conducted to determine the effects of concentration of hydrochloric acids, temperature, and time on the hydrolysis of soya proteins (defatted soya flour) by determining the value of total protein nitrogen concentration, and amino nitrogen concentration of protein, peptides, and amino acids, and then calculated the hydrolysis rate of proteins.
The variables of the conditions of hydrolysis process was achieved in this study with the following range value of tests parameter:
- Concentration of HCl solution ranged between 1-7 N,
- Hydrolysis temperature ranged between 35-95 °C, and
- The time of hydroly
This work has been done with using of epoxy resin mixed with Granite powder were weighted by percent volume (5,10,15, and 20)%and then mixed with epoxy polymer to compose polymer composite. Hand lay-up technique is used in fabrication of the composite samples. Hardness test was carried out for the proper samples in both normal condition and after immersion in HCL (1 M and 2 M) solutions for periods ranging up to 10 weeks. After comparing the results between the polymer and their composite, the hardness increased with increasing Granite weight percent, it was found that Hardness were greater for the composites before immersion compared with their values after immersion.
Abstract
The study aims to identify the levels of core competencies dimensions and types of organizational flexibility in the investigated organization, as well as to determine the nature of the relationship and the impact of core competencies dimensions with the process of organizational flexibility. Thus, a number of research questions were presented to express the research problem as follows:
- What is the level of the investigated individuals' awareness to core competencies and organizational flexibility across their dimensions and types in the investigated organization?
- To what extent are core competencies and organizational flexibility available in the Organiz