Friction stir welding (FSW) of Tee-joints is obtained by inserting a specially designed rotating pin into the clamped blanks, through top plate (skin) to bottom plate (stringer), and then moving it along the joint, limiting the contact between the tool shoulder and the skin. The present work aims to investigate the defects occur for Tee-joint of an Aluminum alloy (Al 5456) with dimensions (180mm x 70mm) for the skin plate, (180mm x 30mm) for stringer plate and thickness of (4mm).
The effects of welding parameters such as rotational speed, linear speed, plunging depth, tool tilting, and die radii of welding fixture on the welding quality of Aluminum Alloy will be studied. Weld defects had been summarized and studied, and then the best conditions that led to good welds had been estimated.
Resistance spot welding (RSW) aluminum alloys has a major problem of inconsistent quality from weld to weld, because of the problems of the non-uniform oxide layer. The high resistivity of the oxide causes strong heat released which influence significantly on the electrode lifetime and the weld quality. Much effort has been devoted experimentally to the study of the sheet surface characteristics for as-received sheet and surface pretreatment sheet by pickling in NaOH and glassblasted with three thicknesses (0.6, 1.0, and 1.5 mm) of AA1050. Three different welding process parameters energy setup as a low, medium, and high were carried. Tensile-shear strength tests were performed to indicate the weld quality. Moreover, microhardness tests,
... Show MoreThe method of powder technology has been utilized for fabrication of ceramic filters. Ceramic filters with interconnected porosity have been achieved via mixes of ceramic powders with addition of glass powders, therefore, interparticle glassy phase is introduced and act as a weld between the crystalline grains in a high porosity microstructure. Tow types of ceramic filters have been produced, the first with high silica content and the other is with high alumina content. Both physical and mechanical properties has been performed and discussed
Three different rotational speeds (800, 1000 and 1250 rpm) and traverse speeds of (0.42 mm/sec) at a constant taped pin have been employed to produce the stir zones generated from friction stir processing (FSP) of near eutectic Al- 14 wt.% Si alloy. The processed samples were thoroughly analyzed macroscopically and microscopically. The as-cast microstructure of eutectic (α Al+ Si) and primary Si were fragmented to produce spheroidization of small size of Si and deformed matrix. The stir zones showed an increase in hardness from around 45-50 Hv for as-cast to 40-65 depending on the variables applied. All the processed samples were characterized by advanced and retreated regions with large single piping defects formed m
... Show MoreThis research deals with the effects of welding variables using MIG/MAG spot by using Argon (Ar) gas and CO2 to show their effect on the mechanical characteristics and microstructure of low alloy steel type DIN15Mo3 and determine the optimum condition for the process of welding ; current & time. The results show the possibility of using CO2 and also Ar in low alloy steel welding with a little decrease in the shear force of not more than 13% for 4mm thickness and time 2sec. The shear force increased when using Ar instead of CO2 to be , The shear force reach 36KN when using Ar at 2mm thickness time of 8 sec and current of 220 Amp. , when used CO2 instead of Ar d
... Show MoreRobots have become an essential part of modern industries in welding departments to increase the accuracy and rate of production. The intelligent detection of welding line edges to start the weld in a proper position is very important. This work introduces a new approach using image processing to detect welding lines by tracking the edges of plates according to the required speed by three degrees of a freedom robotic arm. The two different algorithms achieved in the developed approach are the edge detection and top-hat transformation. An adaptive neuro-fuzzy inference system ANFIS was used to choose the best forward and inverse kinematics of the robot. MIG welding at the end-effector was applied as a tool in this system, and the wel
... Show MoreA fuzzy logic approach (FLA) application in the process of stud arc welding environment was implemented under the condition of fuzziness input data. This paper is composed of the background of FLA, related research work review and points for developing in stud welding manufacturing. Then, it investigates thecase of developingstud arc welding process on the controversial certaintyof available equipment and human skills.Five parameters (welding time, sheet thickness, type of coating, welding current and stud shape) were studied.A pair of parameter was selected asiteration whichis welding current and welding time and used fo
... Show MoreThe present research investigates joints welding of 304L austenitic stainless steel using metal inert gas (MIG) welding method. The research explores the effect of process parameters (arc voltage, wire feed rate, and electrode wire diameter) on the mechanical properties of stainless steel. The above variables are varied respectively with 18.5, 19, 19.5 V, 116, 127, 137 mm/s, and 0.8, 1, 1.2 mm, with E308L as a filler electrode. The design matrix of the experiments was determined using the design of experiment (DOE) program Minitab 17 based on the levels of input elements used. The Taguchi orthogonal matrix methodology (Taguchi) technique was used to develop some empirical analysis for the maximum tensile strength and proper surface
... Show MoreThis paper represents an experimentalattempt to predict the influence of CO2-MAG welding variables on the shape factors of the weld joint geometry. Theinput variables were welding arc voltage, wire feeding speed and gas flow rate to investigate their effects on the shape factorsof the weld joint geometry in terms of weld joint dimensions (bead width, reinforcement height, and penetration). Design of experiment with response surface methodology technique was employed to buildmathematical models for shape factors in terms of the input welding variables. Thepredicted models were found quadratic type and statistically checked by ANOVA analysis for adequacy purpose. Also, numerical and graphical optimizations were carried out
... Show MoreIn the present study, MIG welding is carried out on low carbon steel type (AISI 1015) by using electrode ER308L of 1.5mm diameter with direct current straight polarity (DCSP). The joint geometry is of a single V-butt joint with one pass welding stroke for different plate thicknesses of 6, 8, and 10 mm. In welding experiments, AISI 1015 plates with dimensions of 200×100mm and edge angle of 60o from both sides are utilized. In this work, three main parameters related to MIG welding process are investigated, which are welding current, welding speed, heat input and plate thickness, and to achieve that three groups of plates are employed each one consists of three plates. The results indicate that increasing the weld heat input (t