In this study, thin flms containing titanium dioxide (TiO₂), iron (III) oxide (Fe2O3) and cerium oxide (CeO2), with varying Fe2O3:CeO2 concentrations ranging from 0 to 30 wt% and 10 wt% gold nanoparticles (AuNPs), were prepared on glass using chemical spray pyrolysis. The structural, morphological, and sensing properties of the prepared thin flms were examined. XRD analysis revealed that a phase transformation occurred based on the dopant concentration: flms with x = 0 or 0.1 formed a polycrystalline anatase structure, whereas those with intermediate concentrations (x = 0.15 or 0.20) were amorphous. At higher doping concentrations (x = 0.25, 0.30), the structure developed a hematite Fe2O3, CeO2 and Au phase. Morphologically, atomic force microscopy (AFM) revealed that surface roughness initially decreased and then increased at the beginning of impurity introduction; however, at x = 0.15, roughness was signifcantly high. Gas sensing measurements were carried out through resistance measurements in the absence of, and exposure to, reducing gas (H2S) and oxidizing gas (NO2). The results showed that sensitivity and selectivity varied depending on the gas sensing performance. The addition of Fe2O3:CeO2 increased sensitivity to the reducing gas (H2S) signifcantly, reaching a peak response of 36.31 at x = 0.15 and an operating temperature of 423 K, whereas doping decreased sensitivity to the oxidizing gas (NO2). The highest sensitivity of 30.13 was achieved at x = 0.1, making this the most efective sensor for this gas at 523K.
In this study, a double frequency Q-switching Nd:YAG laser beam (1064 nm and λ= 532 nm, repetition rate 6 Hz and the pulse duration 10ns) have been used, to deposit TiO2 pure and nanocomposites thin films with noble metal (Ag) at various concentration ratios of (0, 10, 20, 30, 40 and 50 wt.%) on glass and p-Si wafer (111) substrates using Pulse Laser Deposition (PLD) technique. Many growth parameters have been considered to specify the optimum condition, namely substrate temperature (300˚C), oxygen pressure (2.8×10-4 mbar), laser energy (700) mJ and the number of laser shots was 400 pulses with thickness of about 170 nm. The surface morphology of the thin films has been studied by using atomic force microscopes (AFM). The Root Mean Sq
... Show MorePure and Fe-doped zinc oxide nanocrystalline films were prepared
via a sol–gel method using -
C for 2 h.
The thin films were prepared and characterized by X-ray diffraction
(XRD), atomic force microscopy (AFM), field emission scanning
electron microscopy (FE-SEM) and UV- visible spectroscopy. The
XRD results showed that ZnO has hexagonal wurtzite structure and
the Fe ions were well incorporated into the ZnO structure. As the Fe
level increased from 2 wt% to 8 wt%, the crystallite size reduced in
comparison with the pure ZnO. The transmittance spectra were then
recorded at wavelengths ranging from 300 nm to 1000 nm. The
optical band gap energy of spin-coated films also decreased as Fe
doping concentra
Thin films of highly pure (99.999%) Tellurium was prepared by high vacuum technique (5*10-5torr), on glass substrates .Thin films have thickness 0.6m was evaporated by thermal evaporation technique. The film deposited was annealed for one hour in vacuum of (5*10-4torr) at 373 and 423 K. Structural and electrical properties of the films are studies. The x-ray diffraction of the film represents a poly-crystalline nature in room temperature and annealed film but all films having different grain sizes. The d.c. electrical properties have been studied at low and at relatively high temperatures and show that the conductivity decreases with increasing temperature at all range of temperature. Two types of conduction mechanisms were found to d
... Show MoreBaTiO3 thin films have been deposited on Si (111) and glass substrates by using pulsed laser deposition technique. The films were characterized by using X-ray diffraction, atomic force microscope and optical transmission spectra. The films growth on Si after annealing at 873K showed a polycrystalline nature, and exhibited tetragonal structure, while on glass substrate no growth was noticed at that temperature. UV-VIS transmittance measurements showed that the films are highly transparent in the visible wavelength region and near-infrared region for sample annealing on glass substrate. The optical gap of the film were calculated from the curve of absorption coefficient (αhν) 2 vs. hν and was found tobe 3.6 eV at substrate temperature 5
... Show MoreThin films of pure and doped nano titanium dioxide (TiO2) were prepared using a chemical pyrolysis technique (CPS), with different nanosize graphene oxide (GO) concentrations in the range (3-9)wt%. The structural, morphological andoptical characteristics of these films were investigated. X-ray diffraction (XRD) technique measurements revealed that the structure properties of TiO2have polycrystalline structure with anatase phase. AFM analysis showed the grain size of TiO2 films with different concentrations was decreased after doping with high concentration of GO ratio. Roughness of these films decreased too after adding of GO impurity for all films from (7.65-5.6)nm except 5wt% percentage where increased to 13.7nm. Optical
... Show MoreIn this research tri metal oxides were fabricated by simple chemical spray pyrolysis technique from (Sn(NO3)2.20 H2O, Zn(NO3)2.6 H2O, Cd(NO3)2.4 H2O) salts at concentration 0.1M with mixing weight ratio 50:50 were fabricated on silicon substrate n-type (111). (with & without the presence of grooves by the following diemensions (20μm width, 7.5μm depth) with thickness was about ( 0.1 ±0.05 µm) using water soluble as precursors at a substrate temperature 550 ºC±5, with spray distance (15 cm) and their gas sensing properties toward H2S gas at different concentrations (10,50,100,500 ppmv) in air were investigated at room te
... Show MoreIn this work, pure and Ag-doped nickel oxide (NiO) thin films were deposited on glass substrates with different dopant concentrations (0.1, 0.2, 0.3 and 0.4 wt.%) by pulsed-laser deposition (PLD) technique at room temperature. These films were annealed at temperature of 450 °C. The structural and optical properties of the prepared thin films were studied. It was found that annealing process has lead to increase the transmittance of the deposited films. Also, the transmittance was found to increase with doping concentration of silver in the deposited NiO films. The optical energy gap was decreased from 3.5 to 3.2 eV as the doping concentration was increased to 0.4 %.
This paper reports the effect of Mg doping on structural and optical properties of ZnO prepared by pulse laser deposition (PLD). The films deposited on glass substrate using Nd:YAG laser (1064 nm) as the light source. The structure and optical properties were characterized by X-ray diffraction (XRD) and transmittance measurements. The films grown have a polycrystalline wurtzite structure and high transmission in the UV-Vis (300-900) nm. The optical energy gap of ZnO:Mg thin films could be controlled between (3.2eV and 3.9eV). The refractive index of ZnO:Mg thin films decreases with Mg doping. The extinction coefficient and the complex dielectric constant were also investigate.