Asphalt pavement properties in Iraq are highly affected by elevated summer air temperatures. One of these properties is stiffness (resilient modulus). To explain the effect of air temperatures on stiffness of asphalt concrete, it is necessary to determine the distribution of temperatures through the pavement asphalt concrete layers. In this study, the distribution of pavement temperatures at three depths (2cm,7cm, 10cm) below the pavement surface is determined by using the temperature data logger instrument. A relationship for determining pavement temperature as related to depth and air temperature has been suggested. To achieve the objective of this thesis, the prepared specimens have been tested for indirect tension in accordance with ASTM D4123, using the pnuematic repeated load apparatus, in order to determine the values of resilient modulus at three different temperatures (10, 25, 40) °C. From results of testing, it is observed that the resilient modulus decreases with increase in test temperature by a rate of 8.78×10 Psi/C' for asphalt concrete wearing courses. An increase in optimum asphalt content by 0.1% (by weight of total mixture) causes a decrease in resilient modulus by 22% at a temperature of 40C". A statistical model for the prediction of resilient modulus has been developed depending on mixture variables of: asphalt content, asphalt hinder viscosity, surface area of combined aggregates, air voids of compacted mixture and test temperature.
Magnetic Abrasive Finishing (MAF) is an advanced finishing method, which improves the quality of surfaces and performance of the products. The finishing technology for flat surfaces by MAF method is very economical in manufacturing fields an electromagnetic inductor was designed and manufactured for flat surface finishing formed in vertical milling machine. Magnetic abrasive powder was also produced under controlled condition. There are various parameters, such as the coil current, working gap, the volume of powder portion and feed rate, that are known to have a large impact on surface quality. This paper describes how Taguchi design of experiments is applied to find out important parameters influencing the surface quality generated during
... Show MoreThe research discussed the topic of the functional role of responsive materials in being elements of a functional transformation in the design of industrial products, based on the study of the structures of smart materials and their performance capabilities at the level of action and self-reaction that characterize this type of materials.
Basic features of responsive materials have been identified to be elements of self-functional insertion into the industrial product design, which contributes to raising the efficiency and functional capacity of the industrial product and enhancing the ability of products to perform self-acting interactions in the structural structure of the material structure of the product and its ability to res
... Show MoreThe inhibitive action of pomegranate peel as a plant source the corrosion of carbon-steel in phosphoric acid solutions was studied using the weight-loss method. Organic compounds present in natural materials are successfully used to reduce the rate of corrosion because they are cheap, renewable and effective. The results showed that the inhibition potency was enhanced with increasing increasing the amount of the inhibitor and the immersion time but it decreased with the increase of the concentration of the acid solution. The results also revealed a gradual increase in the corrosion rate with the increase of temperature, while the corrosion protection efficiency and surface coverage decreased.
One of the major problems facing the road construction engineer is the collapsible granular soil which may be used for embankment construction. Problems appears when such compacted soil come in touch with water, it exhibits cracking and uncontrolled settlement. Collapsible soils are defined as any unsaturated soil that goes through a radical rearrangement of practice and great loss of volume upon wetting, with or without additional loading. An attempt has been made in this investigation to stabilize the collapsible soil of Nasiriya with asphalt emulsion. Specimens of pure and asphalt emulsion stabilized soil have been prepared using optimum fluid content and tested. The first group of specimens of (60x60x20) cm have been tested for direct s
... Show MoreMoisture damage is a primary mode of distress occurring in hot mix asphalt (HMA) pavements in Iraq. Because of the loss of bond, or stripping, caused by the presence of moisture between the asphalt and aggregate, which is a problem in some areas and can be severe in some cases, it is requires to evaluate the design asphalt mixture to moisture susceptibility. Many factors such as aggregate characteristics, asphalt characteristics, environment, traffic, construction practices and drainage can contribute to stripping. Asphalt concrete mixes were prepared at their optimum asphalt content by superpave system and then tested to evaluate their engineering properties, which include tensile strength, resilient modulus, and perman
... Show More