The durability of asphalt concrete is highly dependent on the geometry and mineralogy of coarse aggregates, yet their combined influence on mechanical and moisture resistance properties is still not fully understood. This study evaluates the effects of coarse aggregate geometry, specifically flat and elongated particle ratios and angularity, as well as mineral composition (quartz versus calcite), on asphalt mixture durability. The durability of mixtures was evaluated through Marshall properties as well as moisture susceptibility indicators, including the tensile strength ratio (TSR) and index of retained strength (IRS). Statistical analyses (ANOVA and t-tests) were also conducted to confirm the significance of the observed effects. Results showed that mixtures containing higher proportions of flat and elongated particles exhibited greater void content, reduced stability, and weaker moisture resistance, with the 1:5 flat-to-elongated ratio showing the most adverse impact (TSR 73.9%, IRS 69.2%). Conversely, increasing coarse aggregate angularity (CAA) enhanced mixture performance, with TSR values rising from 63.5% at 0% angularity to 81.2% at 100% angularity, accompanied by corresponding improvements in IRS. Mineral composition analysis further demonstrated that calcite-based aggregates achieved stronger bonding with asphalt binder and superior resistance to stripping compared to quartz-based ones. These findings confirm that aggregate geometry and mineralogy exert a decisive influence on asphalt mixture durability. They also highlight the need to revise current specifications that permit the use of uncrushed coarse aggregate in asphalt base courses, particularly when such layers may serve as surface courses in suburban or low-volume roads, where long-term resistance to moisture damage is critical.
GFRP was employed in constructions as an alternative to steel, which has many advantages like lightweight, large tensile strength and resist corrosion. Existing researches are insufficient in studying the influence of hybrid reinforced concrete composite columns encased by GFRP I-section (RCCCEG) and I-section steel (RCCCES). In this study twenty one (RC) specimens of a cross-section of 130 mm × 160 mm, with different length (long 1600 mm and short 750 mm) were encased by using I-section (steel and GFRP) and tested under various loading (concentric, eccentric and flexural loads). The test was focused on the influence of many parameters; load-carrying capacity, mode of failure, deformation and drawing an interaction diagram (N-
... Show MoreMicrofinance Institutions (MFIs) offers small loans with easy repayment system and till now these institutions have served millions of needy people around the globe. This study highlights the hurdles influence the smooth working and growth of Microfinance institution in Egypt. The structured interviews were conducted from the top and mid-level managers of MFI's. This study revealed that interest rate, political and economic conditions, corruption, customer outreach, competition and technology are the important elements for MFI's success. It is evident that lack of use of technology and less importance drawn on customer outreach programs are the main challenges of MFI's in Egypt. This study provides a roadmap for practitioners and strategic
... Show MoreGypseous soil is considered as a problematic soil for embankment construction, however, implementation of emulsified asphalt as a stabilization agent could be a proper solution for enhancing its properties as a subgrade soil. In this work, the sustainability of asphalt stabilized soil has been assessed in terms of its resistance to cyclic (freezing-thawing) and (heating-cooling) processes. Specimens have been prepared at optimum fluid content (moisture and emulsion) and tested under direct shear stresses while subjected to 30 cycles of (freezing-thawing) and (heating-cooling). Both of dry and soaked testing conditions have been implemented. Data have been observed after each 10 cycles, and compared with that of reference mix. It was conclud
... Show MoreBackground: Due to the complicated and time-consuming physiological procedure of bone healing, certain graft materials have been frequently used to enhance the reconstruction of the normal bone architecture. However, owing to the limitations of these graft materials, some pharmaceutical alternatives are considered instead. Chitosan is a biopolymer with many distinguishing characteristics that make it one of the best materials to be used as a drug delivery system for simvastatin. Simvastatin is a cholesterol lowering drug, and an influencer in bone formation process, because it stimulates osteoblasts differentiation, bone morphogenic protein 2, and vascular endothelial growth factor. Objectives: histological, histochemical and histomorp
... Show MoreThe aim of this research is to develop qualitative workouts based on certain sensory perceptions for the development of offensive basketball abilities and to determine their impact on female pupils. Several findings, based on the au-thor's extensive expertise instructing basketball materials and our closeness to the sample, revealed deficits in some sensory perceptions “in the game of basketball”, which impair the accuracy of passing the ball to the best team-mate. It also affects the pace of dribbling and the difficulty of selecting the op-timal moment and distance to fire. Therefore, the researcher designs qualita-tive activities based on many sensory experiences, including distance, speed, force, and direction shift. In addition, the
... Show MoreThis paper presents an investigation to the effect of the forming speed on healing voids that inhabit at various size in an ingot. The study was performed by using finite element method with bilinear isotropic material option, circular type voids were considered. The closure index was able to predict the minimum press force necessary to consolidate voids and the reduction. The simulation was carried out, on circular cross-section lead specials containing a central void of different size. At a time with a flat die, different ratio of inside to outside radius was taken with different speed to find the best result of void closure.
This research studies the influence of water source on the compressive strength of high strength concrete. Four types of water source were adopted in both mixing and curing process these are river, tap, well and drainage water (all from Iraq-Diyala governorate). Chemical analysis was carried out for all types of the used water including (pH, total dissolved solids (TDS), Turbidity, chloride, total suspended solid (TSS), and sulfates). Depending on the chemical analysis results, it was found that for all adopted sources the chemical compositions was within the ASTM C 1602/C 1602M-04 limits and can be satisfactorily used in concrete mixtures. Mixture of high strength concrete for compressive strength of (60 MPa) was designed and checked using
... Show MoreTo achieve sustainability in the field of civil engineering, there has become a great interest in developing reactive powder concrete RPC through the use of environmentally friendly materials to reduce the release of CO2 gas produced from cement factories as well as contribute to the recycling of industrial wastes that have a great impact on environmental pollution.
In this study, reactive powder concrete was prepared using total binder content of 800 kg/m3, water to binder ratio (0.275), and micro steel fibers 1% by volume of concrete. The experimental program included replacing fly ash with (8, 12, 16) % by cement weight to find the optimal ratio, which achieved the best mechanical proper
... Show MoreDate palm fiber is one of the common wastes available in the M. E. countries essentially Iraq. The aim of search to investigate the performance and effects of fiber date palm on the mechanical properties of high strength concrete, this fiber was used in three ratio 2, 4 and 6 % by vol. of concrete at ages of (7, 28, 90) days. Results demonstrated improvement in the compressive strength increased 19.2 %, 23.6%, 24.9 % for 2%, 4%, 6% of fiber respectively at age 28 days. Flexural strength increases 47.6%, 66.2%, 93.8% form (2,4,6) % of fiber respectively at age 28 days. Density increase about 0.41%, 0, 61 % 0.69 % for (2,4,6) % of fiber respectively at age 28. Absorption water decrease