To learn how the manner of preparation influences film development, this study examined film expansion under a variety of deposition settings. To learn about the membrane’s properties and to ascertain the optimal pretreatment conditions, which are represented by ambient temperature and pressure, Laser pressure of 2.5[Formula: see text]m bar, the laser energy density of 500[Formula: see text]mJ, distortion ratio ([Formula: see text]) as a function of laser pulse count, all achieved with the double-frequency Nd: YAG laser operating in quality-factor mode at 1064[Formula: see text]nm. MgxZn[Formula: see text] films of thickness [Formula: see text][Formula: see text]nm were deposited on glass substrates at pulse frequencies of (1–6)[Formula: see text]Hz and pulse durations of 10[Formula: see text]ns. The spectrum of rays. The X-rays demonstrated that the diffraction peaks’ findings show that the crystallinity of the films is highly dependent on the quantity of magnesium present in the layers. All the generated movies feature a polycrystalline hexagonal membrane structure, with the (101) plane being the main reflection. The average particle size was determined to be less than 50[Formula: see text]nm using FE-SEM measurements, and (RMS) of the surface roughness of the membranes MgxZn[Formula: see text] may be calculated using AFM analysis. The spectrum spans from (300)[Formula: see text]nm to (900) nm in wavelength. All films have a transmittance rate of more than 70% for the visible area of the spectrum[Formula: see text][Formula: see text][Formula: see text](400–800)[Formula: see text]nm, and in one model, it reaches greater than 95%. The energy gap (Eg) for these films is (2.68, 2.6, 2.4 and 2.32) electron volts, with a standard deviation of (100, 200, 300, and 400) shoot. In addition, the energy gap values drop as the laser pulse strength increases, and the range in which these values may be set is quite narrow (2.68–2.32).
Study was made on the optical properties of Ge2oSe8othinfilms prepared by vac-uum evaporation as radiated by (0,34,69) Gy of 13 ray.The optical band gab Eg and tailing band A.Et were studied in the photon energy range ( 1 to 3)eV. The a-Ge20Se8o film was found to be indirect gap with energy gap of (1.965,1.9 , 1.82) eV at radiated by B ray with absorption doses of (0,34,69)Gy respectively.The Ea and AEt of Ge20Se80 films showed adecrease in E8 and an increase in AEt with radiation. This be-havior may be related to structural defects and dangling bonds.
One of the most important problems that faces the concrete industry in Iraq is the deterioration due to internal sulfate attack , since it reduces the compressive strength and increases the expansion of concrete. Consequently, the concrete structure may be damage .The effects of total and total effective sulfate contents on high strength concrete (HSC) have been studied in the present study.
The research studied the effect of sulfate content in cement , sand and gravel , as well as comparing the total sulfate content with the total effective SO3 content. Materials used were divided into two groups of SO3 in cement ,three groups of SO3 in sand ,and two groups of SO
... Show MoreBackground: Denture lining materials are widely used in prosthodontic treatment and management of traumatized oral mucosa. A contaminated prosthesis can provide a source of cross-contamination between patients and dental personnel as well as a cause for denture stomatitis. Therefore, denture disinfection has been recommended as an essential procedure for maintenance of a healthy oral mucosa. This study investigated the effect of SOLO disinfectant solution on some properties of different denture lining materials. Materials and methods: Three different solutions were used in this study; SOLO disinfectant solution, sodium hypochlorite solution, and water on three types of acrylic denture lining materials; hot cure, cold cure, and soft acrylic
... Show MoreThis paper examines the mechanical properties of a composite material made of modified Iraqi gypsum (juss) reinforced with polypropylene fibers. The modified juss was prepared by adding two percentages of cement (5, 10) %. Two percentages of polypropylene fibers were used, to reinforce the modified juss (1, 2) %. The water/dry compound ratio used was equal to 0.53%. The composite was evaluated based on compressive strength, flexural strengths, absorption percentage, density, acoustic impedance, ultra - pulse velocity, longitudinal shrinkage and setting time tests. The results indicated that the inclusion of cement on to juss increases the compressive strength, absorption percentage, density, acoustic impedance, ultra - pulse velocit
... Show MoreConventional flexible pavements are released to different types of failure in the initial phases of their service life due to high traffic density, high speeds, heavy loads, and harsh climates. To eliminate pavement damage and failure early, the present search investigates the impact of adding glass, steel, and basalt fibers in the asphalt mixtures. Also, the study evaluates these materials characteristics compared to the mixtures without fibers. The Marshall test and tensile strength ratio test (TSR) were utilized to evaluate the asphalt mixture's performance. A set of specimens were produced by incorporating glass fiber (GF), steel fiber (SF), and basalt fiber (BF) at (0.10%, 0.15%, 0.20%), (0.25%, 0.35%, 0.45%), and (0.15%, 0.35%
... Show MoreThe electrical properties of the AlNiCo thin films with thickness (1000oA) deposited on glass substrates using Ion – Beam sputtering (IBS) technique under vacuum <10-6 torr have been studied . Also it studied the effect of annealing temperature from this films , It is found that the effective energy decrease with increase of temperature and the conductivity decrease with increase temperature 323oK but after this degree the conductivity increasing .
Free cement refractory concrete is a type of refractory concrete with replacing alumina cement by bonding materials such as white kaolin, red kaolin and fumed silica. The free cement refractory concrete used in many applications like Petrochemicals, iron furnaces and cement production industries. The research clarifies the effect of steel fibers with two types crimped steel fibers and hooked steel
fibers with percentages 0.5%, 1% and 1.5% by volume from weight of bauxite aggregates. The additions of steel fibers with two types gave good properties in high temperatures where the specimens keep the dimension without failure and the properties made the best. the percentage of increasing for thermal conductivity was 44% for 1.5% crimped
Portland cement is considered the most involved product in environmental pollution. It is responsible for about 10% of global CO2 emissions [1]. Limestone dust is a by-product of limestone plants and it is produced in thousands of tons annually as waste material. To fulfill sustainability requirements, concrete production is recommended to reduce Portland cement usage with the use of alternative or waste materials. The production of sustainable high strength concrete by using nanomaterials is one of the aims of this study. Limestone dust in 12, 16, and 20% by weight of cement replaced cement in this study. The study was divided into two parts: the first was devoted to the investigation of the best percentage of replacement of waste
... Show MoreNo-fine concrete (NFC) is cellular concrete and it’s light weight concrete produced with the exclusion of sand from the concrete. This study includes the mechanical properties of lightweight reinforced by steel fiber, containing different proportions of steel fiber. This study was done using number of tests. These tests were density, compressive strength, flexural strength and absorption. These tests of the molds at different curing time. The results of tests that implication of fiber to No. fine concrete did not affect significantly on the compressive strength, While the flexural strength were gets better. Results explained that, the flexural strength of (1%) fiber No- fine concrete molds are four times that of the reference mold
... Show MoreBackground: Deterioration of maxillofacial silicone properties due to microbial colonization is a common problem and leads to the replacement of the prosthesis. Incorporation of the antimicrobial agent into the silicone could be a solution. The purpose of this study was to evaluate the effect of silver-zinc zeolite addition on some mechanical properties of a maxillofacial silicone (VST-50). Materials and methods: Total 120 specimens were fabricated and divided into 3 groups: 40 specimens for tear strength test, 40 specimens for tensile and percentage of elongation tests and 40 specimens for Shore A hardness and surface roughness. Each group was divided into 4 subgroups according to the amount of zeolite added (0% “control”, 0.5%, 1% and
... Show More