The permanent deformation of flexible pavement represent serious problem in hot climate region. Numerous efforts are devoted to mitigate this distress such as modifying asphalt binder by polymers. The present study demonstrate the effect of utilizing four types of polymers to reduce the permanent deformation, these polymers are Polyethylene Wax (PEW), Styrene Butadiene Rubber (SBR), Ethylene Propylene Dien Monomer (EPDM) and Ethylene Vinyl Acetate (EVA). The prepared mixtures composed of 4.9 % of 40/50 asphalt binder, 12.5 mm nominal aggregate maximum size and limestone dust as filler. The permanent and resilient strains have been recorded when the cylindrical specimens, 101.6 mm in diameter and 203.2 mm in height, tested by repeated loading system. The main conclusions exhibit that SBR and EPDM with the same concentration (15 % by weight of asphalt binder) reduced the permanent deformation by 30.20 % and 30.46 % respectively. Although, the PEW and EVA reduced permanent deformation by lower values, 13.24 % and 17.35 % respectively, but the incremental percentage of their action are higher. The influences of testing temperature and stress level on permanent deformation were investigated. Linear regression model was established to correlate the values of permanent deformation and the resilient modulus of asphalt mixtures.
In this study, the response and behavior of machine foundations resting on dry and saturated sand was investigated experimentally. A physical model was manufactured to simulate steady state harmonic load at different operating frequencies. The effect of relative density, depth of embedment, foundation area as well as the imposed harmonic load was investigated. It was found that the amplitude of displacement of the foundation increases with increasing the amplitude of dynamic force and operating frequency meanwhile it decreases with increasing the relative density of sand, degree of saturation, depth of embedment and contact area of footing. The maximum displacement was noticed at 33.34 to 41.67 Hz. The maximum displaceme
... Show MoreThis study evaluates the performance of magnetic abrasive finishing (MAF) of aluminum alloy in terms of achieving materials removal (MR). A vertical milling machine is used to perform the finishing process using a developed MAF unit that consists of an inductor made out of a 150 mm long and 20 mm diameter iron core wound with 1500 turns and 0.5 mm copper wire. The commutator and magnetic pole are attached at the top and bottom of the inductor, respectively. The required current is supplied using a DC power supply. The South Pole workpiece is a 100×50×3 mm3 plate of AA 1100 aluminum alloy, whereas the magnetic pole represented the North Pole. Pole rotational speed, applied current, and abrasive finishing time was selected as
... Show MoreSelf-compacted concrete (SCC) considered as a revolution progress in concrete technology due to its ability for flowing through forms, fusion with reinforcement, compact itself by its weight without using vibrators and economic advantages. This research aims to assess the fresh properties of SCC and study their effect on its compressive strength using different grading zones and different fineness modulus (F.M) of fine aggregate. The fineness modulus used in this study was (2.73, 2.82,2.9& 3.12) for different zones of grading (zone I, zone II& marginal zone(between zone I&II)) according to Iraqi standards (I.Q.S No.45/1984).Twelve mixes were prepared, each mix were tested in fresh state with slump, V-Funnel and L-Box tests, then 72
... Show MoreSelf-compacted concrete (SCC) considered as a revolution progress in concrete technology due to its ability for flowing through forms, fusion with reinforcement, compact itself by its weight without using vibrators and economic advantages. This research aims to assess the fresh properties of SCC and study their effect on its compressive strength using different grading zones and different fineness modulus (F.M) of fine aggregate. The fineness modulus used in this study was (2.73, 2.82,2.9& 3.12) for different zones of grading (zone I, zone II& marginal zone(between zone I&II)) according to Iraqi standards (I.Q.S No.45/1984).Twelve mixes were prepared, each mix were tested in fresh state with slump, V-Funnel and L-Box tests, t
... Show MoreThe aim of our current study was to identify the effect of particulate matter of both types (PM2.5 and PM10) resulting from hookah smoking on the hemopoietic system of workers (smokers) in closed cafes. This study included six stations (cafes) on the Rusafa side of Baghdad city and conducted a blood test that included a complete blood count (CBC). A multifunctional air quality detector measured both types of particulate matter in the morning and evening. The study included 30 men (workers and smokers) and 30 men (non-smokers), whose ages ranged from 20 to 40 years. The study found that smokers had an increase in white blood cells and red blood cells, as well as an increase in the percentage of hemoglobin (HGB), hematocrit (HCT), the mean co
... Show MoreThe structural, optical properties of cupper indium gallium selenite (CuIn1-xGaxSe) have been studied. CuIn1-xGaxSe thin films for x=0.6 have been prepared by thermal evaporation technique, of 2000±20 nm thickness, with rate of deposition 2±0.1 nm/sec, on glass substrate at room temperature. Heat treatment has been carried out in the range (373-773) K for 1 hour. It demonstrated from the XRD method that all the as-deposited and annealed films have polycrystalline structure of multiphase. The optical measurement of the CIGS thin films conformed that they have, direct allowed energy gap equal to 1.7 eV. The values of some important optical parameters of the studied films such as (absorption coefficient, refractive index, extinction coeffici
... Show MoreThe paper include study the effect thickness of the polymeric sample which is manufactured by thermo press way. The sample was used as an active tunable R6G laser media. The remarks show that, when the thickness of the samples is increased, with the same concentration, the spectrum will shift towards the short wavelength, & the quantum fluorescence yield will increased. The best result we obtained for the quantum fluorescence yield is (0.68) at the sample, with thickness (0.304mm) in Ethanol solvent, while when we used the Pure Water as a solvent, we found that the best quantum fluorescence yield is (0.63) at (0.18mm) thickness of the sample.
Newcastle Disease is one of the most important disease world wide distributions which invade the flock in different age resulting in large economic losses. This study aimed to evaluate the effect of treatment with 4 different concentrations (0.25, 0.5, 1.0 and 2.0 %) of Sodium deoxycholate (SDC) on the vaccinal virus (La Sota) using inoculation in the fragments of Chorioallantoic membrane. The treatment with each of the above 4 concentrations of SDC resulted in an increase in the Hemagglutination titer (HA) of the virus (28, 29.6, 211.6, 214.6) respectively as compared to the HA titer value for the untreated virus (26.6). No significant differences were noticed among all concentrations with regard to their effect on the HA titer, except
... Show More