The adsorption of copper ions onto produced activated carbon from banana peels (with particle size 250 µm) in a single component system with applying magnetic field has been studied using fixed bed adsorber. The fixed bed breakthrough curves for the copper ions were investigated. The adsorption capacity for Cu (II) was investigated. It was found that 1) the exposure distance (E.D) and strength of magnetic field (B), affected the degree of adsorption; and 2) experiments showed that removal of Cu ions and accumulative adsorption capacity of adsorbent increase as the exposure distance and strength of magnetic field increase.
The aqueous extract of banana fruits peal was tested for its effect on mitosis . The root tips of Allium cepa were used as plant test system and the bone marrow cells of the albino mice Mus musculus were used as mammalians test system in vivo .Root tips of Allium cepa were treated for four hours with five concentrations of the extract (5 , 10 , 20 , 40 ,60 mg / ml.).The Metaphase was arrested in all the treatments , the highest percentage ( 100 % ) was recorded in the first concentration , the last concentration caused stickiness and clumping of the chromosomes. The treatments did not cause significant difference in the mitotic index. The peals extract (5 mg /ml) was compared with the extracts of fruits bulb, leaves and roots of
... Show MoreThe aqueous extract of banana fruits peal was tested for its effect on mitosis . The root tips of Allium cepa were used as plant test system and the bone marrow cells of the albino mice Mus musculus were used as mammalians test system in vivo .Root tips of Allium cepa were treated for four hours with five concentrations of the extract (5 , 10 , 20 , 40 ,60 mg / ml.).The Metaphase was arrested in all the treatments , the highest percentage ( 100 % ) was recorded in the first concentration , the last concentration caused stickiness and clumping of the chromosomes. The treatments did not cause significant difference in the mitotic index. The peals extract (5 mg /ml) was compared with the extracts of fruits bulb, leaves and r
... Show MoreArsenic is a prevalent and pervasive environmental contaminant with varied amounts in drinking water. Arsenic exposure causes cancer, cardiovascular, liver, nerve, and ophthalmic diseases. The current study aimed to find the best conditions for eliminating arsenic from simulated wastewater and their effect on biomarkers of hepatic in mice. Adsorption tests including pH, contact duration, Al-kheriat dosage, and arsenic concentrations were evaluated. Seventy-two healthy albino mice (male) were accidentally allocated into nine groups (n = 8), the first group was considered as healthy control, the second group (AL-Kheriat), and other groups received AL-Kheriat and arsenic 25, 50, 75, 100, 125, 150 and 175 mg/kg, respectively. Next 10 days, the
... Show MoreThe Islamic Issue did not rise the “widespread arguments” in contemporary times, just as the issue of applying Islamic Law. Just as the Islamic forces used this purpose, or employed it during their march to reach to power by adopting the sacred as motivation towered the power, or control the governance. However, the reality show that this goal remained within the boundaries of slogans in the sense of a teleological slogan, and did not go beyond the limits of advocacy or arrangement as the primary source of legislation with differences of teleological reasoning, in a manner that reflected an intellectual problem about the validity of the use of this concept or the ability to apply and enforce the law in today's world, to impose
... Show MoreUndoped and Co-doped zinc oxide (CZO) thin films have been prepared by spray pyrolysis technique using solution of zinc acetate and cobalt chloride. The effect of Co dopants on structural and optical properties has been investigated. The films were found to exhibit maximum transmittance (~90%) and low absorbance. The structural properties of the deposited films were examined by x-ray diffraction (XRD). These films, deposited on glass substrates at (400? C), have a polycrystalline texture with a wurtzite hexagonal structure, and the grain size was decreased with increasing Co concentration, and no change was observed in lattice constants while the optical band gap decreased from (3.18-3.02) eV for direct allowed transition. Other parameters
... Show MoreStructural and optical properties of CdO and CdO0.99Cu0.01 thin
films were prepared in this work. Cadmium Oxide (CdO) and
CdO0.99Cu0.01semiconducting films are deposited on glass substrates
by using pulsed laser deposition method (PLD) using SHG with Qswitched
Nd:YAG pulsed laser operation at 1064nm in 6x10-2 mbar
vacuum condition and frequency 6 Hz. CdO and CdO0.99Cu0.01 thin
films annealed at 550 C̊ for 12 min. The crystalline structure was
studied by X-ray diffraction (XRD) method and atomic force
microscope (AFM). It shows that the films are polycrystalline.
Optical properties of thin films were analyzed. The direct band gap
energy of CdO and CdO0.99Cu0.01 thin films were determined from
(αhυ)1/2 v
In this research, Mn-doped TiO2 thin films were grown on glass, Si and OIT/glass substrates by R.F magnetron sputtering technique with thicknesses (250 nm) using TiO2:Mn target under Ar gas pressure and power of 100 Watt. Through the results of X-ray diffraction, the prepared thin films are of the polycrystallization type after the process of annealing at 600°C for two hour The average crystalline size were 145.32, 280.97 and 261.23 nm for (TiO2:Mn) thin film on glass, Si and OIT/glass substrates respectively, while the measured surface roughness is between 0.981nm and 1.14 nm. The fabricated (TiO2:Mn) thin film on glass sensors have high sensitivity for hydrogen( H2 reducing gas) compared to the sensitivity for hydrogen gas on Si and OIT/
... Show MoreBeryllium Zinc Oxide (BexZn1-xO) ternary nano thin films were deposited using the pulsed laser deposition (PLD) technique under a vacuum condition of 10-3 torr at room temperature on glass substrates with different films thicknesses, (300, 600 and 900 nm). UV-Vis spectra study found the optical band gap for Be0.2Zn0.8O to be (3.42, 3.51 and 3.65 eV) for the (300, 600 and 900nm) film thicknesses, respectively which is larger than the value of zinc oxide ZnO (3.36eV) and smaller than that of beryllium oxide BeO (10.6eV). While the X-ray diffraction (XRD) pattern analysis of ZnO, BeO and Be 0.2 Zn 0.8 O powder and nano-thin films indicated a hexa
... Show MoreEffect of [Cu/In] ratio on the optical properties of CuInS2 thin films prepared by chemical spray pyrolysis on glass slides at 300oC was studied. The optical characteristics of the prepared thin films have been investigated using UV-VIS spectrophotometer in the wavelength range (300-1100 nm). The films have a direct allow electronic transition with optical energy gap (Eg) decreased from 1.51 eV to 1.30 eV with increasing of [Cu/In] ratio and as well as we notice that films have different behavior when annealed the films in the temperature 100oC (1h,2h), 200oC (1h,2h) for [Cu/In]=1.4 . Also the extinction coefficient (k), refractive index (n) and the real and imaginary dielectric constants (ε1, ε2) have been investigated