The filler in the asphalt mixture is essential since it plays a significant role in toughening and stiffening the asphalt. Changes in filler type can lead the asphalt mixtures to perform satisfactorily during their design life or degrade rapidly when traffic and environmental effects are considered. This study aims to assess the impact of filler types such as limestone dust (LS) and hydrated lime (HL) on Marshall characteristics and moisture damage in asphalt mixtures. Three different percentages of HL were employed in this study to partially replace the LS mineral filler: 1.5, 2.0, and 2.5% by aggregate weight. Furthermore, a control mixture was created with 7% LS by overall aggregate weight for the wearing course layer. The Marshall method was used to obtain the optimal asphalt content and the asphalt mixes' volumetric properties. The optimum asphalt content was used to prepare the asphalt concrete mixes, which were then tested for moisture damage resistance using the indirect tensile strength (ITS) and the index of retained strength (IRS). The findings demonstrate that resistance to moisture damage can be significantly enhanced by partially substituting HL for the LS filler. This was verified by the fact that the optimum increase in the tensile strength ratio (TSR) was 7.29% at 2.5% of HL, and at the same HL percent, the greatest rise in the IRS was 9.81% compared with the control mix.
The aim of this research work is to study the effect of stabilizing gypseous soil, which covers
vast areas in the middle, west and south parts of Iraq, using liquid asphalt on its strength properties
to be used as a base course layer replacing the traditional materials of coarse aggregate and broken
stones which are scarce at economical prices and hauling distances.
Gypseous soil brought from Al-Ramadi City, west of Iraq, with gypsum content of 66.65%,
medium curing cutback asphalt (MC-30), and hydrated lime are used in this study.
The conducted tests on untreated and treated gypseous soil with different percentages of medium
curing cutback asphalt (MC-30), water, and lime were: unconfined compression strength, and o
The aim of this research work is to study the effect of stabilizing gypseous soil, which covers vast areas in the middle, west and south parts of Iraq, using liquid asphalt on its strength properties to be used as a base course layer replacing the traditional materials of coarse aggregate and broken stones which are scarce at economical prices and hauling distances. Gypseous soil brought from Al-Ramadi City, west of Iraq, with gypsum content of 66.65%, medium curing cutback asphalt (MC-30), and hydrated lime are used in this study. The conducted tests on untreated and treated gypseous soil with different percentages of medium curing cutback asphalt (MC-30), water, and lime were: unconfined compression strength, and one dimensional confine
... Show MoreModified asphalt is considered one of the alternatives to address the problems of deficiencies in traditional asphalt concrete, as modified asphalt addresses many of the issues that appear on the pavement layers in asphalt concrete, resulting from heavy traffic and vehicles loaded with loads that exceed the design loads and the large fluctuations in the daily and seasonal temperatures of asphalt concrete. The current study examined the role of polyphosphoric acid (PPA) as a modified material for virgin asphalt when it was added in different proportions (1%, 2%, 3%, 4%) of the asphalt weight. The experimental program includes the volumetric characteristics associated with the Marshall test, the physical properties, and th
... Show MoreThe excessive permanent deformation (rutting) in asphalt-concrete pavements resulting from frequent repetitions of heavy axle loads is studied in this paper. Rutting gradually develops with additional load applications and appears as longitudinal depressions in the wheel path. There are many causes of the rutting of asphalt roads, such as poor asphalt mixing and poor continuous aggregate gradation. All factors affecting the mixture resistance to permanent deformation must be discussed, and all must be properly considered to reduce the rutting propensity of asphalt-aggregate mixtures. In this study, several mixtures were produced with the most common techniques in rutting resistance (using the most effective additives for each mixture), and
... Show More
In past years, structural pavement solution has been combined with destructive testing; these destructive methods are being replaced by non-destructive testing methods (NDT). Because the destructive test causes damage due to coring conducted for testing and also the difficulty of adequately repairing the core position in the field. Ultrasonic pulse velocity was used to evaluate the strength and volumetric properties of asphalt concrete, of binder course. The impact of moisture damage and testing temperature on pulse velocity has also been studied. Data were analyzed and modeled. It was found that using non-destructive testing represented by pulse velocity could be useful to predict the quality of asphalt c
... Show MoreThis experiment was conducted in field of Agricultured Department Baquba/Diyala province in spring season 2011 to study the water stress by using foliar application concentrations of each Proline acid and Abscisic acid on proline content , ABA content , chlorophyll content, protein conten and water content in leaves of Maize( cultivar, Buhooth 106). The layout of the experiments was Split- split plot design as RCBD with three replicates. The three concentrations of spraying Proline acid levels ( 0 , 150 , 200 mg Proline .l-1 ) Three Abscisic acid levels ( 0 , 15 , 20 mgABA.l-1. ) and three periods of irrigation after(25, 50, 75%) of available water . Folair fertilizer were applied at three
... Show MoreGas hydrate formation is considered one of the major problems facing the oil and gas industry as it poses a significant threat to the production, transportation and processing of natural gas. These solid structures can nucleate and agglomerate gradually so that a large cluster of hydrate is formed, which can clog flow lines, chokes, valves, and other production facilities. Thus, an accurate predictive model is necessary for designing natural gas production systems at safe operating conditions and mitigating the issues induced by the formation of hydrates. In this context, a thermodynamic model for gas hydrate equilibrium conditions and cage occupancies of N2 + CH4 and N2 + CO4 gas mix
The aim of this study to investigate the microbial load and type of preservative for the types of yogurt available in the Iraqi market to ensure the safety of food provided to the consumer and protect through examining the types of yogurt from harmful bacteria as well as to contain ratios acceptable to yeasts and molds is to find out by comparing models curd careless Iraqi standard quality(ISQ) and see how they conform to these specifications have been collecting 12 brands of yoghurt types it was been (Kala, Activia 1, Activia 2, Mazia, Shelan, Aib, Mersin, Morsi, Al-Safi, Zabady, Zakho, Arbil). Bacteriological tests were conducted on samples of yogurt (total bacterial count, coliform count, counting yeasts and molds). The results showed
... Show More