Mechanical degradation hampers the practical usage of polymers for turbulent drag reduction
application. Mechanical degradation refers to the chemical process in which the activation energy of
polymer chain scission is exceeded by mechanical action on the polymer chain, and bond rupture
occurs. When a water-soluble polymer and surfactant are mixed in water solution, the specific structures
(aggregates) are formed, in which polymer film is formed around micelle. In this work, Xanthan gum (XG) –
Sodium lauryl ether sulfate (SELS) complex formation and its effect on percentage viscosity reduction
(%VR) was studied. It was found that SELS surfactant reduced the mechanical degradation of XG much
more efficiently than this polymer alone. Xanthan Gum (XG) has been tested for its shear stability and
degradability. 0.5% and 1.0 % by weight concentration solutions were exposed to shear stirring at different
speeds and time; also 0.5% through 1.5% by weight concentration solutions of SELS were added to XG
solutions to determine the ability of SELS to reduce the mechanical degradation of XG. It has been noticed
by measuring the percentage viscosity reduction (%VR) of the mixture of XG-SELS that the % VR
decreases when added this surfactant to XG polymer
In this work, porous silicon (PS) are fabricated using electrochemical etching (ECE) process for p-type crystalline silicon (c-Si) wafers of (100) orientation. The structural, morphological and electrical properties of PS synthesized at etching current density of (10, 20, 30) mA/cm2 at constant etching time 10 min are studied. From X-ray diffraction (XRD) measurement, the value of FWHM is in general decreases with increasing current density for p-type porous silicon (p-PS). Atomic force microscope (AFM) showed that for p-PS the average pore diameter decreases at 20 mA. Porous silicon which formed on silicon will be a junction so I-V characteristics have been studied in the dark to calculate ideality factor (n), and saturation current (Is
... Show MoreBackground: syndrome X or metabolic syndrome is a collection of multiple diseases mainly visceral obesity , hypertriglyceridemia , decrease HDL level, hypertension and elevated fasting blood glucose that lead to accelerated atherosclerosis through multiple mechanisms, one of the most important is increase inflammation of the vessels manifested by elevated high sensitivity C reactive protein (hs-CRP).Objective: The aim of the study was to assess the prevalence of elevatedhs CRP in people with metabolic syndrome and atherosclerosis complication (IHD, Cerebrovascular disease, peripheral vascular disease) and metabolic syndrome without these complication.Patients and methods:;This is a cross sectional study carried out in Diabetic referral c
... Show MoreLiquid electrodes of domperidone maleate (DOMP) imprinted polymer were synthesis based on precipitation polymerization mechanism. The molecularly imprinted (MIP) and non-imprinted (NIP) polymers were synthesized using DOMP as a template. By methyl methacrylate (MMA) as monomer, N,Nmethylenebisacrylamide (NMAA) and ethylene glycol dimethacrylate (EGDMA) as cross-linkers and benzoyl peroxide (BP) as an initiator. The molecularly imprinted membranes were synthesis using acetophenone (APH), di-butyl sabacate (DBS), Di octylphthalate (DOPH) and triolyl phosphate (TP)as plasticizers in PVC matrix. The slopes and limit of detection of l
... Show MoreNanofluids, liquid suspensions of nanoparticles (NPs) dispersed in deionized (DI) water, brine, or surfactant micelles, have become a promising solution for many industrial applications including enhanced oil recovery (EOR) and carbon geostorage. At ambient conditions, nanoparticles can effectively alter the wettability of the strongly oil-wet rocks to water-wet. However, the reservoir conditions present the greatest challenge for the success of this application at the field scale. In this work, the performance of anionic surfactant-silica nanoparticle formulation on wettability alteration of oil-wet carbonate surface at reservoir conditions was investigated. A high-pressure temperature vessel was used to apply nano-modification of oil-wet
... Show MoreThe dry weight of the liver of Rana ridibunda was expressed as percentage of the dry
weight of the body. The female liver weight always exceeds that of the male, except in July
and September. The difference between males and females for the whole year, regardless of
months, was not significant. Livers of both sexes were relatively large prior to hibernation
(December), decreased during hibernation (January and February) until a minimum weight in
March (post-hibernation).
The increase of liver weight during December is apparently simply to meet the metabolic
requirements for survival during hibernation. The percent reduction in liver weight during
hibernation was 1.081% in males and 1.356% in females. The decrease
Thin films were prepared from melting coumrin C 2 dye in solvent DMF with PMMA with the same solvent and concentrations(1*10-2 5*10-3, 1*10-3 )M ,Films were either left on Flat surface for24hours or dried in avacuum oven for five hours at a temperature of 80c.The relative intensity of both the absorption and fluorescece spectrum are found to be increased with the increase of thickness of these films and concentration .Also the thickness of these films was measured by Mickelsons interfearing method.Also quantum efficiency of these films were measured too
ABSTRACT Background: Improving the properties of heat- cured and self-cured acrylic resin have been studied by many researchers. However, little studies concerned with visible light cured resin (VLCR) improved through addition of nanofiller are available. The purpose of this study was to evaluate some properties of (VLCR) after addition of SiO2 nanofiller. Materials and Methods: SiO2 nanofiller were added to (VLCR) tray material after being dissolved in tetrahydrofuran (THF) solvent. According to the pilot study 2% SiO2 nanofiller addition exhibited better properties than the other percentages (1%, 3%). The main study conducted involved (100) specimens divided into 5 groups according to the test included. (20) Specimens were selecte
... Show MoreThis paper aims to study the chemical degradation of Brilliant Green in water via photo-Fenton (H2O2/Fe2+/UV) and Fenton (H2O2/Fe2+) reaction. Fe- B nano particles are applied as incrustation in the inner wall surface of reactor. The data form X- Ray diffraction (XRD) analysis that Fe- B nanocomposite catalyst consist mainly of SiO2 (quartz) and Fe2O3 (hematite) crystallites. B.G dye degradation is estimated to discover the catalytic action of Fe- B synthesized surface in the presence of UVC light and hydrogen peroxide. B.G dye solution with 10 ppm primary concentration is reduced by 99.9% under the later parameter 2ml H2O2, pH= 7, temperature =25°C within 10 min. It is clear that pH of the solution affects the photo- catalytic degradation
... Show More