Background: The bond strength of root canal sealers to dentin and gutta-percha seems to be an important property for maintaining the stability of root canal filling, which potentially influences both leakage and root strength. The objective of this, in vitro, study was to evaluate the shear bond strength of three different endodontic sealers (Gutta-Flow, AH Plus, Apexit Plus) to dentin, in the presence and absence of the smear layer and gutta percha. Material and Methods: After slicing off the occlusal 2mm of 60 extracted human maxillary premolar teeth, the exposed dentin served as the tested surfaces; the teeth were fixed with cold cure acrylic, and were divided into two groups according to the smear layer presence, group A without smear
... Show MoreBackground: The present study was carried out to compare shear bond strength of sapphire bracket bonded to zirconium surface after using different methods of surface conditioning and assessment of the adhesive remnant index. Materials and methods: The sample composed of 40 zirconium specimens divided into four groups; the first group was the control, the second group was conditioned by sandblast with aluminum oxide particle 50 μm, the third and fourth group was treated by (Nd: YAG) laser (1064nm)(0.888 Watt for 5 seconds) for the 1st laser group and (0.444 Watt for 10 seconds) for the 2nd laser group. All samples were coated by z-prime plus primer. A central incisor sapphire bracket was bonded to all samples with light cure adhesive res
... Show MoreBackground: Debonding and fracture of artificial teeth from denture bases are common clinical problem, bonding of artificial teeth to heat cure acrylic and high impact heat cure acrylic denture base materials with autoclave processing method is not well known. The aim of this study was to evaluate the effect of autoclave processing method on shear bond of artificial teeth to heat cure denture base material and high impact heat cure denture base material. Materials and methods: Heat polymerized (Vertex) and high impact acrylic (Vertex) acrylic resins were used. Teeth were processed to each of the denture base materials after the application of different surface treatments. The sample (which consist of artificial tooth attached to the dentur
... Show MoreIn this study, a predicated formula is been proposed to find the shear strength of non-prismatic beams with or without openings. It depends on the contributions of concrete shear strength considering the beam depth variation and existing openings, shear steel reinforcements and defines the critical shear section, the effect of diagonal shear reinforcement, the effect of inclined tensile steel reinforcement, and the compression chord influence. The verification of the proposed formula has been conducted on the experimental test results of 26 non-prismatic beams with or without openings at the same loading conditions. The results reflect that the predicted formula finds the shear capacity of non-prismatic beams with openings, it is co
... Show MoreBackground: Sealers should demonstrate adhesive properties to dentin, decreasing the chance of endodontic treatment failure. Increased adhesive properties to dentin may lead to greater strength of the restored tooth, which may provide greater resistance to tooth fracture and clinical longevity of an endodontically treated tooth. The aim of this study was to evaluate the shear bond strength of Bioceramic iRoot SP sealer, AH plus sealer and Apexit plus sealer in absence or presence of smear layer using push out bond strength test. Materials and Methods: Sixty straight single roots of the mandibular premolars were selected for this study. All canals were instrumented using ProTaper rotary instruments to achieve tapered canal walls, instrumenta
... Show MoreBackground: The main drawback of soft lining materials was that they debonded from the denture base after a certain period of usage. Therefore, the purpose of this research was to determine the impact of oxygen and argon plasma treatment on the shear bonding strength of soft liners to two different kinds of denture base materials: conventional acrylic resin and high impact acrylic resin. Materials and Methods: Heat cure conventional and high impact acrylic blocks (40 for each group) were prepared. A soft liner connected the final test specimen of two blocks of each acrylic material. Shear bond strength (SBS) was assessed using universal testing machine. Additional blocks were also prepared for analyzing Vickers microhardness, contact ang
... Show MoreThe research presents a case study of collecting materials and raw materials in a visual space that allows them to form a perception and meanings that inform the recipient by reconstructing them and inserting them into the surface of the artistic work and in such a way that the aesthetic act consists of a variety of media, touches and surfaces. The overlap of races within an environment characterized by unity. That is why the researcher in chapter one presented the problem of research, and the focus was on studying the multiplicity of materials and their aesthetic and functional role in the structure of creative work. The aim of the research is enhanced to identify the aesthetic performance function of the multiplicity of ores in the col
... Show MoreBackground: evaluate the effects of three different intracoronal bleaching agents on the shear bond strengths (SBS) and failure site of stainless steel and monocrystalline (sapphire) orthodontic brackets bonded to endodontically treated teeth using light cured orthodontic adhesive in vitro. Materials and methods: Eighty extracted sound human upper first premolars were selected, endondontically treated and randomly divided equally (according to the type of the brackets used) into two main groups (n = 40 per group). Each main group were subdivided (according to the bleaching agent used) into four subgroups 10 teeth each; as following : control (un bleached) group, hydrogen peroxide group (Hp) 35%, carbamide peroxide group (CP) 37% group and s
... Show MoreBackground: The finite element method (FEM) is expected to be one of the most effective computational tools for measuring the stress on implant-supported restorations. This study was designed using the 3D-FEM to evaluate the effect of two adhesive luting types of cement on the occlusal stress and deformation of a hybrid crown cemented to a mono-implant. Materials and Method: The mono-screw STL file was imported into the CAD/CAM system library from a database supported by De-Tech Implant Technology. This was to assist in the accurate reproduction of details and design of a simulated implant abutment. Virtually, a digital crown was designed to be cemented on an abutment screw. A minimum occlusal thickness of 1mm and marginal fitting of 1.2
... Show More