Experimental Investigation of Short Square Normal and Hybrid Fiber Reactive Powder Concrete Columns Subjected to Chloride Solution Attack
...Show More Authors

In this research, the structural behavior of reinforced concrete columns made of normal and hybrid reactive powder concrete (hybrid by steel and polypropylene fibers) subjected to chloride salts with concentration was 8341.6 mg/l. The study consists of two parts, the first one is experimental study and the second one is theoretical analysis.  Three main variables were adopted in the experimental program; concrete type, curing type and loading arrangement. Twenty (120x120x1200) mm columns were cast and tested depending on these variables. The samples were reinforced using two different bars; Ø8 for ties and Ø12 with minimum longitudinal reinforcement (0.01Ag). The specimens were divided into two main groups based on curing type: The first group consists of casting and testing of ten columns that cured in tap water for 28 days with two types of concrete (normal and hybrid), five columns for each type. While the second group consists of ten columns that direct cured and fully immersed in chloride water (8341.6 mg/l) 6 months with two types of concrete (normal and hybrid), five columns for each type. The specimens were tested under three types of loading, the first one is axial load, the second one is eccentric load with three different eccentricities (50,100 and 150) mm and where (e/h) are (0.42, 0.83 and 1.25) respectively from the center of column while the third type of loading is tested the specimens as beam.

The experimental results showed an increase in ultimate load capacity and higher chlorides resisting for hybrid reactive powder concrete in comparison with normal concrete in both types of curing (tap and chloride water) through studying strain profile. Interaction diagram charts were obtained from different types of loading for each specimen. These charts showed high values for hybrid reactive powder concrete in comparison with normal concrete.

 

Crossref
View Publication Preview PDF
Quick Preview PDF
Publication Date
Wed Mar 16 2022
Journal Name
2022 Muthanna International Conference On Engineering Science And Technology (micest)
A hybrid feature selection technique using chi-square with genetic algorithm
...Show More Authors

View Publication
Scopus (2)
Crossref (1)
Scopus Crossref
Publication Date
Thu Sep 01 2022
Journal Name
Engineering Structures
Mesoscale analysis of Fiber-Reinforced concrete beams
...Show More Authors

Crossref (3)
Crossref
Publication Date
Fri Nov 13 2020
Journal Name
Mechanics Of Advanced Materials And Structures
Enhancing the strength of reinforced concrete columns using steel embedded tubes
...Show More Authors

This paper demonstrates an experimental and numerical study on the behavior of reinforced concrete (RC) columns with longitudinal steel embedded tubes positioned at the center of the column cross-section. A total of 12 pin-ended square sectional columns of 150 × 150 mm having a total height of 1400 mm were investigated. The considered variables were the steel tube diameters of 29, 58, and 76 mm and the load eccentricity (0, 50, and 150) mm. Accordingly, these columns were divided into three groups (four columns in each group) depending on the load eccentricity (e) to column depth (h) ratio (e/h = 0, 1/3, and 1). For each group, one column was solid (reference), and the other three columns contained steel tubes with hollow rat

... Show More
Crossref (10)
Crossref
Publication Date
Tue Feb 12 2019
Journal Name
Iraqi Journal Of Physics
Effect of industrial powder on mechanical properties of glass fiber reinforced epoxy composite
...Show More Authors

In the present study, composites were prepared by Hand lay-up molding and investigated. The composites constituents were epoxy resin as the matrix, 6% volume fractions of Glass Fibers (G.F) as reinforcement and 3%, 6% of industrial powder (Calcium Carbonate CaCO3, Potassium Carbonate K2CO3 and Sodium Carbonate Na2CO3) as filler. Density, water absorption, hardness test, flexural strength, shear stress measurements and tests were conducted to reveal their values for each type of composite material. The results showed that the non – reinforced epoxy have lower properties than composites material. Measured density results had show an incremental increase with volume fraction increase

... Show More
View Publication Preview PDF
Crossref (2)
Crossref
Publication Date
Sat Aug 21 2021
Journal Name
Engineering, Technology & Applied Science Research
The Impact of Hybrid Fibers on Punching Shear Strength of Concrete Flat Plates Exposed to Fire
...Show More Authors

This study presents an investigation about the effect of fire flame on the punching shear strength of hybrid fiber reinforced concrete flat plates. The main considered parameters are the fiber type (steel or glass) and the burning steady-state temperatures (500 and 600°C). A total of 9 half-scale flat plate specimens of dimensions 1500mm×1500mm×100mm and 1.5% fiber volume fraction were cast and divided into 3 groups. Each group consisted of 3 specimens that were identical to those in the other groups. The specimens of the second and the third groups were subjected to fire flame influence for 1 hour and steady-state temperature of 500 and 600°C respectively. Regarding the cooling process, water sprinkling was applied directly aft

... Show More
View Publication
Crossref (6)
Crossref
Publication Date
Wed Nov 28 2018
Journal Name
International Journal Of Engineering & Technology
Using Polyurethane Coating of Concrete Pipes with Acid Attack Resistance in Sewer Lines
...Show More Authors

One of the most important challenges facing the designers of the sewerage system is the corrosion of sewers due to the influence of sewerage contaminates which lead to failure of the main lines of sewers. In this study, a reference mix of 1: 1.5: 3 was used and the 4% Flocrete PC200 by weight of cement was added to the same mixing ratio in the second mixture. Twenty-four samples were tested for each mixture, 12 of which were used to compression strength test in ages (7, 14 and 28) day and six samples were submerged after 28 days of wet treatment at (5 and 10) % concentrations of sulfuric acid. The other six samples were painted after 28 days of wet treatment with coating Polyurethane and after 24 hours were flooded with a concentrat

... Show More
View Publication
Crossref
Publication Date
Thu Dec 01 2022
Journal Name
Journal Of Engineering
An Experimental Study of Compaction and Strength of Stabilized Cohesive Soil by Stone Powder
...Show More Authors

The In this experimental study, natural stone powder was utilized to improve a cohesive soil’s compaction and strength properties. According to the significant availability of limestone in the globe, it has been chosen for the purpose of the study, in addition to considering the existing rock industry massive waste. Stone powder was used in percentages of 4, 8, 12, 16% replaced from the soil weight in dry state. Some of cohesive soil’s consistency, shear, and compaction properties were depicted after improvement. The outcomes yielded in significant amendments in the experimented geotechnical properties after stone powder addition considering 60 days curing period. Cohesion and friction angle were notably increased by

... Show More
View Publication Preview PDF
Crossref
Publication Date
Mon Aug 01 2022
Journal Name
Journal Of Engineering
Production of Load Bearing Concrete Masonry Units (blocks) From Green Concrete Containing Plastic Waste and Nano Silica Sand Powder
...Show More Authors

Industrial development has recently increased, including that of plastic industries. Since plastic has a very long analytical life, it will cause environmental pollution, so studies have resorted to reusing recycled waste plastic (sustainable plastic) to produce environmentally friendly concrete (green concrete). In this research, producing environmentally friendly load-bearing concrete masonry units (blocks) was considered where five concrete mixtures were compressed at the blocks producing machine. The cement content reduced from 400 kg/m3 (B-400) to 300 kg/m3 (B-300) then to 200 kg/m3 (B-200). While (B-380) was produced using 380 kg/m3 cement and 20 kg/m3 nano-sil

... Show More
View Publication Preview PDF
Crossref (2)
Crossref
Publication Date
Thu Jan 30 2020
Journal Name
Journal Of Engineering
Flexural Behavior of Fiber Reinforced Self-Compacting Rubberized Concrete Beams
...Show More Authors

The massive growth of the automotive industry and the development of vehicles use lead to produce a huge amount of waste tire rubber. Rubber tires are non-biodegradable, resulting in environmental problems such as fire risks. In this search, the flexural behavior of steel fiber reinforced self-compacting concrete (SFRSCC) beams containing different percentages and sizes of waste tire rubbers were studied and compared them with the flexural behavior of SCC and SFRSCC. Micro steel fiber (straight type) with aspect ratio 65 was used in mixes. The replacement of coarse and fine aggregate was 20% and 10% with chip and crumb rubber. Also, the replacement of limestone dust and silica fume was 50%, 25%, and 12% with ground rubbe

... Show More
View Publication Preview PDF
Crossref (4)
Crossref
Publication Date
Wed May 10 2023
Journal Name
Journal Of Engineering
Effect of Petroleum Products on Steel Fiber Reinforced Concrete
...Show More Authors

This Investigation aims to study the effect of adding Steel fibers with different volume fractions Vf (o.5, 0.75, and 1% by volume of concrete) with aspect ratio 100 on mechanical properties of concrete, and also
finding the influence of petroleum products (Kerosene and Diesel) on mechanical properties of Steel Fiber Reinforced Concrete (SFRC).
The experimental work consists of two groups: group one consists of specimens (cubes and prisms) plain and concrete reinforced with steel fiber exposed to continuous curing with water. Group two consists of
specimens (cubes and prisms) plain and concrete reinforced with steel fiber exposed to kerosene and diesel after curing them in water for 28 days before exposure. The results of all te

... Show More
View Publication Preview PDF
Crossref