Manganese dioxide rotating cylinder electrode prepared by anodic deposition on a graphite substrate using MnSO4 solution in the presence of 0.918 M of H2SO4. The influence of different operational parameters (MnSO4 concentration, current density, time, and rotation speed) on the structure, and morphology of MnO2 deposit film was examined widely. The structure and crystal size determined by X-ray diffraction (XRD), the morphology examined by scanning electron microscopy (SEM) and atomic force microscopy (AFM) techniques. The γ-MnO2 obtained as the main product of the deposition process. It found that the four parameters have a significant influence on the structure, morphology, and roughness of the prepared MnO2 deposit. The crystal size increases with MnSO4 concentration, current density, and rotation speed, and decreasing with time, while the roughness decreases with increasing all of four parameters. It found that the optimum conditions used in preparing MnO2 rotating electrode that gave the smallest crystal size, low roughness and less cracking were 0.33 M of MnSO4, 6 mA/cm2, 2 h, and 200 rpm. Electrochemical oxidation of phenol in a batch reactor was carried out in the presence of NaCl to examine the performance of the prepared MnO2 electrode for degrading phenol and any organic byproducts at different current densities. The results indicate that as the current density increased from 25 to 100 mA/cm2, the chemical oxygen demand (COD) removal efficiency was increased from 59.26 to 99.90%. Kinetics and the effect of temperature on the COD disappearance have been studied. It was clear that COD decreases with time and as the temperature increases, and the value of reaction order equals to 1 as has been found.
Herein, the interfacial polymerization method has been used for the synthesis of PPy/NaVO3 composites with different compositions of NaVO3 (10 %, 20 %, 30 %, 40 % and 50 %) as an efficient electrode material for supercapacitors. The successful formation and composition of the as-prepared composites (PV1-PV5) were confirmed by FTIR, XRD, EDX, and SEM analysis. The electrochemical properties were investigated by cyclic voltammetry (CV), galvanometric charge–discharge measurement (GCD), and electrochemical impedance spectroscopy (EIS) in 0.5 M H2SO4 electrolyte. As compared to other, the PV4 composite exhibit excellent specific capacitance of 391 F g−1 at a current density of 0.75 A/g with good cycling stability of ∼59 % after 1000 cycle
... Show MoreThis research includes depositionof thin film of semiconductor, CdSe by vaccum evaporation on conductor polymers substrate to the poly aniline where, the polymer deposition on the glass substrats by polymerization oxidation tests polymeric films and studied the structural and optical properties through it,s IR and UV-Vis , XRD addition to thin film CdSe, on of the glass substrate and on the substrate of polymer poly-aniline and when XRD tests was observed to improve the properties of synthetic tests as well as the semiconductor Hall effect proved to improve the electrical properties significantly
A new Schiff bases ligand 4- ((2-hyolroxy phenylimino) methyl) -2, 6-dimethoxyphenol derived from condensation of 2- amino phenol with 4-hydroxy -3, 5-dimethoxy benzaldehyde have been synthesized and characterized by spectroscopy, spectra, Mass spectrum and elemental microanalysis (C.H.N). Metal Complexes with ions have been also synthesized and characterized spectroscopic methods spectroscopy, flame atomic absorption, molar conductivity measurements and magnetic susceptibility. These studies indicate that the moler ratio for the complexes. The complexes showed characteristics octahedral geometry with the (O,N) ligand coordinated in bidentate mode while with showed square planer. The enzyme activity of the ligand and i
... Show MoreThis work presents an innovative approach to enhancing the performance of concrete with reclaimed asphalt pavement (RAP) aggregates using titanium dioxide (TiO2) nanoparticles. Traditional limestone coarse aggregates were partially replaced with 30% and 50% RAP aggregates; a subset of mixtures containing RAP aggregates was treated with TiO2 nanoparticles. The rheological, mechanical, and long-term properties of concrete, along with changes in its chemical composition following the addition of RAP and TiO2, were evaluated. Results revealed that using 30% and 50% RAP in concrete mixtures reduced their compressive strength by 18% and 27%, respectively. However, using TiO2 in those mixtures enhanced their compressive strength by 8.7% an
... Show MoreNew series of metal ions complexes have been prepared from the new ligand 1,5- Dimethyl-4- (5-oxohexan-2- ylideneamino) -2-phenyl- 1H-pyrazol-3 (2H)-one derived from 2,5-hexandione and 4-aminophenazone. Then, its V(IV), Ni(II), Cu(II), Pd(II), Re(V) and Pt(IV) complexes prepared. The compounds have been characterized by FT-IR, UV-Vis, mass and 1H and 13C-NMR spectra, TGA curve, magnetic moment, elemental microanalyses (C.H.N.O.), chloride containing, Atomic absorption and molar conductance. Hyper Chem-8 program has been used to predict structural geometries of compounds in gas phase, the heat of formation, (binding, total and electronic energy) and dipole moment at 298 K.
A new method for the determination of the drug cefalexin in some Pharmaceuticals using (UV-Vis) and indirect Flame Atomic Absorption Spectrophotometer (FAAS) , Fe III should forms a chelating complex with cefalexin (CEX –Fe III) at pH (1-8) and the best pH for the formation of (CEX –Fe III) chelating complex was (2) .The complex extracted with Methanol and Dimethy-Sulphoxide .The mole-ratio method has been used to determine the structure of chelate (CEX - Fe III) and found to be 2:1 LM ( Ligand : Metal.) .
Keywords : Cefalexin , chelating complex.
The exploitation of obsolete recyclable resources including paper waste has the advantages of saving resources and environment protection. This study has been conducted to study utilizing paper waste to adsorb phenol which is one of the harmful organic compound byproducts deposited in the environment. The influence of different agitation methods, pH of the solution (3-11), initial phenol concentration (30-120ppm), adsorbent dose (0.5-2.5 g) and contact time (30-150 min) were studied. The highest phenol removal efficiency obtained was 86% with an adsorption capacity of 5.1 mg /g at optimization conditions (pH of 9, initial phenol concentration of 30 mg/L, an adsorbent dose of 2 g and contact time of 120min and at room temperature).
... Show More