Fiber Reinforced Polymer (FRP) bars are anisotropic in nature and have high tensile strength in the fiber direction. The use of High-Strength Concrete (HSC) allows for better use of the high-strength properties of FRP bars. The mechanical properties of FRP bars can yield to large crack widths and deflections. As a result, the design of concrete elements reinforced with FRP materials is often governed by the Serviceability Limit States (SLS). This study investigates the short-term serviceability behavior of FRP RC I-beams. Eight RC I-beams reinforced with carbon-FRP (CFRP) and four steel RC I-beams, for comparison purposes, were tested under two-point loading.
Deformations on the concrete and crack widths and spacing are measured and analyzed. A discussion on the main aspects of the SLS of FRP RC is introduced. The service load that fulfills the serviceability requirements, at a cross-section level, ranges between 0.27 and 0.38 times the ultimate load for sections dimensioned to fail in concrete crushing. The determinant criterion is the deflection limitation
The goal of this article is to construct fibrewise w-compact (resp. locally w-compact) spaces. Some related results and properties of these concepts will be investigated. Furthermore, we investigate various relationships between these concepts and three classes of fibrewise w-separation axioms.
Reactive Powder Concrete (RPC) can be incorporate as a one of the most important and progressive concrete technology. It is a special type of ultra-high strength concrete (UHSC) that’s exclude the coarse aggregate from its constitutive materials. In this research an experimental study had been carried out to investigate the effect of using three types of materials (porcelain aggregate) and others sustainable materials (glass waste and granular activated carbon) as a partial replacement of fine aggregate. Four percentages had considered (0, 10, 15 and 20) % to achieve better understanding for the influence of these materials upon the compressive strength of RPC. Four curing ages had included in this study, these are; 7, 28, 60 and
... Show MoreThe aim of this study is to determine the flexural properties of steel fiber as a metal fiber and polyester resin as a matrix. The steel fibers were added to polyester resin at the various fiber volume fractions of 5, 10, and 15% steel fiber, and with different fiber orientations such as woven steel fiber type (0-45) ° and woven steel fiber type (0-90) ° indicate. Hand layup processes in these experiments were used to produce specimens test with the curing time of 24 hr. for the composite at room temperature. The results show that the flexural strength and flexural modulus values for 15 % vol.of woven steel fiber composite type (0-90) ° are (210MPa) and (2.29GPa( respectively. The results above indicate that the woven steel fiber (0-9
... Show MoreThe association of phytoplasma was investigated in symptomatic tomato (
Background: Change in palatal vault shape and Reinforcement of high impact acrylic denture base resin may in turn affect the dimensional accuracy of acrylic resin and affecting the fitness of the denture. The aim of study is to evaluate the effect of fiber reinforcement for high-impact acrylic resin denture base with different palatal vault shapes on linear dimensional change and effect of palatal vault shapes on linear dimensional changes of non-reinforced and fiber reinforced high impact denture base acrylic resin Material and method: Three different palatal vault shapes were prepared on standard casts using CNC (computer numerical control) machine. 60 samples of heat polymerized high impact acrylic resin maxillary denture base were fabri
... Show MoreStudies on the flexural behavior of post-tensioned beams subjected to strand damage and strengthened with near-surface mounted (NSM) technique using carbon fiber-reinforced polymer (CFRP) are limited and fail to examine the effect of CFRP laminates on strand strain and strengthening efficiency systematically. Furthermore, a design approach for UPC structures in existing design guidelines for FRP strengthening techniques is lacking. Hence, the behavior of post-tensioned beams strengthened with NSM-CFRP laminates after partial strand damage is investigated in this study. The testing program consists of seven post-tensioned beams strengthened by NSM-CFRP laminates with three partial strand damage ratios (14.3% symmetrical damage, 14.3%
... Show MoreIn individuals with type 2 diabetes mellitus (T2DM), the cannabinoid receptor 1 (CNR1) gene polymorphism has been linked to diabetic nephropathy (DN). Different renal disorders, including DN, have been found to alter cannabinoid (CB) receptor expression and activation. This cross-sectional study aimed to investigate the relationship between CNR1 rs1776966256 and rs1243008337 genetic variants and the risk of developing DN in Iraqi patients with T2DM. The study included 100 patients with T2DM, divided into two groups: 50 with DN and 50 without DN. Genotyping of CNR1 rs1776966256 and rs1243008337 polymorphisms was conducted using PCR in DN patients and control samples. The distribution of rs1776966256 and rs1243008337 genotypes and alleles bet
... Show MoreIn recent years, there has been a rapid development in research on high performance ceramics for mechanical, electrical and medical industries. This development will be shown for alumina as a representative for oxide ceramics powders.
Dry–pressing forming technique was used to prepare different ceramic compacts for alumina grafted by polymethacrylate polymers. All Alumina compact were fired firstly at 1200 ◌ْ C, then
at 1600 ◌ْ C.
Mechanical strength was examined in different means, some
depends on compression and other depends on impact. Hardness was
also measured .The results obtained were compared with that of
Alumina compact prepared under the same condition from Alumina
especially made for pressing .
The polymeric hydrogels composed of poly vinyl alcohol (m.wt 72000) and glutaraldehyde(5%,8% and 10%) , have been thermally prepared for the purpose of studying their swelling and drug release behavior . The swelling ratio was measured for all the hydrogel samples at 37°C, in three different media pH (1.2, 4.7 and 6.8) as a function of time. The results show that the maximum swelling ratios were arranged as follows :pH =6.8 > pH =4.7 > pH =1.2 hydrogels cross linked PVA showed a typical pH responsive behavior such as high pH has maximum swelling while low pH shows minimum swelling.