In this paper the analysis of the corrosion basic types destructions on an example of buildings constructions is carried out and the basic requirements to materials for designs in construction are defined. A classification of corrosion damage is proposed, which became a prerequisite for selecting the main indicators of materials that maximally affect the quality and durability. The main methods for determining the main indicators of corrosion damage are identified.
Abstract
The current research aims to identify the level of partnership between school and community agencies to improve secondary school outcomes for students with intellectual disabilities and develop strategies that help enhance community partnerships between schools and agencies. The researcher used the qualitative research approach; he utilized the interviews as a tool for data collection. The sample of research included (12) participants: three female school leaders, three male-school leaders, three female-school supervisors, and three male-school supervisors in schools that have programs for students with intellectual disabilities in Riyadh. The results of the study showed that the level of partnership bet
... Show MoreThis study has been carried out to evaluate the expression level of beta 2 microglobulin gene on patients infected by hepatitis C virus before and after treatment with interferon. The study included 117 hepatitis C patients comprising as 63 pre-treated patients, the range of age was between 20-65 year with a mean age of 48.12 ± 16.1 and 54 post-treated patients with age range was between 23-63 year with the mean of 46.1 ± 18.1. Also it was found that more than half of patients were located within third and fourth decade i.e. 30-49 year, with a percentage of 52.4% and 55.6 % for pre-treatment and post-treatment patients respectively. Moreover , regarding both groups, males are more than females with the ratio of ( 3.2:1) among p
... Show MorePurpose: Current denture liner materials suffer from low tear strength, poor abrasion resistance, weak bond strength to denture material, and increasing risk of denture stomatitis due to adherence. The aim of this study was to evaluate the effects of the addition of cellulose nanofibers (CNFs) to commercial soft denture liner material on the adherence of and physical and mechanical properties. Materials and Methods: CNFs at concentrations of 0.0, 0.5, and 1.0 wt.% were incorporated into a soft liner material. Antifungal effects were assessed by quantifying the adherence of . The Shore A hardness, tensile strength, peel bond strength, and surface roughness tests were employed to assess the properties of the denture liner materials. Chemica
... Show MoreA thin film of AgInSe2 and Ag1-xCuxInSe2 as well as n-Ag1-xCuxInSe2 /p-Si heterojunction with different Cu ratios (0, 0.1, 0.2) has been successfully fabricated by thermal evaporation method as absorbent layer with thickness about 700 nm and ZnTe as window layer with thickness about 100 nm. We made a multi-layer of p-ZnTe/n-AgCuInSe2/p-Si structures, In the present work, the conversion efficiency (η) increased when added the Cu and when used p-ZnTe as a window layer (WL) the bandgap energy of the direct transition decreases from 1.75 eV (Cu=0.0) to 1.48 eV (Cu=0.2 nm) and the bandgap energy for ZnTe=2.35 eV. The measurements of the electrical properties for prepared films showed that the D.C electrical conductivity (σd.c) increase
... Show MoreThis study offers numerical simulation results using the ABAQUS/CAE version 2019 finite element computer application to examine the performance, and residual strength of eight recycle aggregate RC one-way slabs. Six strengthened by NSM CFRP plates were presented to study the impact of several parameters on their structural behavior. The experimental results of four selected slabs under monotonic load, plus one slab under repeated load, were validated numerically. Then the numerical analysis was extended to different parameters investigation, such as the impact of added CFRP length on ultimate load capacity and load-deflection response and the impact of concrete compressive strength value on the structural performance of
... Show MoreThree-dimensional (3D) reconstruction from images is a most beneficial method of object regeneration by using a photo-realistic way that can be used in many fields. For industrial fields, it can be used to visualize the cracks within alloys or walls. In medical fields, it has been used as 3D scanner to reconstruct some human organs such as internal nose for plastic surgery or to reconstruct ear canal for fabricating a hearing aid device, and others. These applications need high accuracy details and measurement that represent the main issue which should be taken in consideration, also the other issues are cost, movability, and ease of use which should be taken into consideration. This work has presented an approach for design and construc
... Show MoreIn this study, several ionanofluids (INFs) were prepared in order to study their efficiency as a cooling medium at 25 °C. The two-step technique is used to prepare ionanofluid (INF) by dispersing multi-walled carbon nanotubes (MWCNTs) in two concentrations 0.5 and 1 wt% in ionic liquid (IL). Two types of ionic liquids (ILs) were used: hydrophilic represented by 1-ethyl-3-methylimidazolium tetrafluoroborate [EMIM][BF4] and hydrophobic represented by 1-hexyl-3-methylimidazolium hexafluorophosphate [HMIM][PF6]. The thermophysical properties of the prepared INFs including thermal conductivity (TC), density and viscosity were measured experimental
Industrial development has recently increased, including that of plastic industries. Since plastic has a very long analytical life, it will cause environmental pollution, so studies have resorted to reusing recycled waste plastic (sustainable plastic) to produce environmentally friendly concrete (green concrete). In this research, producing environmentally friendly load-bearing concrete masonry units (blocks) was considered where five concrete mixtures were compressed at the blocks producing machine. The cement content reduced from 400 kg/m3 (B-400) to 300 kg/m3 (B-300) then to 200 kg/m3 (B-200). While (B-380) was produced using 380 kg/m3 cement and 20 kg/m3 nano-sil
... Show MoreThe cement slurry is a mixture of cement, water and additives which is established at the surface for injecting inside hole. The compressive strength is considered the most important properties of slurry for testing the slurry reliability and is the ability of slurry to resist deformation and formation fluids. Compressive strength is governed by the sort of raw materials that include additives, cement structure, and exposure circumstances. In this work, we use micro silica like pozzolanic materials. Silica fume is very fine noncrystalline substantial. Silica fume can be utilized like material for supplemental cementations for increasing the compressive strength and durability of cement. Silica fume has very fine particles size less
... Show More