The filler in the asphalt mixture is essential since it plays a significant role in toughening and stiffening the asphalt. Changes in filler type can lead the asphalt mixtures to perform satisfactorily during their design life or degrade rapidly when traffic and environmental effects are considered. This study aims to assess the impact of filler types such as limestone dust (LS) and hydrated lime (HL) on Marshall characteristics and moisture damage in asphalt mixtures. Three different percentages of HL were employed in this study to partially replace the LS mineral filler: 1.5, 2.0, and 2.5% by aggregate weight. Furthermore, a control mixture was created with 7% LS by overall aggregate weight for the wearing course layer. The Marshall method was used to obtain the optimal asphalt content and the asphalt mixes' volumetric properties. The optimum asphalt content was used to prepare the asphalt concrete mixes, which were then tested for moisture damage resistance using the indirect tensile strength (ITS) and the index of retained strength (IRS). The findings demonstrate that resistance to moisture damage can be significantly enhanced by partially substituting HL for the LS filler. This was verified by the fact that the optimum increase in the tensile strength ratio (TSR) was 7.29% at 2.5% of HL, and at the same HL percent, the greatest rise in the IRS was 9.81% compared with the control mix.
The construction of highly safe and durable buildings that can bear accident damage risks including fire, earthquake, impact, and more, can be considered to be the most important goal in civil engineering technology. An experimental investigation was prepared to study the influence of adding various percentages 0%, 1.0%, and 1.5% of micro steel fiber volume fraction (Vf) to reactive powder concrete (RPC)—whose properties are compressive strength, splitting tensile strength, flexural strength, and absorbed energy—after the exposure to fire flame of various burning temperatures 300, 400, and 500 °C using gradual-, foam-, and sudden-cooling methods. The outcomes of this research proved that the maximum reduction in mechanical prop
... Show MoreThis study was carried out in Plant Tissue Culture Labs, College of Agricultural Engineering Sciences, University of Baghdad from November 2018 to June 2019. Fresh stem cuttings, 5 cm long were selected from 6-month old C-35 Citrange rootstock. Five concentrations of BA (0, 1, 1.5, 2 and 2.5 mg.L-1) were studied and addition of meta-Topolin (mT) at four concentrations (0, 1, 5 and 10 mg.L-1) was also studied to find out its effect individually on shoot number and shoot length in multiplication stage. Rooting media supplemented with four concentrations of IBA (0, 1, 2 and 3 mg.L-1) was also studied to find out its effect on rooting percentage, root number and root length. Results showed that BA as concentration of 2.5mg.L-1 significantly gav
... Show MoreThe effect of the aqueous extract of fig (Ficus carica) fruit was studied by using different concentrations of this fruit (15, 20 and 25 mg/kg of body weight) on some hematological parameters (hemoglobin concentration, packed cell volume, white blood cell count and platelets count) in female rabbits. Twenty female rabbits were randomly divided into four groups (five animals in each group). Three groups were dosed with the concentrations mentioned above, while the last was administered with distilled water and considered as control group. These animals were orally dosed by aqueous extract using a micropipette. The results showed that there was a significant (P<0.05) increase in hemoglobin concentration and packed cell volume means for all
... Show MoreIn this study, geopolymer mortar was designed in various experimental combinations employing 1% micro steel fibers and was subjected to different temperatures, according to the prior works of other researchers. The geopolymer mortar was developed using a variety of sustainable material proportions (fly ash and slag) to examine the influence of fibers on its strength. The fly ash weight percentage was 50%, 60%, and 70% by slag weight to study its effect on the geopolymer mortar's properties. The optimal ratio produced the most significant results when mixed at a 50:50 ratio of fly ash and slag with 1% micro steel fibers at curing temperature 240oC for 4 hours through two days. The compressive strength of the geopolymer mortar increas
... Show MoreThis research foxed on the effect of fire flame of different burning temperatures (300, 400 and 500)oC on the compressive strength of reactive powder concrete (RPC).The steady state duration of the burning test was (60)min. Local consuming material were used to mixed a RPC of compressive strength around (100) MPa. The tested specimens were reinforced by (3.0) cm hooked end steel fiber of (1100) MPa yield strength. Three steel fiber volume fraction were adopted in this study (0, 1.0and 1.5)% and two cooling process were included, gradual and sudden. It was concluding that increasing burning temperature decreases the residual compressive strength for RPC specimens of(0%) steel fiber volume fraction by (12.16, 19.46&24.49) and (18.20, 27.77 &3
... Show MoreThis experiment was carried out in one of the fields (A) affiliated to the College of Agricultural Engineering Sciences / University of Baghdad, for the spring season 2021, On hybrid tomato plants (Mayai Mayai) to test flower viability, using two factors, the first was three levels of irrigation interval (2, 4, 6) days, and the second factor three concentrations of compound Nano fertilizer with concentrations (0, 1.5, 2.5) gm liter-1, so that the number of treatments is 9 treatments and three replications, the number of experimental units is 27 experimental units distributed randomly according to the random drawing method to ensure reducing experimental error and obtaining the most accurate results. A factorial experiment 3 x 3 x 3 was carr
... Show MoreThin films of ZnSxSe1-x with different sulfide content(x)
(0, 0.02, 0.04, 0.06, 0.8, and 0.1), thickness (t) (0.3, 0.5, and 0.7 μm) and annealing temperature (Ta) (R.T 373 and 423K) were fabricated by thermal evaporating under vacuum of 10-5 Toor on glass substrate. The results show that the increasing of sulfide content (x)and annealing temperature lead to decrease the d.c conductivity σDC of and concentration of charge carriers (nH) but increases the activation energy (Ea1,Ea2), while the increasing of t increases σDC and nH but decrease (Ea1,Ea2). The results were explained in different terms