Denture bases are fabricated routinely using Poly(methyl methacrylate) (PMMA) acrylic resin. Yet, it is commonly known for its major drawbacks such as insufficient strength and ductility. The purpose of this study was to improve the performance of PMMA acrylic resin as a denture base material by reinforcement with surface treated lithium disilicate glass ceramic powder. The ceramic powder was prepared by grinding and sieving IPS e.max CAD MT blocks. Then, the powder was surface treated with an organosilane coupling agent (TMSPM) and added to PMMA in amount of 1%, 3%, 5% and 7% by weight. Characterizations of the powder was done by particle size analysis, XRD and FTIR. Transverse strength, Impact strength, Shore D hardness and surface roughness were tested for the prepared composites and neat PMMA. Particle size analysis showed that the average particle diameter was 1.46 µm. XRD confirmed the microstructure of IPS e.max CAD MT. FTIR showed the presence of TMSPM functional groups in the powder after treatment and there was a chemical interaction between the treated powder and the PMMA after the addition. One-way ANOVA and Tukey’s HSD test showed that there was a highly significant increase (P < 0.01) in transverse strength, impact strength and hardness with non-significant increase in roughness for 1% group. The mean values of 1% group were 67.3 MPa for transverse strength, 5.21 kJ/m2 for impact strength, 89.8 for Shore D hardness and 1.22 µm for surface roughness. While for control group, mean values were 59.3 MPa for transverse strength, 3.74 kJ/m2 for impact strength, 87.1 for Shore D hardness and 1.1 µm for surface roughness. However, with higher amounts of powder, there was a highly significant decrease in transverse strength and increase in roughness which was considered undesirable. In conclusion, reinforcing PMMA denture base material with 1% lithium disilicate glass ceramic powder may have the potential for enhancing the clinical performance of this material.
In this work, lanthanium (III) complexes were synthesized using by Schiff base ligand (L) derived from benzaldehyde and o-aminoaniline with five amino acids (AA) from glycine (Gly), L-alanine (Ala), L-valine (Val), L-asparagine (Asp) and DL- phenylalanine (Phe). The Schiff base ligand has been characterized by elemental analysis, (MASS, FTIR, 1HNMR, 13CNMR, UV-VIS) electronic spectra. The structures of the new complexes have been described of analysis of elements, molar conductivity, (UV-Vis electronic, FTIR, mass) spectra also magnetic moment. The molar conductivity values of the complexes indicat this every of complexes are electrolytes and other analytical studies reveal octahedral geometry for La (III) ion. The Schiff base ligand, five
... Show MoreMany tools and techniques have been recently adopted to develop construction materials that are less harmful and friendlier to the environment. New products can be achieved through the recycling of waste material. Thus, this study aims to use recycled glass bottles as sustainable materials.
Our challenge is to use nano glass powder by the addition or replacement of the weight of the cement for producing concrete with enhanced strength.
A nano recycled glass p
Sixteen new complexes with the general formula [M(L)2(H2O)2] were prepared resulting from the reaction of the two new Schiff base ligands, which are: - L1= (E)-5-((2-hydroxybenzylidene)amino)-2-phenyl-2,4-dihydro-3H-pyrazol-3-one) L2 = (E)-5-((2-hydroxy-3-methoxybenzylidene)amino)-2-phenylpyrazolidin-3-one) With divalent metal ions (manganese, cobalt, nickel, copper, zinc, cadmium, mercury) and (tetravalent platinum). Ligands was derived from the reaction of the amine (5-amino-2-phenyl-2,4-dihydro-3H-pyrazol-3-one) with Salicylaldehyde and ortho-vanillin, which is linked to the metal ions via the nitrogen atoms are the isomethene group and the oxygen is the hydroxide group of t
... Show MoreThis study aims to test ceramic waste's capacity to remove nickel from aqueous solutions through adsorption. Ceramic wastes were collected from the Refractories Manufacturing Plant in Ramadi. Through a series of lab tests, the reaction time (5, 10, 15, 20, 25, 30, 35, 40, 45, and 50 minutes, and Ni concentrations (20, 40, 60, and 80) were tested using ceramic wastes with a solid to liquid ratio of 2g/30ml. At a temperature of 30ºC, the pH, total dissolved solids (TDS), and electrical conductivity (EC) were all measured. The equilibrium time was set at 30 min. Thereafter, the sorption (%) somewhat increased positively with the Ni concentration. Freundlich's equation showed that the adsorption intensity is 1.1827 and the Freundlich c
... Show MoreThe effect of irradiation and exposure time of laser light on the fluorescence emission of DCM dye in PMMA polymer contained in the composition mold using different metals have been investigated. It was found that the fluorescence intensity decreases as the exposure time increases and then reaches stabilization at long times. The effect of the incident laser power on fluorescence intensity of DCM dye in PMMA polymer at 10-3 M and 20% mixing ratio, using copper disks of composition molds, has been studied too. It was observed that there is an upward knick in the curve at laser intensity of 19.2 W/cm2, which may be associated with the threshold for amplified spontaneous emission (ASE) or laser action. And at intensity higher than about 88.
... Show MoreDue to the advantages over other metallic materials, such as superior corrosion resistance, excellent biocompatibility, and favorable mechanical properties, titanium, its alloys and related composites, are frequently utilized in biomedical applications, particularly in orthopedics and dentistry. This work focuses on developing novel titanium-titanium diboride (TiB2; ceramic material) composites for dental implants where TiB2 additions were estimated to be 9 wt.%. In a steel mold, Ti-TiB2 composites were fabricated using a powder metallurgy technique and sintered for five hours at 1200 °C. Microstructural and chemical properties were analyzed by energy dispersive X-ray spectroscopy (EDX), scanning electron microscopy (SEM), and X-ra
... Show MoreIn this research, Zinc oxide (ZnO)/epoxy nanocomposite was synthesized by simple casting method with 2wt. % ZnO concentration. The aim of this work was to study the effect of pH and composite dosage on the photocatalytic activity of ZnO/ epoxy nanocomposite. Scanning electron microscopy (SEM) technique images proof the homogeneous distribution of ZnO nanoparticles in epoxy. A synthesized nanocomposite samples were characterized by Fourier Transform Infrared spectrometer (FTIR) measurements. Two spectra for epoxy and 2wt.% ZnO/epoxy nanocomposites were similar and there are no new bonds formed from the incorporation of ZnO nanoparticles. Using HCl and NaOH were added to Methylene blue (MB) dye (5ppm) to gat pH values 3 and 8. The degradat
... Show More